Alloy Digest (1983) 32 (11): CS-98.
Published: 01 November 1983
... AISI 1144 is a resulfurized carbon steel containing nominally 1.50% manganese and 0.24-0.33% sulfur to provide a free-machining steel. It is recommended especially for high-production automatic machine products. It has relatively low hardenability. Its ductility and toughness are reasonably good...
Journal Articles
Alloy Digest (2006) 55 (6): CS-31.
Published: 01 June 2006
... Fatigue-Proof and Stressproof steel bars are melted as a modification of AISI 1144 steel. Fatigue-Proof is made by various combinations of mechanical working and thermal treatments including LaSalle’s e.t.d. (elevated-temperature drawing) process. Similarly, Stressproof is made by a process...
Journal Articles
Alloy Digest (2013) 62 (5): SS-1144.
Published: 01 May 2013
... International, Materials Park, OH 44073-0002, 440-338-5151 MemberServiceCenter@asminternational.org Fax 440-338-8542 www.asminternational.org Filing Code: Stainless Steel May 2013 SS-1144 AK Steel 13-4SR equals AISI Type 409 in corrosion. The alloy with 3.75% Al is used in exhaust systems and has excellent...
Journal Articles
Alloy Digest (2019) 68 (10): SA-854.
Published: 01 October 2019
... and wear. Chemical Composition, wt.% (Typical) AISI 1144 heats to be used for Fatigue-Proof are usually nitrogen treated and contain nitrogen in quantities normally associated with steel produced by the electric furnace process. Carbon 0.40/0.48 Manganese 1.35/1.65 Phosphorus 0.040 max Sulfur 0.24/0.33...
Journal Articles
Alloy Digest (1961) 10 (6): CS-16.
Published: 01 June 1961
... Equivalents: AISI Cl 144 SAE 1144 ASTM Al08 Gr. 1144 ASTM A311 Gr. 1144 Acl 1320 deg. F Ac3 1400 deg. F Machinability: Ar3 1290 deg. F ArI 1200 deg. F General Characteristics: The machinability rating is 65% for hot rolled material, 76% for as cold drawn and 85% for annealed cold drawn material compared...
Journal Articles
Alloy Digest (1957) 6 (6): CS-6.
Published: 01 June 1957
... AISI C1144 is a tough, carbon-manganese steel characterized by its free-machining qualities. It is especially recommended for high production automatic machine products. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture...
Journal Articles
Alloy Digest (1960) 9 (5): CS-12.
Published: 01 May 1960
... Equivalents: (Chemical Composition Only) SAP-1144 ASTM A108 and A311 Gr. 1144 AISI Cl144 General Characteristics: Jaloase 100 (also 100-L) is a free machining, stress stabilized, cold drawn bar steel for production of machined parts. Uniform high strength and hardness imparts wear resistance and in many cases...
Journal Articles
Alloy Digest (2007) 56 (2): SS-986.
Published: 01 February 2007
... oxidation resistance than AISI Type 304 stainless. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance, corrosion and wear resistance as well as forming, heat treating, machining...
Journal Articles
Alloy Digest (2003) 52 (4): SS-882.
Published: 01 April 2003
... to shape. Machinability: Project 70+ Type 416 stainless steel cuts very freely, primarily because of the addition of sulfur. When used in automatic screw machines, this grade machines like AISI C1117. Additional data on drilling and die threading are available from the producer. Weldability: Project 70...