Alloy Digest (1989) 38 (2): SS-103.
Published: 01 February 1989
... AISI TYPE 414 is a martensitic type stainless steel of intermediate hardness. It offers combined corrosion and heat resisting properties with high strength and toughness. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well...
Journal Articles
Alloy Digest (1982) 31 (9): SS-414.
Published: 01 September 1982
... CRUCIBLE XM 19 Stainless is a nitrogen-strengthened, low-carbon austenitic stainless steel that provides good corrosion resistance in combination with high strength. The alloy has better corrosion resistance than AISI Type 316 with approximately twice the yield strength. It can be welded, machined...
Journal Articles
Alloy Digest (1984) 33 (1): SS-438.
Published: 01 January 1984
.... Scale formation starts above 1200°F (649 C). It will discolor slightly at about 45O F (232°C) but scale does not form until I 200 F( 649 C) is exceeded. Specification Equivalents: ASTM A 276 and A 314 (Bars). ASTM A 580 (Wire). AISI Type 414. UNS No. S41400. AMS 5615. Federal QQ-S-763. SAE 5405 (51414...
Journal Articles
Alloy Digest (1972) 21 (12): SS-284.
Published: 01 December 1972
... worked readily by blanking, drawing, forming or heading. It has better cold-forming properties than AISI Type 414 stainless steel. Weldability: Carpenter Stainless No. 404 can be readily welded free from cracking without preheating or postheating. Be- cause it is air-hardening, it should be stress...
Journal Articles
Alloy Digest (1961) 10 (6): SS-118.
Published: 01 June 1961
..., such as sodium hydride, is strongly recommended, if this equipment is available. Specification Equivalents: SAE 51414 AISI Type 414 Fed. QQS-763 AMS 5615 USN 46S12 Cl. A & B MIL-S-861 Cl. A & B General Characteristics: Eoduro S-1 Nickel is a chromium rype marrensicic corrosion resisting steel to which nickel...
Journal Articles
Alloy Digest (1974) 23 (3): SS-293.
Published: 01 March 1974
.... The polishability of prehardened Crucible CSM 414 mold steel is outstanding and is ideally suited for optical finishes. Weldability: Crucible CSM 414 should be welded using either Crucible CSM 414 or Type 410 stainless electrode. In welding annealed Crucible CSM 414, the steel should be preheated to 4000F prior...
Journal Articles
Alloy Digest (1996) 45 (1): SS-633.
Published: 01 January 1996
... Crucible Maxel 2000 is a corrosion resistant, pre-hardened, free machining steel based on AISI 414 (Alloy Digest SS-103, February 1989) stainless steel. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information...
Journal Articles
Alloy Digest (1976) 25 (8): SS-332.
Published: 01 August 1976
... AQUAMET 18 is a low-nickel austenitic stainless steel having seawater corrosion resistance better than AISI Type 304 and approaching that of AISI Type 316 stainless steel. Its good strength and super toughness make it an ideal material for pleasure and work boats. This datasheet provides...
Journal Articles
Alloy Digest (1996) 45 (2): SS-637.
Published: 01 February 1996
...: Welding of Maxel 400 FM presents the same risks inherent in welding any hardened tool steel. Maxel400 FM should always be preheated to 6OOnOO F before welding. Type 410 or 414 stainless steel filler materials is recommended. Weld using light The introduction of new highly corrosive resins has led...
Journal Articles
Alloy Digest (1975) 24 (6): SS-312.
Published: 01 June 1975
.... psi PROPERTIES Table 1 - ROOM-TEMPERATURE TENSILE PROPERTIES OF UNILOY 18-2 FM AND TWO OTHER STAINLESS STEELS Grade Tensile Yield Strength Strength (0.2% Offset) psi Psi Annealed Properties Uniloy 18-2 Fhl 70000 AISI Type 303 90000 AISI Type 416 7.5000 Cold-Drawn Properties Uniloy 18-2 FM 8.5000 AIS1...
Journal Articles
Alloy Digest (2000) 49 (7): SS-798.
Published: 01 July 2000
... Armco Type 444 is a low-carbon, low-nitrogen, ferritic stainless steel that provides pitting and crevice corrosion resistance superior to that of most ferritic stainless steels. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also...
Journal Articles
Alloy Digest (1991) 40 (11): Co-82.
Published: 01 November 1991
... high even with severe working. Welding: MP35N alloy can be successfully TIC welded. Keep heat input per pass low (about l/2 to 2/3 that used to weld maraging steels or AISI Type 304 stainless). Joint efficiency of MP35N alloy is highest when performed on annealed material. If filler is required, use...
Journal Articles
Alloy Digest (1966) 15 (4): TS-178.
Published: 01 April 1966
... AISI Type H25 is a high-tungsten hot-work steel having heat resitance. It retains a high degree of working hardness at elevated temperatures. It is recommended for brass extrusion and forging dies, punches, cut-off knives, backet and dummy blocks. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1979) 28 (10): SS-368.
Published: 01 October 1979
... CARPENTER STAINLESS TYPE 304HN is essentially a high-nitrogen version of AISI Type 304 stainless steel. By means of solid-solution strengthening, the nitrogen provides significantly higher yield strength and tensile strength as annealed than conventional Type 304, without adversely affecting...
Journal Articles
Alloy Digest (1983) 32 (6): TS-414.
Published: 01 June 1983
... rights reserved. ISSN: 002-614X Alloy Digest. Inc. Post Office Box 823 Upper Montclair, New Jersey GUTERL* S-7 (Shock-Resisting Tool Steel; AlSl Type S7) GUTERL S-7 is a chromium-molybdenum, general-purpose. air-hardening tool steel recommended for uses where shock resistance. good hot-work properties...
Journal Articles
Alloy Digest (2004) 53 (3): SS-901.
Published: 01 March 2004
... Type 441 is a fully ferritic stainless steel with extra-low carbon and nitrogen contents. The alloy is resistant to stress-corrosion cracking and also has corrosion properties comparable to AISI type 316. Type 441 has a high yield strength, good weldability, and good formability. This datasheet...
Journal Articles
Alloy Digest (1980) 29 (7): SS-275.
Published: 01 July 1980
... CARPENTER STAINLESS No. 5-F is a modification of AISI Type 416 stainless steel and was designed for an optimum combination of machinability and corrosion resistance. It comprises a specially balanced analysis and is essentially non-hardenable. It is recommended for all screw-machine applications...
Journal Articles
Alloy Digest (1965) 14 (5): SS-169.
Published: 01 May 1965
... at 540-65OoC(lOOO-12OOoF) cool in air or oil. Machinability: Sub-critical annealing is ordinarily done for best machinability. Fair machinability rating about 50% of AISI B1112 Bessemer screw stock. It is easier to machine than Type 18-8 stainless steel, but there is a tendency to gall or build up...
Journal Articles
Alloy Digest (1956) 5 (9): SS-47.
Published: 01 September 1956
... CARPENTER STAINLESS No. 2 is a high carbon heat-treatable chromium stainless steel equivalent to AISI Type 420; while No. 2-FM is the free-machining modification equivalent to AISI Type 420-F. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1990) 39 (4): SS-304.
Published: 01 April 1990
... machines with good surface f&h. It is more susceptible to work hardening than AISI Type 304 or 316 and should be machined at slower speeds and higher feeds. Itsmachinabilityratingisabout21%thatofAISIB1112carbon steel. Coated carbide tools will permit higher cutting rates. Working: Forge NITRON IC 50...