Alloy Digest (1960) 9 (12): SA-107.
Published: 01 December 1960
... AISI 6145 is a tough, shock resisting, shallow-hardening chromium-vanadium steel. It has high fatigue and impact resistance in the heat treated condition. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture...