Alloy Digest (1965) 14 (6): SA-178.
Published: 01 June 1965
... AISI 8660 is a high carbon, chromium-nickel-molybdenum alloy steel having high hardness and strength, suitable for springs and axle shafts. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on forming, heat treating, machining, and...