Alloy Digest (1961) 10 (3): SA-112.
Published: 01 March 1961
... AISI 4615 is a low-carbon, nickel-molybdenum alloy steel of the carburizing grade, recommended for applications where high toughness and excellent wear resistance are required. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness...
Journal Articles
Alloy Digest (1959) 8 (8): SA-88.
Published: 01 August 1959
...: Can be readily welded under all normal conditions. It is free from air-hardening in the weld owing to its low carbon content. Although it can be welded by the electric arc or gas process, shielded arc ekctrodes for arc welding are preferred. Specification Equivalents: AISI 4615 QQ-S-624, FS4615 SAE...