Alloy Digest (1958) 7 (7): SA-71.
Published: 01 July 1958
... AISI 5140 is a low chromium alloy steel of the deep hardening type. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: SA-71. Producer...