Alloy Digest (1988) 37 (9): SA-18.
Published: 01 September 1988
... AISI 4140 is a through-hardening chromium-molybdenum medium carbon steel. It is not subject to temper embrittlement. It is recommended for heavy duty service. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture...
Journal Articles
Alloy Digest (1975) 24 (8): SA-317.
Published: 01 August 1975
... CANNON-MUSKEGON 4140 is a medium-carbon cast alloy steel with good hardenability, strength and toughness. It is used in large quantities in the investment casting industry. A higher silicon content is permissible in this steel than in AISI 4140 (wrought) alloy steel. This datasheet provides...
Journal Articles
Alloy Digest (1994) 43 (8): SA-212.
Published: 01 August 1994
... Table 4 - TYPICAL CHARPY V NOTCH/TRANSITION TEMPERATURES AT THE 15 FOOT POUND (20.34 JOULES) ENERGY LEVEL FOR LONGITUDINAL HOT ROLLED SPECIMENS Steel Grade Condition Transition Temperature OF OC AISI 4140 Tempered** at 95O F (510°C) -110 -79 LEDLOY 4 140 Tempered** (AISI 41L40) at 950°F (510°C) -110...
Journal Articles
Alloy Digest (1993) 42 (9): SA-468.
Published: 01 September 1993
.... Machinability: Thyssen 4 140 Holder is a fkee machining alloy tool steel. The sulfur content is maintained at higher levels than in AISI 4140. Data for milling and drilling is found in Table 1. Weldability: Welding is often an integral part of the production of mold base or holder material. When welding Thyssen...
Journal Articles
Alloy Digest (2008) 57 (8): TS-668.
Published: 01 August 2008
... LSS 2714 is a hot-work steel with resistance to softening and good toughness. 2714HT is the same steel available as aged. The alloy is used to replace AISI 4140 and 4340. This datasheet provides information on composition, physical properties, and hardness. It also includes information on heat...
Journal Articles
Alloy Digest (2009) 58 (10): SA-608.
Published: 01 October 2009
... Crucible #135 Modified is a variation of AISI 4140 for nitriding the surface for hardness and abrasion resistance. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on heat treating, joining, and surface treatment. Filing Code: SA...
Journal Articles
Alloy Digest (1999) 48 (3): SA-498.
Published: 01 March 1999
... Lescalloy 6305 VAC-ARC steel is a modified AISI 4140 steel with higher molybdenum content and additional vanadium. The alloy is most frequently used in the quenched and tempered condition. Jet engine shafting is a typical application. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1961) 10 (6): SA-116.
Published: 01 June 1961
... condition its machinabiliry characteristics are similar to AISI 4140. Single point turning tools of high speed steel should be ground to 8-12 deg. side rake, 6-10 deg. back rake, 7-10 deg. side relief, 7-10 deg. end relief, E-15 deg. end cutting-edge angle, 12-18 deg. side cutting-edge angle, and a nose...
Journal Articles
Alloy Digest (2017) 66 (7): SA-793.
Published: 01 July 2017
... MTD 1 is a 4140 plate steel modified with slightly higher carbon and a vanadium addition. Vanadium improves graining refinement and, coupled with the higher carbon, promotes hardness and wear resistance. ArcelorMittal USA MTD steels comprise a family of pre-hardened alloy plate steels developed...
Journal Articles
Alloy Digest (1988) 37 (9): SA-432.
Published: 01 September 1988
... chro- mium-nickel-molybdunun electrodes. Austeni tic electrodes may be used but weld metal will be weaker than parent metal. Specification Equivalents: AISI 4140. mod&d. General Characteristics: HOLDAX has excellent machinability, good resistance to in- dentation and hardens uniformly. It can be flame...
Journal Articles
Alloy Digest (1958) 7 (6): SA-69.
Published: 01 June 1958
...&king chips. Rycut 40 anneaI&l is generally machined at 135 to 195 sfpm against 80 to 120 sfpm for ALSI 4140, depending on the part and type of operation performed. Heat treated stock machines at 90 to 140 sfpm compared to 65 to 110 sfpm for AISI 4140 hear neared. Single point turning tools of high...
Journal Articles
Alloy Digest (1998) 47 (1): SA-492.
Published: 01 January 1998
... AISI 4140; 5X is comparable to AISI 1055). Tea condirions: 108 end mill. 5 mm deep cur.lOmm~cu~UnironNo.3cutringoil Table 3 Welding Parameters for nG Welding Rlkmd wddiq- mm. N?de-, -mm -mm Pdi=m.A Lfmh W 1.0 1.0 E-80 4-8 8 1.6 1.6 70-150 6-9 8-10 24 2.4 lch?54l 7-10 &lo 3.2 3.2 10-16 8-10 General...
Journal Articles
Alloy Digest (1977) 26 (11): SA-338.
Published: 01 November 1977
..., % (Mean) 37 Rockwell C hardness, minimum 32 Table 2 - MACHINABILITY OF DYNA-LOY HS-32 AND THREE OTHER STEELS Relative Speed** Production Rate?? Production surface Feed? pieces per hour Capability feet per inch per (Basis 1.5 seconds Steel Grade RPc* minute revolution index time) AISI 4140 Anne&d 49 109...
Journal Articles
Alloy Digest (1953) 2 (3): SA-8.
Published: 01 March 1953
... tipped-carbide took General Characteristics: While comparable in composition to standard AISI 4140, it is closely controlled during manufacture to produce an especially high quality alloy. This steel shows better than average creep values and gives splendid service on such applications as high tempera...
Journal Articles
Alloy Digest (1979) 28 (4): SA-358.
Published: 01 April 1979
... water. For more details consult the manufacturer. Machining and Grinding: These are about the same for Cabot ESR HY 140 as for quenched and tempered AISI 4140 steel at Rockwell C 36. Workability: The Cabot ESR HY 140 steel is readily forgeable in the temperr ture range 170@2250oF, the maximum forging...
Journal Articles
Alloy Digest (1983) 32 (9): SA-393.
Published: 01 September 1983
... about the same for Ingersoll-Rand ESR HY 140 as for quenched and tempered AISI 4140 steel at Rockwell C 36. Workability: Ingersoll-Rand ESR HY I40 steel is readily forgeable in the temperature range I700-2250 F. the maximum forging temperature is 23000 F. The alloy may be either hot or cold formed by...
Journal Articles
Alloy Digest (1968) 17 (9): TS-210.
Published: 01 September 1968
...-ES018B2, AWS-E502. Bare rods: Eureka 130A, AISI 4130, AWS-E502. In case of atomic hydrogen or oxyacetylene welding, use AISI 4140. For non-hardensble filler metal, sustenicic types 312 or WH (wear hardening) costed elecvodes are recommended. The 312 electrode corre- sponds to AWS-E312 while WH is...
Journal Articles
Alloy Digest (1985) 34 (7): SS-461.
Published: 01 July 1985
... different heating remperatures and cooling methods on typical mechanical properties. Machinability: Allegheny Stainless Type 405 can be machined readily. In turning operations it behaves much like AISI 4140 at the same hardness level. Typical speeds for turning operations are 90- I20 surface feet per minute...
Journal Articles
Alloy Digest (1972) 21 (9): SA-280.
Published: 01 September 1972
... same for HY-130 and HY-140(T) as for quenched and tempered AISI 4140 steel at Rockwell C 36. Thus the machinability rating is approximately 60 10 65% of AISI B1112 Bessemer screw stock. Workability: The 5 NiCr-MO-V steel is readily forgeable in the temperature range 1700-2250oF. the maximum forging...
Journal Articles
Alloy Digest (2005) 54 (2): TS-612.
Published: 01 February 2005
... in a case hardness of 53 67 HRC. See Table 2. Weldability: Welding procedures similar to those used for 4140 or 4340 should be followed. P20, 4130, or 4140 filler material is accept- able. For prehardened material, preheat to 425 480 °C (800 900 °F). Maintain temperature above 425 °C (800 °F) dur...