1-20 of 26 Search Results for

AISI Type 348

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1963) 12 (9): SS-147.
Published: 01 September 1963
... AISI Type 348 is an austenitic chromium-nickel type stainless steel with the carbon stabilized by columbium-tantalum for welding and elevated temperature service. This type is useful when the weldment is not annealed after welding. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1979) 28 (5): TS-348.
Published: 01 May 1979
... properties workability UNS T11307 I I Filing Code: TS-348 1 CARPENTER SEVEN STAR 1 Tool Steel I I MAY 1979 OIG19FT - DATA ON WORLD WIDE METALS AND ALLOYS lbbldkdbu CARPENTER* SEVEN STAR (High-Speed Sted; AISI Type M7) CARPENTER SEVEN STAR is a molybdenum-type high-speed steel containing tungsten...
Journal Articles
Alloy Digest (1978) 27 (3): SS-348.
Published: 01 March 1978
... TECH-TRONIC 32 stainless steel is essentially a low-nickel chromium-manganese austenitic iron-base alloy. In the annealed condition it provides about twice the yield strength of AISI Type 304 stainless steel and almost the same resistance to corrosion. It also offers improved wear and galling...
Journal Articles
Alloy Digest (1975) 24 (6): SS-312.
Published: 01 June 1975
.... psi PROPERTIES Table 1 - ROOM-TEMPERATURE TENSILE PROPERTIES OF UNILOY 18-2 FM AND TWO OTHER STAINLESS STEELS Grade Tensile Yield Strength Strength (0.2% Offset) psi Psi Annealed Properties Uniloy 18-2 Fhl 70000 AISI Type 303 90000 AISI Type 416 7.5000 Cold-Drawn Properties Uniloy 18-2 FM 8.5000 AIS1...
Journal Articles
Alloy Digest (2004) 53 (9): SS-908.
Published: 01 September 2004
... strength will be lower for the weld com- pared with the high-strength base material. Therefore, welds in Sandvik 1RK91 are not suitable for active parts of a construction, when extremely high strength is required. Corrosion Resistance: This alloy has a corrosion resistance comparable to AISI type 304L...
Journal Articles
Alloy Digest (1966) 15 (4): TS-178.
Published: 01 April 1966
... AISI Type H25 is a high-tungsten hot-work steel having heat resitance. It retains a high degree of working hardness at elevated temperatures. It is recommended for brass extrusion and forging dies, punches, cut-off knives, backet and dummy blocks. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1997) 46 (12): SS-703.
Published: 01 December 1997
... Finkl 420MB is a resulfurized modification of AISI 420F stainless steel for mold bases. The alloy is clean, tough, and machinable. It is available by VAD and balanced oxidation techniques. This datasheet provides information on composition, physical properties, and hardness. It also includes...
Journal Articles
Alloy Digest (1954) 3 (4): SA-16.
Published: 01 April 1954
... AISI E52100 is a high-carbon, chromium alloy steel of the water hardening type. It has great depth hardenability and high wear resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming...
Journal Articles
Alloy Digest (1954) 3 (3): SA-15.
Published: 01 March 1954
... AISI 8640 is a nickel-chromium-molybdenum alloy steel of the oil hardening type. It has good hardenability and desirable toughness. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on low temperature...
Journal Articles
Alloy Digest (2005) 54 (3): TS-614.
Published: 01 March 2005
... Finkl DC is a single-vacuum melted AISI H13 type material made by the vacuum arc degassing (VAD) process. The vanadium content of 1% in addition to a high chromium (Cr 5%) and molybdenum (Mo 1.4%) promotes hot strength and wear resistance. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1954) 3 (7): SA-21.
Published: 01 July 1954
... AISI 8740 is a medium-carbon, nickel, chromium, molybdenum alloy steel of the oil hardening type. It has good hardenability and desirable toughness. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also...
Journal Articles
Alloy Digest (1997) 46 (7): SS-690.
Published: 01 July 1997
... Armco 11 Cr-Cb stainless steel has higher silicon content and is dual stabilized with titanium and columbium (niobium). The alloy is designed for use in automotive exhaust systems and should be considered where the performance of AISI Type 409 stainless steel is marginal. This datasheet provides...
Journal Articles
Alloy Digest (1984) 33 (2): SA-397.
Published: 01 February 1984
... AISI 4161 is a low-alloy steel of the chromium-molybdenum type; it contains nominally 0.61% carbon. It has relatively high hardenability and good resistance to abrasion, impact and fatigue. It is an oil-hardening grade and is recommended for moderately heavy-duty service. This steel has...
Journal Articles
Alloy Digest (1954) 3 (12): SS-22.
Published: 01 December 1954
... alkaline solutions, good resistsnce to oil refinery audes below 400┬░F., good resistance m mineral and vegetable oils, pwr resistance m am- monium and hot sulphite liquors. Specification Equivalentsz ASTM Al99, Al.0 ASTM A200, Al.8 ASTM A213, T5 ASTM Al58, P5a ASTM A132, F5 ASTM A193, B5 AISI Type 501 + MO...
Journal Articles
Alloy Digest (1964) 13 (6): SS-156.
Published: 01 June 1964
... be used, if a temperature of 750 deg. F and a rime of 15 minutes are not exceeded. General Chomcteri sties: AISI No. 630 is hardenable by hear treatment co hard- ness and tensile strength values similar co those of standard Types 410, 414. 416 and 431 stainless steels, but co much higher yield strength...
Journal Articles
Alloy Digest (1954) 3 (8): SS-17.
Published: 01 August 1954
... 1996DOI: 10.31399/asm.ad.ss0017 Machinability: Machining charactaistics in the annealed condition ate similar to those of Type 410 stainless steel when the latta grade is in the hardness range of 280-320 Brinell An excellent surface 6nish is obtained. For quai hardness the tool life for Type 416...
Journal Articles
Alloy Digest (1954) 3 (1): CS-1.
Published: 01 January 1954
...-speed sate1 driIIs of sraadard design at cnaing speeds of 70-90 %= forV2"driusThread chasing cap be done at 30.65 s ll& using a lo-15 de&$ hookgrindonchecher.Tlmadchvingwirhcarbiduipped dlnddmrscanbedonear375sfpaL Geneml Characteristics2 R. L~& ore-hear~rreaced nr+~ type, high snlphpr chasucd composraon...
Journal Articles
Alloy Digest (1954) 3 (10): TS-25.
Published: 01 October 1954
... SENECA is a tungsten-chromium type of hot work steel having good red hardness and resistance to abrasion. It will withstand high operating temperatures up to 1000 deg. F for long periods. It is a SAE type IV F-2 alloy. This datasheet provides information on composition and hardness as well...
Journal Articles
Alloy Digest (1954) 3 (12): TS-28.
Published: 01 December 1954
... VULCAN NON-SHRINKABLE is a standard manganese type of oil hardening tool steel for use where non-shrinking and non-deforming properties are important. This is an ASM Class II-A2 and SAE Type 02 Alloy. This datasheet provides information on composition and hardness as well as fracture toughness...
Journal Articles
Alloy Digest (2006) 55 (3): SS-956.
Published: 01 March 2006
... as in an ordinary stainless spring steel of the type AISI 301 cannot be reached. Sandvik Steel Co. Scranton, PA 18501-1220 (570) 585-7511 (570) 585-7513 (fax) In Sweden: Sandvik AB Sandviken 46 26 26 30 00 46 26 25 17 10 (fax) www.sandvik.com ISSN: 002-614X SS-956B Annealed Condition. With this alloy...