Skip Nav Destination
Close Modal
Search Results for
AISI Type 321
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 66 Search Results for
AISI Type 321
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Journal Articles
Alloy Digest (1961) 10 (11): SS-124.
Published: 01 November 1961
... AISI Type 321 is a titanium stabilized 18-10 stainless steel having a maximum operating temperature of 1650 F. It is recommended for welded equipment and structures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well...
Abstract
View article
PDF
AISI Type 321 is a titanium stabilized 18-10 stainless steel having a maximum operating temperature of 1650 F. It is recommended for welded equipment and structures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-124. Producer or source: Stainless steel mills.
Journal Articles
Alloy Digest (1983) 32 (5): SS-426.
Published: 01 May 1983
... should be welded using AISI Type 347 coated electrodes. If an inert gas method is used, TIG or MIG, AISI Types 321 or 347 filler weld metal can be used. AI S1 Type 321. because of its resistance to intergranular corrosion, is recommended as electrode or filler wire for those applications where the welded...
Abstract
View article
PDF
CRUCIBLE 321 is a non-hardenable austenitic chromium-nickel steel which is particularly adaptable for parts fabricated by welding without postweld annealing for use at temperatures between 800 and 1500 F. This grade is non-magnetic in the annealed condition but is slightly magnetic when cold worked. Among its many applications are aircraft-engine exhaust manifolds, furnace parts and expansion joints. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-426. Producer or source: Crucible Specialty Metals Division, Colt Industries.
Journal Articles
Alloy Digest (1977) 26 (7): TS-321.
Published: 01 July 1977
... or Source: Tool steel mills Copyright © ASM International® 1996 1996 ASM International AISI TYPE M10 chemical composition elasticity hardness heat treatability lathe tools machinability physical properties reamers taps tensile properties workability A181 Type Ml0 Filing Code: TS-321...
Abstract
View article
PDF
AISI Type M10 is the high vanadium type of molybdenum high-speed steel. It is a deep-hardening steel and offers high cutting ability and excellent finishing properties. It is a general-purpose steel for cutting tools and is used in such applications as taps, lathe tools and reamers. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance as well as forming, heat treating, machining, and surface treatment. Filing Code: TS-321. Producer or source: Tool steel mills.
Journal Articles
Alloy Digest (1990) 39 (8): SS-327.
Published: 01 August 1990
... ARMCO NITRONIC 40 Stainless Steel is one of the most versatile austenitic stainless steels with a room-temperature yield strength about twice that of AISI Types 304, 321 and 347. In addition, NITRONIC 40 has remarkably good elevated temperature properties and oxidation resistance. It retains high...
Abstract
View article
PDF
ARMCO NITRONIC 40 Stainless Steel is one of the most versatile austenitic stainless steels with a room-temperature yield strength about twice that of AISI Types 304, 321 and 347. In addition, NITRONIC 40 has remarkably good elevated temperature properties and oxidation resistance. It retains high toughness down to -423 F. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on low temperature performance and corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-327. Producer or source: Armco Advanced Materials Corporation. Originally published as Nitronic 40, May 1976, revised August 1990.
Journal Articles
Alloy Digest (1981) 30 (11): SS-396.
Published: 01 November 1981
... is usually satisfactory. Where heavier oxides are Involved, the ratio of nitric to hydrofluoric acid should be lowered. Op- erating temperatures are 1 2&140°F. Specification Equivalents: AISI Type 321. UNS No. S32100. ASTM: A 167, A 213, A 240. A 249, A 269, A 276, A 314, A 473, and A 479. General...
Abstract
View article
PDF
EASTERN STAINLESS Type 321 is a titanium-bearing steel designed to be free from the harmful chromium carbide precipitation (and associated intergranular corrosion) after welding or after an extended period of time in the sensitizing temperature range (800-1600 F). Type 321 is used primarily within this sensitizing (damaging) temperature range; however, its carbon combines preferentially with titanium leaving chromium in solution to maintain full corrosion resistance. Among its applications are high-temperature steam service, chemical plants and heavy-duty aircraft exhaust manifolds. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-396. Producer or source: Eastern Stainless Steel Company.
Journal Articles
Alloy Digest (1963) 12 (11): SS-149.
Published: 01 November 1963
... be lowered. Operating temperatures are 120-140 deg. F. Heat Resistance: Scaling temperature is 1600oF for continuous service and 145OoF for intermittent service. Specification Equivalents: AISI Type 321 Single point turning tools of high speed steel should be ground to 5-10 deg. top or rake angle, 5-10 deg...
Abstract
View article
PDF
ENDURO 18-8STi is the titanium-type 304 stainless steel stabilized by titanium. It is not made sensitive to intergranular corrosion by heating within the carbide precipitation range. It is recommended for use at temperatures up to 1600 F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-149. Producer or source: Republic Steel Corporation.
Journal Articles
Alloy Digest (1956) 5 (5): SS-43.
Published: 01 May 1956
... Uppef Montclair, New Jersey U. S. S. 18-8 Ti (Corrosion Resisting Steel, Type 321) U.S. S. 18-8 Ti is an austenitic chromium nickel steel containing titanium. Is is recommended for pam fabriated by welding which annot be subsequently annealed. It is aho recommended for parts to be used at temperaaxes...
Abstract
View article
PDF
U.S.S. 18-8 Ti is an austenitic chromium nickel steel containing titanium. It is recommended for parts fabricated by welding which cannot be subsequently annealed. It is also recommended for parts to be used at temperatures between 800 and 1650 deg. F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-43. Producer or source: United States Steel Corporation.
Journal Articles
Alloy Digest (1967) 16 (6): SS-195.
Published: 01 June 1967
...!oF (32-2120F) Thermal conductivity, Btu/ ft2/fr/hr/oF at 2120F ac 9320F Thermal coef. expansion, in/ in/OF x 10-6 32- 212oF 32-1000oF 32-15000F Electrical resistance, microhm-cm Modulus of elasticity, psi x 106 Specification Equivalents: AISI Type 321 SAE Type 321 ASTM A269 TP 321 ASTM A276 TP 321 Fed...
Abstract
View article
PDF
DARWINS 18/8 W.P.D. is a titanium stabilized 18/8 type stainless steel being free of weld decay. It is recommended for welded equipment and structures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-195. Producer or source: Darwin's Ltd.
Journal Articles
Alloy Digest (1974) 23 (9): Ni-208.
Published: 01 September 1974
... or titanium- bearing grades), AISI Type 346 stainless steel. and 1 l-14% manganese steels. It can be deposited with some difficulty on cast iron, AISI Type 321 stainless steel. chromium stainless steels (400 series) and some tool steels; the manufacturer can provide more details. CAUTION: Welding may produce...
Abstract
View article
PDF
HAYNES Alloy No. 273 is a nickel-base, hard-facing alloy developed to provide extra life for hot-working equipment such as hot-forging dies, hot-shear blades and hot-extrusion dies. It is deposited by using a composite electrode with nickel-base core and the balance of the alloying elements in the flux coating. Deposits retain their hardness up to 1200 F. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-208. Producer or source: Cabot Corporation.
Journal Articles
Alloy Digest (1963) 12 (3): SA-143.
Published: 01 March 1963
... AISI 3150 is a medium carbon, chromium-nickel alloy steel having great depth hardness, high elastic properties and excellent fatigue resistance and toughness. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture...
Abstract
View article
PDF
AISI 3150 is a medium carbon, chromium-nickel alloy steel having great depth hardness, high elastic properties and excellent fatigue resistance and toughness. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on heat treating and machining. Filing Code: SA-143. Producer or source: Alloy steel mills and foundries.
Journal Articles
Alloy Digest (2000) 49 (12): SS-810.
Published: 01 December 2000
...) Shear modulus, GPa (106 psi) 78 (11.2) Tensile strength, MPa (ksi) 621 (90) Yield strength, 0.2%, MPa (ksi) 241 (35) Elongation in 2 in. (50.8 mm), annealed, % 45 Hardness, HRB 80 Heat Treatment: Type 321 is not hardenable by heat treatment. Annealing is ac- complished by heating to 954 1121 °C (1750...
Abstract
View article
PDF
Armco 321 is an austenitic nickel-stainless-steel with the carbon stabilized by titanium for welding and elevated temperature service. It is useful when the weldment is not annealed after welding. This alloy is nonmagnetic when annealed but is slightly magnetic when cold worked. It has excellent resistance to corrosion and oxidation, possesses high creep strength, and may be used at temperatures up to 871 C (1600 F). Titanium is added to this alloy to impart substantial immunity to intergranular corrosion. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-810. Producer or source: AK Steel Inc.
Journal Articles
Alloy Digest (1964) 13 (9): SA-167.
Published: 01 September 1964
... AISI 9260 is an oil-hardening type of spring steel and tool steel recommended for repeated and severe impact service. It is also used for heavy duty, shock resistant machine parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Abstract
View article
PDF
AISI 9260 is an oil-hardening type of spring steel and tool steel recommended for repeated and severe impact service. It is also used for heavy duty, shock resistant machine parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-167. Producer or source: Alloy steel mills and foundries.
Journal Articles
Alloy Digest (1971) 20 (5): SS-254.
Published: 01 May 1971
... AISI 304 and 304L are low-carbon chromium nickel stainless steels which are superior to Type 302 in corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also...
Abstract
View article
PDF
AISI 304 and 304L are low-carbon chromium nickel stainless steels which are superior to Type 302 in corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-254. Producer or source: Stainless steel mills.
Journal Articles
Alloy Digest (1989) 38 (2): SS-103.
Published: 01 February 1989
... AISI TYPE 414 is a martensitic type stainless steel of intermediate hardness. It offers combined corrosion and heat resisting properties with high strength and toughness. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well...
Abstract
View article
PDF
AISI TYPE 414 is a martensitic type stainless steel of intermediate hardness. It offers combined corrosion and heat resisting properties with high strength and toughness. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-103. Producer or source: Stainless steel mills. Originally published May 1960, revised February 1989.
Journal Articles
Alloy Digest (1987) 36 (6): SS-486.
Published: 01 June 1987
... ARMCO 439 HIGH PERFORMANCE-10 is a ferritic stainless steel sheet and strip alloy suited to automotive-exhaust system applications where oxidatin resistance is needed at temperatures beyond the capability of AISI Type 409 to withstand. The alloy also has good resistance to wet chloride...
Abstract
View article
PDF
ARMCO 439 HIGH PERFORMANCE-10 is a ferritic stainless steel sheet and strip alloy suited to automotive-exhaust system applications where oxidatin resistance is needed at temperatures beyond the capability of AISI Type 409 to withstand. The alloy also has good resistance to wet chloride environments. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-486. Producer or source: Armco Inc., Specialty Steels Division.
Journal Articles
Alloy Digest (1987) 36 (4): SS-484.
Published: 01 April 1987
... Hardness 75.8 88.2 91.5 92.8 97.0 C 20.5 Table 3 - COMPARATIVE SHORT-TIME ELEVATED-TEMPERATURE TENSILE PROPERTIES Property Tensile strength, psi Yield strength (0.2?&offset). psi Alloy AlSl Type 409 ARMCO I8Cr-Cb HIGH PERFORMANCE-IO AISI Type 304 AISI Type 409 ARMCO 18Cr-Cb HIGH PERFORMANCE-IO AISI Type...
Abstract
View article
PDF
ARMCO 18Cr-Cb HIGH PERFORMANCE-10 a stabilized ferritic stainless steel. It has optimum forming consistency and very good oxidation and creep resistance. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, and tensile properties as well as deformation, and fatigue. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: SS-484. Producer or source: Armco Inc., Specialty Steels Division.
Journal Articles
Alloy Digest (1971) 20 (5): TS-233.
Published: 01 May 1971
... AISI Type P6 is a low-carbon, high-hardenability steel which is carburized and used for molding plastics. It develops a strong, wear-resistant case combined with a hard, tough core and is recommended for the most demanding mold requirements. This datasheet provides information on composition...
Abstract
View article
PDF
AISI Type P6 is a low-carbon, high-hardenability steel which is carburized and used for molding plastics. It develops a strong, wear-resistant case combined with a hard, tough core and is recommended for the most demanding mold requirements. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-233. Producer or source: Tool steel mills.
Journal Articles
Alloy Digest (1966) 15 (4): TS-178.
Published: 01 April 1966
... AISI Type H25 is a high-tungsten hot-work steel having heat resitance. It retains a high degree of working hardness at elevated temperatures. It is recommended for brass extrusion and forging dies, punches, cut-off knives, backet and dummy blocks. This datasheet provides information on composition...
Abstract
View article
PDF
AISI Type H25 is a high-tungsten hot-work steel having heat resitance. It retains a high degree of working hardness at elevated temperatures. It is recommended for brass extrusion and forging dies, punches, cut-off knives, backet and dummy blocks. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on high temperature performance as well as forming, heat treating, and machining. Filing Code: TS-178. Producer or source: Tool steel mills.
Journal Articles
Alloy Digest (1983) 32 (3): CS-93.
Published: 01 March 1983
... AISI 1141 is a resulfurized carbon steel containing nominally 1.50% manganese and 0.08-0.13% sulfur to give it free-machining characteristics. It has relatively low hardenability. Its ductility and toughness are fairly good in the longitudinal direction but tend to be low in the transverse...
Abstract
View article
PDF
AISI 1141 is a resulfurized carbon steel containing nominally 1.50% manganese and 0.08-0.13% sulfur to give it free-machining characteristics. It has relatively low hardenability. Its ductility and toughness are fairly good in the longitudinal direction but tend to be low in the transverse direction. It is highly recommended for high-production automatic-machine products. Among its many uses are screws, bolts, ball joints, spindles and light-duty gears. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on forming, heat treating, machining, joining, and surface treatment. Filing Code: CS-93. Producer or source: Carbon steel mills.
Journal Articles
Alloy Digest (1965) 14 (10): SS-173.
Published: 01 October 1965
... AISI Type 422 is a hardenable 12% chromium stainless steel recommended for applications requiring superior strength to Type 403 stainless steel at elevated temperatures. It retains high strength and exhibits excellent ductility over the temperature range from room to 1200 F. It is recommended...
Abstract
View article
PDF
AISI Type 422 is a hardenable 12% chromium stainless steel recommended for applications requiring superior strength to Type 403 stainless steel at elevated temperatures. It retains high strength and exhibits excellent ductility over the temperature range from room to 1200 F. It is recommended for turbine and jet engine components. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-173. Producer or source: Stainless steel mills.
1