Journal Articles
Alloy Digest (1973) 22 (10): SA-294.
Published: 01 October 1973
... AISI 5120 is a low-carbon, low-chromium carburizing steel recommended for applications where a core of medium strength and toughness combined with a wear-resistant carburized case is sufficient. It has medium hardenability and can be used without carburizing. This datasheet provides information...
Journal Articles
Alloy Digest (2004) 53 (12): SA-543.
Published: 01 December 2004
... of this alloy is higher than that of another common alloy, JIS SCM420H (a grade similar to AISI 4120), because the formation of an abnormal carburized layer was suppressed by reducing both silicon and manganese, and the strength of the grain boundary was improved by adding boron. The 107 cycle fatigue limit...