Skip Nav Destination
Close Modal
Search Results for
AISI TYPE T5
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-14 of 14 Search Results for
AISI TYPE T5
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (1981) 30 (10): TS-389.
Published: 01 October 1981
... AISI Type T5 is a tungsten high-speed steel to which cobalt (8.9%) is added to provide high and unusual red hardness. It is particularly well adapted for heavy-duty cutting and high-production cutting tools. Because of its high red hardness, a cutting edge can be maintained under conditions...
Abstract
View article
PDF
AISI Type T5 is a tungsten high-speed steel to which cobalt (8.9%) is added to provide high and unusual red hardness. It is particularly well adapted for heavy-duty cutting and high-production cutting tools. Because of its high red hardness, a cutting edge can be maintained under conditions of speed, feed and depth of cut that would not be possible with ordinary high-speed steels. Typical applications of AISI Type T5 are lathe and planer tools, reamers, milling cutters and twist drills for heavy-duty cutting. This datasheet provides information on composition, physical properties, and hardness. It also includes information on forming, heat treating, machining, and surface treatment. Filing Code: TS-389. Producer or source: Tool steel mills.
Journal Articles
Alloy Digest (1978) 27 (11): SS-358.
Published: 01 November 1978
... threads 25-50 - 20-45 - Tooling Note: Use AISI Types T5 and M3 for single-point and bos tools, Types T5 and T15 for form and cut-off tools, Types Ml and Ml0 for taps and drills and Types T5 and M2 for reamers. Cutting speeds may be increased 2 to 3X with the use of Type C-2 carbide tooling. Coolants...
Abstract
View article
PDF
AL Tech 203EZ and 303EZ are non-magnetic, austenitic, free-machining stainless steels specifically designed for use in high-speed, automatic machining operations. These modifications retain, in so far as possible, the good mechanical properties and corrosion resistance of the basic compositions which they represent. Sulfur or selenium is added to produce the free-machining characteristics. Data are typical; do not use for specification or final design. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-358. Producer or source: AL Tech Specialty Steel Corporation.
Journal Articles
Alloy Digest (1986) 35 (1): CS-109.
Published: 01 January 1986
... surface finish in the quenched-and tempered condition. However. in the annealed condition and to some extent if normalized, there is a tendency for tearing which gives a poor surface finish. For turning AISI 1017 steel at I IO to I80 Brinell hardness with high-speed steels AISI Type M2 and AISI Type T5...
Abstract
View article
PDF
AISI 1017 is a carbon steel with a relatively low manganese content (0.30-0.60%); this contributes to relatively low hardenability in all applications and increased ductility with decreased hardness and strength in the core of carburized material and in uncarburized uses. It combines good hot and cold workability, good machinability and good weldability. Typical applications are carburized parts, bolts, trusses and cold-extruded parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: CS-109. Producer or source: Carbon steel mills.
Journal Articles
Alloy Digest (1978) 27 (12): SS-359.
Published: 01 December 1978
... 0.0023 0.0019 0.0065 0.0060 0.0055 0.0045 0.0050 0.0055 0.0055 0.0085 0.0035 - Tooling Note: Use AISI Types T5 and M3 for single-point and box tools, Types T5 and T15 for form and cut-off tools, Types Ml and Ml0 for taps and drills and Types T5 and M2 for reamers. Cut- ting speeds may be increased 2...
Abstract
View article
PDF
AL Tech 416EZ and 430F are magnetic, free-machining stainless steels specifically designed for use in high-speed, automatic machining operations. These modifications retain, in so far as possible, the good mechanical properties and corrosion resistance of the basic compositions which they represent. Sulfur is added to produce the free-machining characteristics. AL Tech 416EZ is a martensitic stainless steel and 430F is ferritic. Data are typical; do not use for specification or final design. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on high temperature performance as well as forming, heat treating, and machining. Filing Code: SS-359. Producer or source: AL Tech Specialty Steel Corporation.
Journal Articles
Alloy Digest (1980) 29 (10): CS-84.
Published: 01 October 1980
... and to some extent if normalized, there is a tendency for tearing which gives a poor surface finish. For turning SAE 1017 steel at 110 to 180 Brine11 hardness with high-speed steels AISI Type M2 and AISI Type T5 and single-point or box tools, use speed of 125 sfpm for roughing cuts of 0.150 in. with feed...
Abstract
View article
PDF
SAE 1017 is a carbon steel with a relatively low manganese content (0.30-0.60%) which contributes to relatively low hardenability in all applications and increased ductility with decreased hardness and strength in the core of carburized material and in uncarburized uses. It combines good hot and cold workability, good machinability and good weldability. Typical applications are carburized parts, bolts, trusses and cold-extruded parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: CS-84. Producer or source: Carbon steel mills.
Journal Articles
Alloy Digest (1979) 28 (6): SS-366.
Published: 01 June 1979
...) M2. T5, T15 Carbide Material Speed Feed Tool sfpm (m/s) ipr (mm/r) Material 165 (0.83) 0.012 (0.30) c-2 220 (1.10) 0.007 (0.18) c-3 DOI: 10.31399/asm.ad.ss0366 Copyright © ASM International® 1996 Table 4 - CORROSION DATA ON CARPENTER 18Cr-ZNi-12Mn AND AISI TYPE 304 (Annealed condition) Average...
Abstract
View article
PDF
CARPENTER STAINLESS 18Cr-2Ni-12Mn is a high-manganese, nitrogen-strengthened austenitic stainless steel with an excellent combination of toughness, ductility, strength, fabricability and corrosion resistance. It provides substantially higher yield and tensile strengths than AISI Type 304 and is comparable to Type 304 in corrosion resistance in many environments. It can be machined, cold worked, and welded using the same equipment and methods used for the conventional AISI 300 series austenitic stainless steels. It is nonmagnetic as annealed and after severe cold work. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-366. Producer or source: Carpenter.
Journal Articles
Alloy Digest (1990) 39 (10): TS-502.
Published: 01 October 1990
... CIRCLE C (AISI T5) tool steel combines increased wear resistance from higher vanadium and carbon contents with higher red hardness due to 8 to 9% cobalt content. This datasheet provides information on composition and hardness as well as fracture toughness, and deformation. It also includes...
Abstract
View article
PDF
CIRCLE C (AISI T5) tool steel combines increased wear resistance from higher vanadium and carbon contents with higher red hardness due to 8 to 9% cobalt content. This datasheet provides information on composition and hardness as well as fracture toughness, and deformation. It also includes information on wear resistance as well as heat treating and machining. Filing Code: TS-502. Producer or source: Teledyne Vasco.
Journal Articles
Alloy Digest (1986) 35 (2): CS-111.
Published: 01 February 1986
.... For turnmg PIISI I522 steel ar I35 to 190 Brine11 hard- ness with high-speed steels AISI Types M2and T5 and single-point or box tools. use speed of 125 sfpm for roughing cuts of 0. I50 in. with feed of 0.015 ipr: and use speed of 165 sfpm for finishing cuts of 0.025 in. with feed of 0.007 ipr. With brazed...
Abstract
View article
PDF
AISI 1522 is a low-carbon steel that combines good workability, good machinability and good weldability. It is used in the hot-rolled, annealed, normalized or water-quenched-and-tempered condition for a variety of applications. It also is used for parts case-hardened by carburizing. It has a relatively high manganese content; this provides increased hardenability which is reflected in all uses and gives increased strength and hardness in the core of carburized parts and in sections and components that have not been carburized. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: CS-111. Producer or source: Carbon steel mills.
Journal Articles
Alloy Digest (1971) 20 (2): CS-39.
Published: 01 February 1971
..., there is a tendency for tearing which gives a poor surface finish. For turning AISI 1020 steel at 100 to 150 Brinell hardness with high-speed steels M2 and T5 and single-point or box tools use speed of 125 sfpm for roughing cuts of 0.150 in. with feed of 0.015 ipr; and use speed of 165 sfpm for finishing cuts...
Abstract
View article
PDF
AISI 1020 is a low carbon steel combining good machinability, workability, and weldability. It is used for case-hardened components and for a wide range of applications in the hot-worked, cold-worked, normalized or quenched-and-tempered conditions. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: CS-39. Producer or source: Carbon and alloy steel mills.
Journal Articles
Alloy Digest (1957) 6 (5): TS-58.
Published: 01 May 1957
... or in the furnace. Pressurdie 2 should always be annealed after forging. Specification Equivalents: AISI Type H12 SAE Type H12 Potomac Crodi Cr-MO-W Chromow Dica B Latrobe LPD Thermold B Hotform 3 vulcan KM Allegheny Ludlum Atlas Bethlehem Crucible EZe Universal-Cyclops Vanadium Alloys vulcan General...
Abstract
View article
PDF
PRESSURDIE-2 is an intermediate chromium-tungsten-molybdenum hot die steel possessing excellent combination of properties particularly adapted for use in the aluminum extrusion industry. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on high temperature performance as well as forming, heat treating, and machining. Filing Code: TS-58. Producer or source: Continental Copper & Steel Industries Inc..
Journal Articles
Alloy Digest (1958) 7 (4): TS-69.
Published: 01 April 1958
... treatability joinability machinability MONARK-2 tensile properties workability MONARK-2 Filing Code: T5-69 Tool steel APRIL 1958 - DATA ON WORLD WIDE METALS AND ALLOYS psblisbd by Eneineenng Alloys Digest, Inc Upper MontcIair, New Jersey MONARK - 2 (Shock Resisting 5teel, Type S5) MONARK-2...
Abstract
View article
PDF
MONARK-2 is a silico-manganese, shock resisting tool steel, designed for applications where high toughness, at high hardness levels, is required to withstand severe impact. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-69. Producer or source: Atlas Steels Company.
Journal Articles
Alloy Digest (1987) 36 (9): TS-481.
Published: 01 September 1987
... TECH HURON* (High-Carbon, High-Chromium Die Steel; AISI Type D3) AL TECH HURON is a cold-work tool steel developed for applications requiring high resistance to wear or to abrasion and for re- sistance to heavy pressure rather than to sudden shock. Because of these qualities and its good nondeforming...
Abstract
View article
PDF
AL TECH HURON is a cold-work tool steel developed for applications requiring high resistance to wear or to abrasion and for resistance to heavy pressure rather than to sudden shock. Because of these qualities and its good nondeforming properties, it is unsurpassed (for an oil-hardening tool steel) for die work on long production runs. It has superior depth of hardening. Its many applications include cold trimmer dies, lamination dies, plug gages, slitting cutters and blanking, stamping and cold-forming dies and punches for long runs. This datasheet provides information on composition, physical properties, hardness, elasticity, and compressive strength as well as fracture toughness. It also includes information on forming, heat treating, and machining. Filing Code: TS-481. Producer or source: AL Tech Specialty Steel Corporation.
Journal Articles
Alloy Digest (1981) 30 (11): CS-87.
Published: 01 November 1981
...- ing which gives a poor surface finish. For turning SAP 1522 steel at 135 to 190 Brinell hard- ness with high-speed steels AISI Types M2 and T5 and single-point or box tools, use speed of 125 sfpm for roughing cuts of 0.150 in. with feed of 0.015 ipr; and use speed of 165 sfpm for ftishing cuts...
Abstract
View article
PDF
SAE 1522 is a low-carbon steel that combines good workability, good machinability and good weldability. It is used in the hot-rolled, annealed, normalized or water-quenched-and-tempered condition for a variety of applications. It also is used for parts case-hardened by carburizing. It has a relatively high manganese content (1.10-1.40%); this provides increased hardenability which is reflected in all uses and gives increased strength and hardness in the core of carburized parts and in sections and components that have not been carburized. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: CS-87. Producer or source: Carbon steel mills.
Journal Articles
Alloy Digest (1954) 3 (12): SS-22.
Published: 01 December 1954
... alkaline solutions, good resistsnce to oil refinery audes below 400°F., good resistance m mineral and vegetable oils, pwr resistance m am- monium and hot sulphite liquors. Specification Equivalentsz ASTM Al99, Al.0 ASTM A200, Al.8 ASTM A213, T5 ASTM Al58, P5a ASTM A132, F5 ASTM A193, B5 AISI Type 501 + MO...
Abstract
View article
PDF
USS 5, Type 501, and 5S, Type 502, contain approximately 5% chromium and 0.50% molybdenum. They resist corrosion and oxidation at elevated temperatures and are particularly adaptable to applications in the petroleum refinery industry. Type 502 contains slightly lower carbon and is used for applications where better weldability is required. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-22. Producer or source: United States Steel Corporation.