Alloy Digest (1984) 33 (7): CS-102.
Published: 01 July 1984
... AISI 1146 is a resulfurized carbon steel containing nominally 0.85% manganese and a range of 0.08-0.13% sulfur to make it free machining. It has relatively low hardenability. Its ductility and toughness are fairly good in the longitudinal direction but are low in the transverse direction...