Journal Articles
Alloy Digest (1955) 4 (11): SA-35.
Published: 01 November 1955
... AISI E3310 is a chromium-nickel carburizing steel having exceptionally high hardenability. It is suited for heavy duty parts which must have high surface hardness combined with a strong and tough core. This datasheet provides information on composition, physical properties, hardness, and tensile...