Alloy Digest (1961) 10 (10): SA-121.
Published: 01 October 1961
... AISI 4650 is an oil hardening, medium-carbon alloy steel having high mechanical properties, endurance limit and shock resistance. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on forming, heat...
Journal Articles
Alloy Digest (1958) 7 (7): TS-72.
Published: 01 July 1958
... HWD No. 3 is an air-hardening hot work steel recommended for dies where a minimum amount of distortion during hardening is required. It is equivalent to AISI Type H13. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness and creep. It...