Alloy Digest (1972) 21 (9): SA-279.
Published: 01 September 1972
... AISI 8645 is a triple-alloy steel of the oil-hardening type. Its good hardenability and strength make it suitable for axles, shafts and a wide variety of other engineering uses. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as...