Alloy Digest (1988) 37 (9): SS-99.
Published: 01 September 1988
... AISI Type 302 is a general purpose austenitic chromium-nickel stainless steel. It has high resistance to corrosion and heat. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also...
Journal Articles
Alloy Digest (1978) 27 (8): SS-354.
Published: 01 August 1978
... UCAR 302 is a cryogenically processed stainless steel wire with the same composition as AISI Type 302. The processing gives tensile and torsional properties that are independent of wire diameter and markedly greater than those of conventional stainless steels. UCAR 302 has uniformly high...
Journal Articles
Alloy Digest (1980) 29 (4): SS-372.
Published: 01 April 1980
... CRYOTECH 302 is a new, cryogenically processed stainless steel wire with the same composition as AISI Type 302. The cryogenic processing gives tensile and torsional properties that are independent of wire diameter (thus simplifying spring design calculations) and markedly greater than those of...
Journal Articles
Alloy Digest (1990) 39 (3): SS-159.
Published: 01 March 1990
... AISI TYPE 202 is an austenitic manganese type stainless steel having similar mechanical properties and corrosion resistance as AISI TYPE 302 stainless steel. It is a general purpose, non-hardenable corrosion resisting steel. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1957) 6 (12): SS-65.
Published: 01 December 1957
... ENDURO 202 is a non-hardenable austenitic chromium-nickel-manganese stainless steel having similar mechanical properties and corrosion resistance to AISI Type 302 stainless steel. It is a general purpose corrosion resisting steel. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2005) 54 (7): SS-935.
Published: 01 July 2005
... Sandvik 13RM19 combines high mechanical strength with a nonmagnetic structure. This combination of properties has previously been found mainly in Co-Ni-base or Cu-Be alloys. The steel has very good corrosion resistance comparable to that of AISI Type 302. This datasheet provides information on...
Journal Articles
Alloy Digest (2000) 49 (4): SS-779.
Published: 01 April 2000
...: Immerse in a solution of 10% sulfuric, 10% hydrochloric acid at about 82 °C (180 °F) to soften oxide scale. Then dip for a short time in warm 5 10% nitric acid to whiten the surface and pro- mote passivity. Machinability: AISI type 302 work hardens readily; therefore, tools must not ride surface without...
Journal Articles
Alloy Digest (1984) 33 (4): SS-443.
Published: 01 April 1984
... particles. After parts are finished they should be passivated for 30 minutes in a solution of 20% by volume nitrtc acid at l20/ 140°F (49 6O C). Rinse thoroughly in water. Scaling: Carpenter Stainless Type 302 has excellent scale resistance up to 16OO F (87l C). Specification Equivalents: AISI Type 302...
Journal Articles
Alloy Digest (1968) 17 (11): SS-216.
Published: 01 November 1968
... machinability physical properties plastic industry tensile properties textile industry welded equipment workability FAGERSTA-R320 Filing Code: 35-216 Stainless Steel - DATA ON WORLD WIDE METALS AND ALLOYS NOVEMBER 1968 Pvblisbd by FAGERSTA-R320 (Stainless Steel - Type 302) Engineering Alloys Digest...
Journal Articles
Alloy Digest (1962) 11 (6): SS-132.
Published: 01 June 1962
... AISI Type 302B is an austenitic chromium nickel stainless steel which has a resistance to scaling at elevated temperatures superior to Type 302. It is used exclusively for parts which are exposed to high temperatures in service. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1964) 13 (4): SS-154.
Published: 01 April 1964
... AISI Type 305 is an austenitic chromium nickel stainless steel with lower rate of work hardening than Type 302 or 304 and less change of magnetic permeability when cold worked. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as...
Journal Articles
Alloy Digest (1971) 20 (5): SS-254.
Published: 01 May 1971
... AISI 304 and 304L are low-carbon chromium nickel stainless steels which are superior to Type 302 in corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also...
Journal Articles
Alloy Digest (1982) 31 (5): TS-399.
Published: 01 May 1982
... area will be hard and brittle. it is desirable to anneal as soon as possible after welding. If a nonhardening weld deposit is desired, AISI Types 302 or 310 stainless steel electrodes may be used, but the base metal will still be hard in the heat-affected zone and annealing or stress relieving should...
Journal Articles
Alloy Digest (1989) 38 (2): SS-103.
Published: 01 February 1989
... AISI TYPE 414 is a martensitic type stainless steel of intermediate hardness. It offers combined corrosion and heat resisting properties with high strength and toughness. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well...
Journal Articles
Alloy Digest (1969) 18 (7): SS-227.
Published: 01 July 1969
... AISI Type 430 is a ductile, non-hardenable type of stainless steel recommended for parts requiring a combination of good formability, weldability and corrosion resistance. It is used for architectural trim, food and dairy handling equipment, chemical and oil refinery plant equipment. This...
Journal Articles
Alloy Digest (1965) 14 (10): SS-173.
Published: 01 October 1965
... AISI Type 422 is a hardenable 12% chromium stainless steel recommended for applications requiring superior strength to Type 403 stainless steel at elevated temperatures. It retains high strength and exhibits excellent ductility over the temperature range from room to 1200 F. It is recommended for...
Journal Articles
Alloy Digest (1971) 20 (1): TS-232.
Published: 01 January 1971
... AISI Type L6 is recommended for tools, dies and machine parts which must develop a rather high degree of hardness, wear resistance and compressive strength combined with toughness. This datasheet provides information on composition, hardness, elasticity, and tensile properties. It also includes...
Journal Articles
Alloy Digest (1972) 21 (9): TS-246.
Published: 01 September 1972
... AISI Type S1 is a chromium-tungsten alloy steel for general use for chisels and other cold-battering tools. Its great toughness and strength also enable it to handle many hot and cold-work tooling jobs. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1965) 14 (11): SS-174.
Published: 01 November 1965
...-temperature alloys joinability machinability physical properties tensile strength workability AN Type 201 Filing Code: 55-174 Stainless Steel NOVEMBER 1965 -DATA ON WORLD WIDE METALS AND ALLOYS AIS1 Type 201 (Stainless Steel) PsbhbdbY Engineering AIIOYS Die& Ix Upper Montdair, Ner Jarcr AISI 201 is a...
Journal Articles
Alloy Digest (1969) 18 (10): SS-230.
Published: 01 October 1969
... AISI Type 309 is a chromium-nickel, austenitic, heat and corrosion resisting steel recommended for high temperature applications in corrosive environments. It is intended primarily for high temperature applications at 1500 F or higher, where resistance to oxidation and/or corrosion is required...