1-2 of 2 Search Results for

AISI 4032

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1985) 34 (8): SA-411.
Published: 01 August 1985
... AISI 4032 is a molybdenum alloy steel of moderate hardenability. It is used extensively in the automotive industry. This steel combines moderate strength and hardness with good ductility and toughness in the quenched-and-tempered condition because it is relatively free from temper embrittlement...
Journal Articles
Alloy Digest (1975) 24 (9): SA-319.
Published: 01 September 1975
.... Hardening: Heat to 15251575oF, quench in oil or water, temper to desired hardness. General Characteristics: Sub-Critical Anneal: Heat to 110@1200oF, air cool. Machinability: For most machining operations the machinability rating of annealed-andcolddrawn SAE 4032 steel is about 75% of AISI B1112 Bessemer...