Alloy Digest (1957) 6 (7): SA-59.
Published: 01 July 1957
... AISI 4150 is a through hardening chromium-molybdenum medium carbon steel not subject to temper embrittlement. It is recommended for heavy duty service. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture...
Journal Articles
Alloy Digest (1971) 20 (5): SA-265.
Published: 01 May 1971
... and AISI 4150) Tool Cutting Speeds, sfpm Life USS CARILLOY FC AISI 4150 minutes 241 BHN 285 BHN 285 BHN 15 No data No data 210 20 305 270 190 30 280 250 165 40 265 235 150 50 250 220 140 60 240 210 130 70 No data 205 125 *Values in this table are interpolated or estrapolated from measured data. Copyright ┬ę...
Journal Articles
Alloy Digest (2017) 66 (10): SA-801.
Published: 01 October 2017
... :: MemberServiceCenter@asminternational.org Published by ASM International® :: Data shown are typical, not to be used for specification or final design. General Characteristics: The steels have been available for over 20 years and possess the flexibility of the AISI 41XX steels. They are available in the 262 321 Brinell...
Journal Articles
Alloy Digest (2005) 54 (4): TS-562.
Published: 01 April 2005
... hardness. Specification Equivalents: UNS T41907 General Characteristics: Crucible S7 XL is a double-refined high-purity grade of AISI S7. The extra melt refining produces a cleaner, more uniform microstructure in S7 XL than in conventional S7. Advantages of Crucible S7 XL over conventional S7 include...
Journal Articles
Alloy Digest (1989) 38 (11): SS-204.
Published: 01 November 1989
..., butcorrosionresistance willbe considerably reduced. *Conditions available from the mill. Inquire regarding availabil- ity of other conditions. hkxthinabiltty: ARMCO 15-5 PH VAC CE can be machined in any heat treated Condition with excellent surface finish. In Condition A. use machining rates as for AISI Type 302 or 304...
Journal Articles
Alloy Digest (1968) 17 (2): SA-222.
Published: 01 February 1968
... AISI No 602 is a low-alloy high-temperature constructional steel of the Cr-Mo-V-Si type that possesses useful strength after suitable heat treatment at temperatures up to 1000 F. It is used for jet engine compressor wheels and blading. This datasheet provides information on composition, physical...