Alloy Digest (1957) 6 (6): CS-6.
Published: 01 June 1957
... AISI C1144 is a tough, carbon-manganese steel characterized by its free-machining qualities. It is especially recommended for high production automatic machine products. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture...
Journal Articles
Alloy Digest (1967) 16 (3): CS-27.
Published: 01 March 1967
... ELASTUF PENN Machinery Steel is a special analysis 0.45% carbon steel that combines the most desirable characteristics of AISI C1045 and C1141. It might be accurately defined as an inexpensive, modified AISI C1144 because of its strength, machinability and excellent response to heat treatment...