Alloy Digest (1960) 9 (10): CS-14.
Published: 01 October 1960
... AISI C1117 is a low-carbon free-machining case-hardening steel. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on heat treating, machining, and joining. Filing Code...
Journal Articles
Alloy Digest (2003) 52 (4): SS-882.
Published: 01 April 2003
... to shape. Machinability: Project 70+ Type 416 stainless steel cuts very freely, primarily because of the addition of sulfur. When used in automatic screw machines, this grade machines like AISI C1117. Additional data on drilling and die threading are available from the producer. Weldability: Project...