Journal Articles
Alloy Digest (1986) 35 (11): SS-478.
Published: 01 November 1986
... AISI No. 651 is an austenitic iron-base superalloy with a relatively high ratio of strength to alloying element content. It is capable of withstanding high static and dynamic stresses through at least 1200 F. It is used for various high-temperature applications such as components for jet engines...
Journal Articles
Alloy Digest (1987) 36 (5): SS-485.
Published: 01 May 1987
... under intermittent operation up to 145O F (788OC). Specification Equivalents: AMS 5526; 5527; 5720: 5721 and 5722. AISI No. 651. UNS No. S63198. .ASTM: A 453 (651). A 457 (651). .A 458 (651) and A 477 (651). SAE 5467 (l9-9DL). General Characteristics: CARPENTER 19-9 DL was designed primarily for scrticc...
Journal Articles
Alloy Digest (2007) 56 (6): TS-651.
Published: 01 June 2007
... 31.0 17.9 Fig. 1 Tempering diagram See also Fig. 1 and 2. DOI: 10.31399/asm.ad.ts0651 Fig. 2 Time-temperature- transformation (TTT) diagram Specification Equivalents: AISI Type 6F7 BS M30 Werkstoff No. 1.2767 General Characteristics: Thyrodur 2767/2767 Supra has high hardenability and toughness...
Journal Articles
Alloy Digest (1997) 46 (1): TS-549.
Published: 01 January 1997
... as a volume loss as required by the ASTM smndard. Note, therefore, that a lower number indicates better wear t&stance. Specification Equivalents: AISI Type T15 UNS T12015 Time--Seconds (Log Scale) Fs 2 Isakml uaas-n diagnm for Caqemr MiamMdr T-15 aby. A-1260OC General Characteristics: Carpemer Micro-Melt T-15...
Journal Articles
Alloy Digest (1996) 45 (7): TS-542.
Published: 01 July 1996
... response to heat neatma& greata== resistance, and kreased toughness of the finished tool. The ahoy is the equivalent composition to AISI Al 1. Forms Available: Bars (rounds, squares. flats). wire. billet, powder, plate. and other shapes on application. Applications: Micro-Melt 10 tool steel should...
Journal Articles
Alloy Digest (2000) 49 (2): TS-572.
Published: 01 February 2000
.... There is a heat treatment needed on weld repairs. General Characteristics: Compax Supreme has been developed as a mold quality steel, based on the widely used AISI S7 grade. The steel is extremely clean and has a ho- mogeneous microstructure. These features are achieved through strict processing control...
Journal Articles
Alloy Digest (1984) 33 (5): SS-444.
Published: 01 May 1984
... is considerably more severe than virtually all field environments. Times to failure for 20Mo-6 stainless were over I50 times greater than those for AISI Type 316. Also, 20Mo-6 stainless was superior to 2OCb-3 stainless in this environment. This is significant because no documented field failure by chloride stress...