Alloy Digest (1980) 29 (3): CS-82.
Published: 01 March 1980
... AISI 1139 is a carbon steel containing 1.35-1.65% manganese and 0.13-0.20% sulfur to furnish free-machining characteristics. It is recommended especially for high-production machined products. Among its many applications are splined shafts, screws, arbors, tool holders and propeller shafts...
Journal Articles
Alloy Digest (2014) 63 (2): SA-691.
Published: 01 February 2014
... Mecasteel 145 (minimum yield strength 145 ksi) is a high-strength prehardened steel that can be used in substitution for conventional steels, such as AISI 4330, in the manufacture of massive steel components such as machines, hydraulic systems, and pumps. This datasheet provides information...
Journal Articles
Alloy Digest (2000) 49 (4): SS-779.
Published: 01 April 2000
...: Immerse in a solution of 10% sulfuric, 10% hydrochloric acid at about 82 °C (180 °F) to soften oxide scale. Then dip for a short time in warm 5 10% nitric acid to whiten the surface and pro- mote passivity. Machinability: AISI type 302 work hardens readily; therefore, tools must not ride surface without...