Alloy Digest (1982) 31 (8): CS-89.
Published: 01 August 1982
... AISI 1548 is a medium-carbon steel with a relatively high manganese content (1.10-1.40%). It can be used in a wide range of applications in the hot-rolled, normalized, annealed, cold-worked or liquid-quenched-and-tempered condition. It combines good machinability, with good workability. Among its...
Journal Articles
Alloy Digest (1956) 5 (1): SA-36.
Published: 01 January 1956
.... Sicromo2smelpossaxs a high degree of hot ductility under the combined iduena of time and stress at each of the temperatures considered. 77.5 78.8 886s: Machinability: Machinability rating of 60% of AISI Blll2 smeL Single poinr turning took of high speed steel should be ground co 10-15 deg. side rake, S-10 deg. back...