... AISI 1541 is a medium-carbon steel containing relatively high manganese (1.35-1.65%). It is characterized by a combination of good machinability and good workability. It may be used in the hot-rolled, annealed, normalized, cold-worked or liquid-quenched-and-tempered condition for numerous...
Journal Articles
Alloy Digest (2022) 71 (11): CS-235.
Published: 01 November 2022
...% for SAE 1212 cold drawn steel. Source: Ref 44 Table 10 Recommended machining data Turning, single point and box tools High speed steel tool Uncoated carbide tool Speed Depth of cut Tool material Speed Feed Tool material Brazed Indexable mm ISO m/min mm/rev ISO m/min m/min (in.) (AISI) (fpm) (ipr) (C) (fpm...
Journal Articles
Alloy Digest (2022) 71 (11): CS-234.
Published: 01 November 2022
... machining data Turning, single point and box tools High speed steel tool Depth of cut Tool material Speed Feed Tool material mm ISO m/min mm/rev ISO (in.) (AISI) (fpm) (ipr) (C) Treatment condition: +AR, +N, +A, or +C. Hardness: 85 125 HBW. 1 (0.040) S4, S5 (M2, M3) 56 (185) 0.18 (0.007) P10 (C-7) 4 (0.150...
Journal Articles
Alloy Digest (2022) 71 (9): CS-230.
Published: 01 September 2022
... cold drawn steel. Source: Ref 48 Table 13 Recommended machining data Turning, single point and box tools High speed steel tool Uncoated carbide tool Depth of cut Tool material Speed Feed Tool material Speed Brazed Indexable mm ISO m/min mm/rev ISO m/min m/min (in.) (AISI) (fpm) (ipr) (C) (fpm) (fpm...