Alloy Digest (1981) 30 (7): SS-389.
Published: 01 July 1981
... AISI No. 633 is a chromium-nickel-molybdenum stainless steel whose properties can be changed by heat treatment. It bridges the gap between the austenitic and martensitic stainless steels; that is, it has some of the properties of each. Its uses include high-strength structural applications...
Journal Articles
Alloy Digest (1996) 45 (1): SS-633.
Published: 01 January 1996
... Crucible Maxel 2000 is a corrosion resistant, pre-hardened, free machining steel based on AISI 414 (Alloy Digest SS-103, February 1989) stainless steel. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information...
Journal Articles
Alloy Digest (1975) 24 (3): CS-56.
Published: 01 March 1975
... corrosion resistance. Specification Equivalents: SAE 1018. QQ-S-633, FS 1018. QQ-W409, Comp 1018. MIL-S-113lO(ord), CS1018. ASTM A 108, Grade 1018. General Characteristics: AISI 1018 steel is a low-carbon steel with a wide range of applications. It has higher hardenability than AISI 1015 or 1020 because...
Journal Articles
Alloy Digest (1960) 9 (6): CS-13.
Published: 01 June 1960
... AISI C1141 is a tough, carbon-manganese steel characterized by its free-machining qualities. It is especially recommended for high production automatic machine products. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well...
Journal Articles
Alloy Digest (1976) 25 (10): CS-63.
Published: 01 October 1976
... resistant to alkalis at ordinary temperatures. Specification Equivalents: SAE 1065. QQ-S-633. QQS-00640 (Army Ord). General Characteristics: Because of its low hardenability, AISI 1065 can be hardened fully by oil quenching only in very thin sections. Only partial hardening can be achieved in heavier...
Journal Articles
Alloy Digest (1977) 26 (8): CS-68.
Published: 01 August 1977
... to alkalis at ordinary temperatures. Specification Equivalents: SAE 1552. ASTM A5. QQS-633, FS1052. MIL-S-11595A (Ord), 1052. General Characteristics: AISI 1552 steel is a medium-carbon steel of higher manganese content; it contains 1.20-1.50% manganese. Although it has this relatively high manganese level...
Journal Articles
Alloy Digest (1996) 45 (2): SS-637.
Published: 01 February 1996
... to a dramatic rise in the use of stainless mold steels throughout the plastics industry. Maxel 400 FTvl is a corrosion resistant, pre-hardened free-ma- chining steel intended for use in holder or backing applications in plastic molding. A modification of AISI 420 stainless mold steel. this grade is specially...
Journal Articles
Alloy Digest (1976) 25 (7): CS-61.
Published: 01 July 1976
.... Small additions of copper increase its atmospheric corrosion resistance. Specification Equivalents: SAE 1524. MIL-S-12505 (CE), Grade 5. QQ-s-633 (-2), FS1024. MIL-S-20145, Grade L. QQ-S-00643 (Army Ord FS-0. General Characteristics: AISI 1524 is a low-to-medium carbon steel with a higher hardenability...
Journal Articles
Alloy Digest (1972) 21 (8): CS-48.
Published: 01 August 1972
... AISI 1015 is a low-carbon steel used in the annealed, cold-worked, hot-rolled or normalized condition for general purpose construction and engineering. It is also used for case-hardened components. It combines good machinability, good workability and good weldability. This datasheet provides...
Journal Articles
Alloy Digest (1971) 20 (6): CS-41.
Published: 01 June 1971
... AISI 1040 is a medium-carbon steel used in the hot-rolled, normalized, oil quenched and tempered or water quenched and tempered condition for general purpose engineering and construction. It provides medium strength and toughness at low cost. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1982) 31 (12): CS-91.
Published: 01 December 1982
... is not satisfactory for welding because of its high sulfur content. II can be joined successfully by soldering or brazing. Specification Equivalents: SAE 1118. ASTM: A I08 and A 576. Federal: QQ-S-633 and QQ-S-00643. Military: MIL-S-16124 and MIL-S-1661 I. UNS No. Gl I 180. General Characteristics: AISI I I I8...
Journal Articles
Alloy Digest (1983) 32 (3): CS-93.
Published: 01 March 1983
... the machinability rating of AISI 1141isashighas90~cofthatofBI112steelscrew stock. The chip character is semi-continuous (broken) and semi-hard. ASTM: A 108, A 311 and A 576. QQ-S-633. UNS No. Cl 11410. General Characteristics: Single-point turning tools of high-speed steel should be ground to IO- I5 deg. side rake...
Journal Articles
Alloy Digest (1974) 23 (6): CS-54.
Published: 01 June 1974
... AISI 1022 is a carbon steel of relatively high manganese content which provides increased hardenability in all applications and increased hardness and strength in uncarburized uses and in the core of carburized components. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1961) 10 (12): CS-17.
Published: 01 December 1961
... AISI C1080 is a high carbon, water or oil hardening tool and spring steel having medium hardness penetration. It is recommended for general purpose tools, springs, and machinery parts requiring high hardness and wear resistance. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1983) 32 (10): CS-97.
Published: 01 October 1983
.... hook grind on the chaser. Thread chasing with carbide-tipped thread chasers can be done at 375 sfpm. ASTM: A 108. A 311 and A 576. Federal: QQ-S-633. AMS 5024. Military: MIL-S-16124. UNS No. G 11370. General Characteristics: Workability: AISI I137 has good hot-working characteristics. Heat the steel...
Journal Articles
Alloy Digest (1983) 32 (8): CS-96.
Published: 01 August 1983
... AISI 1117 is a resulfurized carbon steel for use where a free-machining carburizing steel is required. Its manganese content (nominally 1.15%) provides some increase in hardenability in all applications and increased hardness and strength in uncarburized uses and in the core of carburized parts...
Journal Articles
Alloy Digest (1959) 8 (12): CS-11.
Published: 01 December 1959
...: Specification Equivalents: AMS 5132 - 5121- 5122 - 7304 ASTM A108 Gr. 1095 SAE 1095 QQ-S-633, FS1095 ASTM A107 Gr. 1095 MII-S-16410 Camp. 1 FORGING: Heat slowly and uniformly to a maxioxuo tan- peramre of 1950┬░F. Cool after forging in air. Machinability: Machinability rating of 43% of AISI B1112 steeL Machines...
Journal Articles
Alloy Digest (1983) 32 (2): CS-92.
Published: 01 February 1983
... AISI 1060 is a high-carbon steel of low hardenability; it may be used in the as-rolled, annealed, normalized or liquid-quenched-and-tempered condition, depending on the desired properties. It is normally hardened by austenitizing and quenching in oil; however, it may be quenched in water...
Journal Articles
Alloy Digest (1983) 32 (7): CS-95.
Published: 01 July 1983
... AISI 1080 is a plain carbon steel containing nominally 0.80% carbon; it has relatively low hardenability. It may be used in the as-rolled, annealed, normalized or liquid-quenched-and-tempered condition, depending on the required properties. Normally it is hardened by austenitizing and quenching...
Journal Articles
Alloy Digest (1971) 20 (10): CS-44.
Published: 01 October 1971
... AISI 1045 is a medium-carbon steel used in four conditions: hot rolled, normalized, oil quenched and tempered or water quenched and tempered. It is a general-purpose engineering and construction steel and provides medium strength and toughness at low cost. It is commonly used for flame...