Skip Nav Destination
Close Modal
Search Results for
AISI TYPE 314
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 74
Search Results for AISI TYPE 314
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Journal Articles
Alloy Digest (1988) 37 (10): SS-100.
Published: 01 October 1988
... AISI TYPE 314 is an austenitic chromium-nickel stainless steel with the highest heat resisting properties of any of the chromium-nickel steels. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness...
Abstract
View articletitled, <span class="search-highlight">AISI</span> <span class="search-highlight">TYPE</span> <span class="search-highlight">314</span>: Heat Resistant Stainless Steel
View
PDF
for article titled, <span class="search-highlight">AISI</span> <span class="search-highlight">TYPE</span> <span class="search-highlight">314</span>: Heat Resistant Stainless Steel
AISI TYPE 314 is an austenitic chromium-nickel stainless steel with the highest heat resisting properties of any of the chromium-nickel steels. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-100. Producer or source: Stainless steel mills. Originally published February 1960, revised October 1988.
Journal Articles
Alloy Digest (1977) 26 (2): TS-314.
Published: 01 February 1977
... Code: TS-314 Tool Steel FEBRUARY 1977 - DATA ON WORLD WIDE METALS AND ALLOYS Pablisbd by AISI Type Ml Engineering Alloys Digest. Inc Upper Montclair, New Jetsq (High-Speed Tool Steel) AISI Type Ml is a general-purpose high-molybdenum, low-tungsten type of high-speed tool steel. It has an excellent...
Abstract
View articletitled, <span class="search-highlight">AISI</span> <span class="search-highlight">TYPE</span> M1: High-Speed Tool Steel
View
PDF
for article titled, <span class="search-highlight">AISI</span> <span class="search-highlight">TYPE</span> M1: High-Speed Tool Steel
AISI Type M1 is a general-purpose high-molybdenum, low-tungsten type of high-speed tool steel. It has an excellent combination of cutting ability, toughness and finishing properties. Its cutting ability is good except for heavy-duty, continuous cutting operations where the ultimate in red-hardness is required. Its toughness is as great as that of any other high-speed steel. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on forming, heat treating, and machining. Filing Code: TS-314. Producer or source: Tool steel mills.
Journal Articles
Alloy Digest (2005) 54 (8): SS-937.
Published: 01 August 2005
... Sirius 314 is a high-temperature stainless steel with the elements of silicon, cerium, and lanthanum added for better oxidation resistance compared to AISI Type 310. Applications are in burners, recuperators, and ducts. This datasheet provides information on composition, physical properties...
Abstract
View articletitled, SIRIUS <span class="search-highlight">314</span>: Heat-Resisting Stainless Steel
View
PDF
for article titled, SIRIUS <span class="search-highlight">314</span>: Heat-Resisting Stainless Steel
Sirius 314 is a high-temperature stainless steel with the elements of silicon, cerium, and lanthanum added for better oxidation resistance compared to AISI Type 310. Applications are in burners, recuperators, and ducts. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming and joining. Filing Code: SS-937. Producer or source: Industeel USA, LLC.
Journal Articles
Alloy Digest (1955) 4 (6): SS-30.
Published: 01 June 1955
... which will apply to all smite conditions. Specification Equivalents: MIL-S-854 Cl. 11 ML-S-862A Cl. 11 ASTM A314 Ty. 314 ASTM A297 Gr. HK (cast > ME-60310 ASTM Al67 Gr. 10 AISI 314 General Characteristics: In this grade, the standard 25-20, Type 310, has been varied by the addition of silicon to impart...
Abstract
View articletitled, ALLEGHENY METAL 25-20B: Heat and Corrosion Resistant Steel, <span class="search-highlight">Type</span> <span class="search-highlight">314</span>
View
PDF
for article titled, ALLEGHENY METAL 25-20B: Heat and Corrosion Resistant Steel, <span class="search-highlight">Type</span> <span class="search-highlight">314</span>
ALLEGHENY METAL 25-20B is an austenitic chromium-nickel stainless steel with the highest oxidation resistance of any of the chromium-nickel steels. It has been developed from AISI 310 by raising the silicon content in order to improve the resistance to oxidation and the resistance to carburization. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-30. Producer or source: Allegheny Ludlum Corporation.
Journal Articles
Alloy Digest (1991) 40 (9): TS-32.
Published: 01 September 1991
... I201477-9161 Lmsshownsre&picsLnmmbsussdkn 27 Canfiid Streets Orange, NJ. 07050 I U.S.A spsc#kation w fd &sign. SOLAR TOOL STEEL (Water Hardening Tool Steel, AISI Type S2) SOLAR TOOL STEEL is a very tough water hardening tool steel. Even at Rockwell C 59/60, it will bend before breaking. In medium...
Abstract
View articletitled, SOLAR TOOL STEEL: Water Hardening Tool Steel, <span class="search-highlight">Type</span> S2
View
PDF
for article titled, SOLAR TOOL STEEL: Water Hardening Tool Steel, <span class="search-highlight">Type</span> S2
SOLAR TOOL STEEL is a very tough water hardening tool steel. Even at Rockwell C 59/60, it will bend before breaking. If medium and large sections, the steel develops a hard case and tough core when hardened. This datasheet provides information on composition, physical properties, and hardness. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-32. Producer or source: Carpenter. Originally published as Solar, April 1955, revised September 1991.
Journal Articles
Alloy Digest (1990) 39 (6): TS-501.
Published: 01 June 1990
... TOOL STEEL Filing Code: Tool Steel TS-501 - DIGEST- DATA ON WORLD WIDE METALS AND ALLOYS JUNE 1990 eyight 1990. Al& LXgest. Inc. All rights mwvd PdMby: Alloy Oiiet, Inc. /201-677-9161 y!g No. 484* TOOL STEEL 27 CatWield Stmel. Orange. N.J. 07050 I U.S.A. (Air Hardening Tool Steel: AISI Type A2) No. 484...
Abstract
View articletitled, No. 484 TOOL STEEL: Air Hardening Tool Steel, <span class="search-highlight">Type</span> A2
View
PDF
for article titled, No. 484 TOOL STEEL: Air Hardening Tool Steel, <span class="search-highlight">Type</span> A2
No. 484 tool steel is an air hardening tool steel capable of through hardening in heavy sections. Isothermal transformation of material austenitized at 1750 starts after about 400 seconds at 1300 F and after about 1000 seconds at 600 F. The calculated Ms temperature is 325 F. The steel has a good hardness/toughness balance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on wear resistance as well as forming, heat treating, and machining. Filing Code: TS-501. Producer or source: Carpenter.
Journal Articles
Alloy Digest (1956) 5 (10): SA-49.
Published: 01 October 1956
... AISI 8630 is a chromium, nickel, molybdenum alloy steel. It is of the moderate deep hardening type and develops high toughness at high tempering temperatures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture...
Abstract
View articletitled, <span class="search-highlight">AISI</span> 8630: Triple Alloy Steel
View
PDF
for article titled, <span class="search-highlight">AISI</span> 8630: Triple Alloy Steel
AISI 8630 is a chromium, nickel, molybdenum alloy steel. It is of the moderate deep hardening type and develops high toughness at high tempering temperatures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on low temperature performance as well as forming, heat treating, machining, and joining. Filing Code: SA-49. Producer or source: Alloy steel mills and foundries.
Journal Articles
Alloy Digest (1975) 24 (6): SS-312.
Published: 01 June 1975
.... psi PROPERTIES Table 1 - ROOM-TEMPERATURE TENSILE PROPERTIES OF UNILOY 18-2 FM AND TWO OTHER STAINLESS STEELS Grade Tensile Yield Strength Strength (0.2% Offset) psi Psi Annealed Properties Uniloy 18-2 Fhl 70000 AISI Type 303 90000 AISI Type 416 7.5000 Cold-Drawn Properties Uniloy 18-2 FM 8.5000 AIS1...
Abstract
View articletitled, UNILOY 18-2 FM: Free Machining, Corrosion Resistant Stainless Steel
View
PDF
for article titled, UNILOY 18-2 FM: Free Machining, Corrosion Resistant Stainless Steel
UNILOY 18-2 FM is a ferritic stainless steel designed to offer an optimum combination of machinability and corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-312. Producer or source: Cyclops.
Journal Articles
Alloy Digest (1991) 40 (6): TS-344.
Published: 01 June 1991
... will machine somewhat easierthanthe18-4-1 type(AISITypeTl).Ithasama&nabEity rating of about 45% of a 1% carbon tool steel or 33% of AISI B1112 screw stock. See Table 2 for suggested machming param- eters. Workability: For forging Ten Star high-speed steel preheat very slowly to 1500/1600°F (816/871OC...
Abstract
View articletitled, CARPENTER TEN STAR HIGH-SPEED STEEL: High-Speed Steel, <span class="search-highlight">Type</span> M10
View
PDF
for article titled, CARPENTER TEN STAR HIGH-SPEED STEEL: High-Speed Steel, <span class="search-highlight">Type</span> M10
CARPENTER TEN STAR is a general-purpose molybdenum-bearing high-speed steel. Its excellent wear and cutting properties are the result of its high percentages of carbon and vanadium. It is produced by the ESR (Electro Slag Remelting) process. This datasheet provides information on composition and hardness as well as deformation. It also includes information on forming, heat treating, and machining. Filing Code: TS-344. Producer or source: Carpenter. Originally published as Carpenter Ten Star, January 1979, revised June 1991.
Journal Articles
Alloy Digest (1976) 25 (3): TS-298.
Published: 01 March 1976
... Copyright © ASM International® 1996 1996 ASM International abrasion resistance AISI TYPE F2 chemical composition dies elasticity finishing tools hardness heat treatability machinability physical properties reamers wear resistance workability AISI Type F2 Filing Code: TS-298 Tool Steel...
Abstract
View articletitled, <span class="search-highlight">AISI</span> <span class="search-highlight">TYPE</span> F2: Water Hardening Tool Steel
View
PDF
for article titled, <span class="search-highlight">AISI</span> <span class="search-highlight">TYPE</span> F2: Water Hardening Tool Steel
AISI is a water-hardening tool steel that resists wear and abrasion from four to ten times longer than plain carbon tool steels. When hardened, it acquires a hard-slippery surface that is difficult to scratch. Its many uses for tools include dies for a variety of products, reamers and finishing tools. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, and surface treatment. Filing Code: TS-298. Producer or source: Tool steel mills.
Journal Articles
Alloy Digest (1978) 27 (11): SS-358.
Published: 01 November 1978
... threads 25-50 - 20-45 - Tooling Note: Use AISI Types T5 and M3 for single-point and bos tools, Types T5 and T15 for form and cut-off tools, Types Ml and Ml0 for taps and drills and Types T5 and M2 for reamers. Cutting speeds may be increased 2 to 3X with the use of Type C-2 carbide tooling. Coolants...
Abstract
View articletitled, AL TECH 203EZ and 303EZ: Free Machining Austenitic Stainless Steel
View
PDF
for article titled, AL TECH 203EZ and 303EZ: Free Machining Austenitic Stainless Steel
AL Tech 203EZ and 303EZ are non-magnetic, austenitic, free-machining stainless steels specifically designed for use in high-speed, automatic machining operations. These modifications retain, in so far as possible, the good mechanical properties and corrosion resistance of the basic compositions which they represent. Sulfur or selenium is added to produce the free-machining characteristics. Data are typical; do not use for specification or final design. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-358. Producer or source: AL Tech Specialty Steel Corporation.
Journal Articles
Alloy Digest (1986) 35 (2): SS-424.
Published: 01 February 1986
... ARMCO 12 SR was developed specifically for automotive exhaust applications. It has greater oxidation resistance than AISI Type 409 and it exhibits formability and weldability comparable to more highly alloyed ferritic grades. This datasheet provides information on composition, physical properties...
Abstract
View articletitled, ARMCO 12 SR: Ferritic Stainless Steel
View
PDF
for article titled, ARMCO 12 SR: Ferritic Stainless Steel
ARMCO 12 SR was developed specifically for automotive exhaust applications. It has greater oxidation resistance than AISI Type 409 and it exhibits formability and weldability comparable to more highly alloyed ferritic grades. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-424. Producer or source: Armco Inc., Eastern Steel Division. Originally published April 1983, revised February 1986.
Journal Articles
Alloy Digest (1981) 30 (6): SS-387.
Published: 01 June 1981
... CRUCIBLE 303 PLUS-X is a non-hardenable austenitic chromium-nickel steel to which elements have been added to improve machinability and non-galling characteristics. Better machinability than that of standard AISI Type 303 stainless is obtained by the use of higher manganese content to give...
Abstract
View articletitled, CRUCIBLE 303 PLUS-X: Austenitic Stainless Steel
View
PDF
for article titled, CRUCIBLE 303 PLUS-X: Austenitic Stainless Steel
CRUCIBLE 303 PLUS-X is a non-hardenable austenitic chromium-nickel steel to which elements have been added to improve machinability and non-galling characteristics. Better machinability than that of standard AISI Type 303 stainless is obtained by the use of higher manganese content to give a uniquely soft and machinable sulfide inclusion. This grade is non-magnetic in the annealed condition but slightly magnetic when cold worked. Typical applications are screw machine products and all machined parts requiring good corrosion resistance or non-magnetic properties. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-387. Producer or source: Crucible Specialty Metals Division, Colt Industries.
Journal Articles
Alloy Digest (1961) 10 (12): SS-126.
Published: 01 December 1961
... AISI Types 303 and 303 Se austenitic chromium nickel stainless steels to which elements have been added to improve machining and non-seizing characteristics. They are the most readily machinable of all the austenitic chromium nickel grades and are suitable for use in automatic screw machines...
Abstract
View articletitled, <span class="search-highlight">AISI</span> <span class="search-highlight">TYPE</span> 303 and 303Se: Free Cutting Stainless Steel
View
PDF
for article titled, <span class="search-highlight">AISI</span> <span class="search-highlight">TYPE</span> 303 and 303Se: Free Cutting Stainless Steel
AISI Types 303 and 303 Se austenitic chromium nickel stainless steels to which elements have been added to improve machining and non-seizing characteristics. They are the most readily machinable of all the austenitic chromium nickel grades and are suitable for use in automatic screw machines. They are widely used to minimize seizing and galling. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-126. Producer or source: Stainless steel mills.
Journal Articles
Alloy Digest (1987) 36 (8): SS-488.
Published: 01 August 1987
.... Specification Equivalents: AISI Type 316. UNS No. S31600. Plate, sheet and strip: ASTM A 167 & A 240. Bar: ASTM A 276, A 314 & A 479. Forgings: ASTM 473. SAE 5405 (30316). There are many more: See UNS No. S31600, p. 223, Unified Numbering System, fourth ed., 1985. General Characteristics: Jessop Type 316...
Abstract
View articletitled, JESSOP <span class="search-highlight">TYPE</span> 316: Austenitic Stainless Steel, <span class="search-highlight">Type</span> 316
View
PDF
for article titled, JESSOP <span class="search-highlight">TYPE</span> 316: Austenitic Stainless Steel, <span class="search-highlight">Type</span> 316
JESSOP Type 316 is a molybdenum-bearing austenitic chromium-nickel stainless steel with greatly increased resistance to pitting and crevice corrosion in comparison with AISI Type 304 stainless steel. In addition, Jessop Type 316 offers superior creep, stress-to-rupture and tensile strengths at elevated temperatures. Type 316 is suitable for a wide range of applications in chemical and petroleum processing, power plants, pollution-control equipment, pulp and paper plants and food and pharmaceutical processing. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-488. Producer or source: Jessop Steel Company.
Journal Articles
Alloy Digest (1985) 34 (10): SS-73.
Published: 01 October 1985
... AISI TYPE 410 is a hardenable 12% chromium stainless steel. It offers a wide range of mechanical properties and has good resistance to corrosion and oxidation. It can be hardened readily by austenitizing and air cooling. Among its many applications are knives, mechanical blades and other cutting...
Abstract
View articletitled, <span class="search-highlight">AISI</span> <span class="search-highlight">TYPE</span> 410: Corrosion and Heat Resistant Steel
View
PDF
for article titled, <span class="search-highlight">AISI</span> <span class="search-highlight">TYPE</span> 410: Corrosion and Heat Resistant Steel
AISI TYPE 410 is a hardenable 12% chromium stainless steel. It offers a wide range of mechanical properties and has good resistance to corrosion and oxidation. It can be hardened readily by austenitizing and air cooling. Among its many applications are knives, mechanical blades and other cutting tools for numerous corrosive environments. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-73. Producer or source: Stainless steel mills. Originally published April 1958, revised October 1985
Journal Articles
Alloy Digest (1982) 31 (2): SS-402.
Published: 01 February 1982
... solution at 140OF. Specification Equivalents: AISI Type 405. UNS No. S40500. ASTM: A 276, A 314 and A 479. General Characteristics: Uniloy 405 is a ferritic stainless steel which, unlike other 12% chromium steels, is not subject to appreciable hardening through air cooling from high temperatures. This non...
Abstract
View articletitled, UNILOY 405: Non Hardenable Stainless Steel
View
PDF
for article titled, UNILOY 405: Non Hardenable Stainless Steel
UNILOY 405 is a non-hardening modification of the 12% chromium stainless steel, AISI Type 410. A small addition of aluminum (about 0.20%) restricts the formation of austenite at high temperature so that hardening does not occur upon quenching. This characteristic makes Uniloy 405 especially suited for welding; the welds are ductile and there is no need for controlled cooling rates. Applications of Uniloy 405 include all types of welded structures that cannot be annealed after welding. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-402. Producer or source: Cyclops.
Journal Articles
Alloy Digest (1980) 29 (12): SS-378.
Published: 01 December 1980
... CRUCIBLE 316 PLUS is a non-hardenable austenitic chromium-nickel steel with superior corrosion and heat resisting qualities. Better machinability than that of standard AISI Type 316 stainless is obtained by the use of balanced chemistry and special manufacturing techniques. This grade is non...
Abstract
View articletitled, CRUCIBLE 316 PLUS: Austenitic Stainless Steel
View
PDF
for article titled, CRUCIBLE 316 PLUS: Austenitic Stainless Steel
CRUCIBLE 316 PLUS is a non-hardenable austenitic chromium-nickel steel with superior corrosion and heat resisting qualities. Better machinability than that of standard AISI Type 316 stainless is obtained by the use of balanced chemistry and special manufacturing techniques. This grade is non-magnetic in the annealed condition but slightly magnetic when cold worked. Typical applications are screw machine products and all machined parts requiring good corrosion resistance or non-magnetic properties. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-378. Producer or source: Crucible Specialty Metals Division, Colt Industries.
Journal Articles
Alloy Digest (1982) 31 (5): SS-407.
Published: 01 May 1982
... AISI Type 446 is a high-chromium (nominally 25%), ferritic, heat-resistant alloy with excellent resistance to oxidation and to various forms of hot corrosion. The alloy is used most commonly for service between 1500 and 2200 F (815 and 1200 C), although its elevated-temperature strength is quite...
Abstract
View articletitled, <span class="search-highlight">AISI</span> <span class="search-highlight">TYPE</span> 446: Ferritic Stainless Steel
View
PDF
for article titled, <span class="search-highlight">AISI</span> <span class="search-highlight">TYPE</span> 446: Ferritic Stainless Steel
AISI Type 446 is a high-chromium (nominally 25%), ferritic, heat-resistant alloy with excellent resistance to oxidation and to various forms of hot corrosion. The alloy is used most commonly for service between 1500 and 2200 F (815 and 1200 C), although its elevated-temperature strength is quite low. Among its many applications are combustion chambers, kiln linings, oil-burner components and annealing boxes. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-407. Producer or source: Stainless steel mills.
Journal Articles
Alloy Digest (1975) 24 (2): SS-305.
Published: 01 February 1975
... USS 18-8S (AISI Type 304) and USS 18-8I (AISI Type 304L) are austenitic chromium-nickel steels that are easy to fabricate and weld. They combine high strength with excellent stability and shock resistance, even at cryogenic temperatures. This datasheet provides information on composition, physical...
Abstract
View articletitled, USS 18-8S and 18-8L: Austenitic Stainless Steels
View
PDF
for article titled, USS 18-8S and 18-8L: Austenitic Stainless Steels
USS 18-8S (AISI Type 304) and USS 18-8I (AISI Type 304L) are austenitic chromium-nickel steels that are easy to fabricate and weld. They combine high strength with excellent stability and shock resistance, even at cryogenic temperatures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on low temperature performance and corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-305. Producer or source: United States Steel Corporation.