Journal Articles
Alloy Digest (1988) 37 (6): SS-101.
Published: 01 June 1988
... AISI TYPE 440C is a hardenable high-carbon chromium steel designed to provide stainless properties with maximum hardness. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, and tensile properties. It also includes information on corrosion...
Journal Articles
Alloy Digest (1978) 27 (10): SS-356.
Published: 01 October 1978
... LESCALLOY BG42 VIM-VAR combines the tempering, hardness and hardness-retention characteristics of AISI M50 high-speed steel with the corrosion and oxidation resistance of AISI Type 440C stainless steel. LESCALLOY BG42 VIM-VAR is double vacuum melted (VIM, Vacuum Induction Melted; VAR, Vacuum Arc...
Journal Articles
Alloy Digest (1992) 41 (2): SS-179.
Published: 01 February 1992
... LESCALLOY BG42 VIM-VAR is a martensitic stainless high-speed steel that combines the temper resistance and hot hardness characteristics of M-50 high-speed steel with the corrosion resistance of AISI Type 440C stainless steel. (See also LESCALLOY BG42, Alloy Digest SS-280, October 1972...
Journal Articles
Alloy Digest (1989) 38 (11): SS-510.
Published: 01 November 1989
... 738 36 z 85-109 115-148 Table 5 - GALLING AND WEAR TEST PROPERTIES OF VARIOUS ALLOYS Threshold Galling Stress Volume Loss in 4000 Cycles, cu mm MOY Psi l*m 4-m Gall-Tough WOO* 103* 5 4 AISI Type 440C (Rockwell C56) 14 95 55 AISI Type 304 <;E 7** 2; 2.5 AISI Type 430 <1ooo** 7** 172 Testing at higher...
Journal Articles
Alloy Digest (1979) 28 (11): SS-370.
Published: 01 November 1979
... similar to those used for high-speed steels. It can be machined in the annealed condition with no unusual problems. It has good hot-working characteristics. Its corrosion resistance, in general, is similar to that of AISI Type 440C stainless steeL Scale can be removed from Carpenter CR&7 by blasting...
Journal Articles
Alloy Digest (1972) 21 (10): SS-280.
Published: 01 October 1972
.... In this regard it compares favorably with AISI Type 440C. General Characteristics: Lescalloy BG42 is essentially a martensitic stainless high-speed steel. It was developed for specialty applications requiring a combination of good corrosion resistance, wear resistance and resistance to softening at elevated...
Journal Articles
Alloy Digest (1993) 42 (9): SS-550.
Published: 01 September 1993
... in the fully annealed condition and has a machinability rating of 40 Venus the standard AISI B1112 as 100%. Typical feeds and speeds for this grade on various machining operations are shown in Table 5. Grinding and Polishing: Since AL Tech Type 440C pans gener- ally are heat treated to the full hardness...
Journal Articles
Alloy Digest (2012) 61 (8): SS-1125.
Published: 01 August 2012
... vanadium carbide content, the machinability and grindability of S90V will be slightly more difficult than that of D2 or 440C. Similar grinding equipment and practices are acceptable. SG type alumina wheels or CBN wheels have generally given the best performance with the CPM steels. Crucible Particle...
Journal Articles
Alloy Digest (1959) 8 (9): SS-93.
Published: 01 September 1959
... due to relief of residual stresses. Specification Equivalents: SAE 5144Oc AISI 44oc ASTM A314 Type 44OC General Characteristics: Allegheny Ludlum 440C is a general purpose hardenable stainless steel, which upon quenching develops maximum hardness together with high strength and corrosion resistana...
Journal Articles
Alloy Digest (2018) 67 (1): SS-1275.
Published: 01 January 2018
... of this alloy leads to very attractive corrosion resistance versus hardness properties. Processing similar to type 1.4034 (AISI 420) stainless steel; therefore, much easier than 1.4112/1.4125 (AISI 440B and 440C). Classification. Martensitic stainless steel with nitrogen addition. Product Forms Available Bars...
Journal Articles
Alloy Digest (1999) 48 (1): SS-736.
Published: 01 January 1999
... re- sistance. CPM 420V offers significant improvements over CPM 440V and other high chromium P/M and conventional tool steels in both wear and corrosion resistance. The wear and corrosion resistance of CPM 420V make it an ex- cellent candidate to replace CPM 440V or AISI 440C where in- creased wear...
Journal Articles
Alloy Digest (1975) 24 (6): SS-312.
Published: 01 June 1975
.... psi PROPERTIES Table 1 - ROOM-TEMPERATURE TENSILE PROPERTIES OF UNILOY 18-2 FM AND TWO OTHER STAINLESS STEELS Grade Tensile Yield Strength Strength (0.2% Offset) psi Psi Annealed Properties Uniloy 18-2 Fhl 70000 AISI Type 303 90000 AISI Type 416 7.5000 Cold-Drawn Properties Uniloy 18-2 FM 8.5000 AIS1...
Journal Articles
Alloy Digest (1976) 25 (1): SS-324.
Published: 01 January 1976
..., in these specific areas NITRONIC 33 is superior to AISI Type 304 stainless steel. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on low and high temperature performance, corrosion and wear...
Journal Articles
Alloy Digest (1969) 18 (11): SS-231.
Published: 01 November 1969
... AISI No. 617 is a general purpose hardenable stainless steel which can be heat treated to the highest hardness and strength level. It is recommended for many applications where corrosion and oxidation resistance coupled with high strength and wear resistance are required as in bearings, cams...
Journal Articles
Alloy Digest (2000) 49 (1): SS-774.
Published: 01 January 2000
... to that of AISI 420 and AISI 440C Applications: Injectible molds for corrosive plastics, rubber, and the medical and food industry; as extrusion dies; in plastic processing as screws, nozzles, and so on, and as engineering parts Producer: Uddeholm Corporation In Sweden: Rolling Meadows, IL 60008 Uddeholm Tooling...