Alloy Digest (1985) 34 (6): TS-442.
Published: 01 June 1985
... AISI Type H10 is a hot-work tool steel of the chromium type, although it contains a substantial amount of molybdenum. It is a high-hardenability steel and possesses a combination of high tensile strength and hardness with excellent toughness. Typical hot work applications include forging dies...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1968) 17 (8): TS-209.
Published: 01 August 1968
... the last welding pass. Welding after hear ttearmenr of the ptoducr is not recommended. Specification Equivalents: AISI Type HI0 General Characteri sti cs: THERMOLD H10 (formerly Thetmold M) is a chtomium- molybdenum hot-work steel rhar exhibits excellenr re- sistance to softening at elevated tempetarutes...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1964) 13 (7): TS-149.
Published: 01 July 1964
... and inerc arc process. It is essential for best results co preheat at 6OOoF prior co welding and follow with a thorough post hearing at 14000F immediately after cbe last welding pass. Welding after beat cceacment of rhe product is nor recommended. Specification Equivalents: AISI Type HlO General Characteri...