1-4 of 4 Search Results for

AISI TYPE H26

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1975) 24 (12): TS-294.
Published: 01 December 1975
... AISI Type H26 hot-work tool steel is the 18 tungsten-4 chromium-1 vanadium high-speed composition with lowered carbon to provide a high-degree of toughness. It has high red hardness and good resistance to abrasion. It is preferable to the conventional hot-work tool steels for applications in which...
Journal Articles
Alloy Digest (1969) 18 (12): TS-225.
Published: 01 December 1969
... in the preheating furnace and slowly cooling in the furnace. Specification Equivalents: AISI Type H26 SAE Type H26 General Characteristics: Special HS-55 is a tungsten-chromium-vanadium type high-speed steel with a carbon content of about 0.55%. It has high red-hardness and good abrasion resistance. It also has...
Journal Articles
Alloy Digest (1987) 36 (8): TS-479.
Published: 01 August 1987
.... insulating material. or dry sand. Following cooling, anneal before hardening. Specification Equivalents: AISI Type H26. ASTM A 68l(H-26). Federal QQ-T-57O(H-26). UNS No. T20826. General Characteristics: CLARITE HW26 is similar io composition to the I8 W-4 Cr-I V high-speed steel (AISI Type TI), except...
Journal Articles
Alloy Digest (1983) 32 (1): TS-410.
Published: 01 January 1983
... T20826 RED CUT SUPERIOR J Filing Code: TS-410 Tool Steel JANUARY 1983 - DATA ON WORLD WIDE METALS AND ALLOYS PlAbliddbU @ Copyright 1980. Engineering Publications, Inc. Ail rights reserved. MN: 002-614X RED CUT* SUPERIOR J (Hot-Work Tool Steel; AISI Type H26) RED CUT SUPERIOR J is a tungsten...