Alloy Digest (1973) 22 (9): TS-262.
Published: 01 September 1973
... AISI Type A6 is an air-hardening high-carbon tool steel designed for a combination of high strength, good wear resistance, and good toughness. It is easy to heat treat with a minimum of distortion and is used extensively for plastic molds. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1987) 36 (3): TS-472.
Published: 01 March 1987
... 07050 (201) 761-1090 AL TECH APACHE* (Air-Hardening Die Steel; AISI Type A6) AL TECH APACHE is an air-hardening, cold-work die steel that exhibits less distortion during heat treatment than water or oil- hardening steels and most high-alloy. air-hardening die steels. Its low-distortion characteristic...
Journal Articles
Alloy Digest (1976) 25 (1): TS-295.
Published: 01 January 1976
... mica, or other insulating material. Weldability: Annealed or hardened-and-tempered tools and dies of Apache can be repair welded successfully, but extreme care must be taken, particularly with dies of complex design. AISI Type A6 ffier weld metal is recommended if the mechanical properties of the weld...
Journal Articles
Alloy Digest (1965) 14 (1): TS-157.
Published: 01 January 1965
... musr be taken in cooling co prevent cracking. Specification Equivalents: AISI Type A6 SAE Type A6 General Characteri sties: Jessair is a low-temperature, airhardening tool steel with dimensional scabiliry. Ic offers greater freedom from cracking during hardening especially in intricate sections...
Journal Articles
Alloy Digest (1963) 12 (3): TS-131.
Published: 01 March 1963
... temperature in furnace, ashes or lime. Weldability: Can be welded with relative ease in the hands of a competent operator. However, since it is an unusually deep hardening, air-hardening steel, special pre- cautions must be taken in cooling to prevent cracking. Specification Equivalents: AISI Type A6 SAE Type...
Journal Articles
Alloy Digest (1990) 39 (7): SA-448.
Published: 01 July 1990
... 1.35 max 0.04 max 0.05 max 0.4 max l/2 - 1 l/4 65 0.23 max 1.65 max 0.04 max 0.05 max 0.4 max l/2 65 0.26 max 1.35 max 0.04 max 0.05 max or l/2 65 0.21 max 1.65 max 0.04 max 0.05 max Sfrengthening elements: Type 1 0.005-0.05% columbium Type 2 0.01-0.15% vanadium Type 3 0.05max. columbium + vanadium24...
Journal Articles
Alloy Digest (1973) 22 (5): SA-46.
Published: 01 May 1973
... 46000 42000 40000 45000 Elongation (8 in min. % 18 I8 21 &tt - I9 Elongation (2 in min. $8; - 21 21 25 *Test specimens, procedures and elongation modifications shall conform to ASTM A6, A370 and A441; ASTM AS68 and A607. **The minimum yield point a&l tensile strength requirements of plates and bars...
Journal Articles
Alloy Digest (1959) 8 (12): TS-87.
Published: 01 December 1959
... marked hardness and brittleness in the fusion zone. Specification Equivalents: AISI Type L6 Fig? BetMeheol Allegheny Ludlum ElpaIOY e Tough No. 4 EFsE Jessop Universal-Cyclops General Characteristics: N&o-M is a chromium-nickel-molybdenum tool steel con- taining 0.70% carbon. This is a deep hardening...