Alloy Digest (1973) 22 (12): CS-53.
Published: 01 December 1973
... AISI 1132 is a relatively tough, manganese alloy steel characterized by its free-machining qualities. It is recommended especially for high production machine products. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (1974) 23 (5): SA-303.
Published: 01 May 1974
... AISI 1330 is a through-hardening low-alloy steel for applications where medium hardenability and strength with low to medium toughness are sufficient. It may be used in the unhardened condition or after quenching in oil or water followed by tempering. This datasheet provides information...
Journal Articles
Alloy Digest (1973) 22 (6): SA-290.
Published: 01 June 1973
... AISI 5145 is a through-hardening, low-chromium alloy steel of intermediate hardenability. It is used in a number of machinery and tool applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness...
Journal Articles
Alloy Digest (1988) 37 (1): CS-117.
Published: 01 January 1988
...: AISI 1055. ASTM A 26, A 107, A241 and A 329. MIL-S-20145, MIL-S-10520 (Ord), MIL-E-18193 (-2) (Ships). QQ-S-633 (-2), QQ-S-00640 (Army Ord). General Chamcteristics: SAE 1055 has a low hardenability and can be hardened fully by water quenching only in very thin sections. Only partial hardening can...
Journal Articles
Alloy Digest (2014) 63 (7): SA-703.
Published: 01 July 2014
.... Materials Park, OH 44073-0002, 440-338-5151 MemberServiceCenter@asminternational.org Fax 440-338-8542 www.asminternational.org Filing Code: SA-703 Steel Alloy July 2014 Mecasteel is a series of high-strength prehardened steels based on improvement on AISI 4130 4330. The number relates to the minimum yield...
Journal Articles
Alloy Digest (1955) 4 (9): SA-33.
Published: 01 September 1955
... AISI 4037 is a molybdenum steel combining moderate strength and great toughness in the heat treated condition. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining...
Journal Articles
Alloy Digest (2014) 63 (2): SA-691.
Published: 01 February 2014
... Mecasteel 145 (minimum yield strength 145 ksi) is a high-strength prehardened steel that can be used in substitution for conventional steels, such as AISI 4330, in the manufacture of massive steel components such as machines, hydraulic systems, and pumps. This datasheet provides information...
Journal Articles
Alloy Digest (1981) 30 (1): CS-85.
Published: 01 January 1981
... AISI 1043 is a carbon steel that provides medium strength and medium toughness at relatively low cost. It can be used in the hot-rolled, normalized, oil-quenched-and-tempered or water-quenched-tempered condition for general-purpose construction and engineering. Its manganese content is a little...
Journal Articles
Alloy Digest (1977) 26 (8): SA-337.
Published: 01 August 1977
... AISI 81B45 is a nickel-chromium-molybdenum alloy steel to which boron has been added to increase its hardenability. It has intermediate hardenability for medium-duty applications. Its many uses include axles, gears and machinery components. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1963) 12 (10): SA-155.
Published: 01 October 1963
... AISI 8742 is a chromium, nickel, molybdenum alloy steel. It is oil hardening, has good hardenability and has desirable toughness. It is recommended for tough, high strength, heavy duty applications. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1975) 24 (9): SA-318.
Published: 01 September 1975
... AISI 1345 is a through-hardening, low-manganese alloy steel with intermediate hardenability. It is used where good strength is needed but low-to-medium toughness is sufficient. Applications include many parts for machines and tools. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1980) 29 (3): SA-370.
Published: 01 March 1980
... 118 1132 258-279 l/4 I/32 228-247 l/2 l/32 185-200 Hot-working operations, such as forging and hot rolling, can be done on AISI 4142 in the range 1900.22000F. Sections greater than four inches in thickness should be heated slowly through the transformation range, then rapidly to the hot-working...
Journal Articles
Alloy Digest (1972) 21 (9): SA-279.
Published: 01 September 1972
... 86-93 l/32 l/64 337-364 l/16 l/32 69-74 l/16 l/32 283-306 118 -, - 1132 6166 3;32 l/8 1;4 l/32 258-279 118 4448 l/32 228-247 l/4 l/32 52-56 112 l/32 185-200 Workability: AISI 8645 can be hot rolled or hot forged at 1950 to 22000F. Sections greater than four inches in thickness should be heated slowly...
Journal Articles
Alloy Digest (1974) 23 (2): TS-267.
Published: 01 February 1974
... side cuttingedge angle, and a nose radius of 1132 to l/l6 inch. Workability: AISI Type W2 can be forged by heating slowly, uniformly and thoroughly to 1800 to 1950oF. Forging should be completed at about 1500oF to insure fine austenitic grams and to leave the steel in good condition for annealing...
Journal Articles
Alloy Digest (1976) 25 (2): TS-297.
Published: 01 February 1976
... AISI Type S7 is a chromium-molybdenum, general-purpose, air-hardening tool steel recommended for uses where shock-resistance, good hot-work properties, good wear resistance, excellent toughness and easy machining are important. These properties make it suitable for many hot-work and cold-work...
Journal Articles
Alloy Digest (1955) 4 (1): SA-26.
Published: 01 January 1955
... AISI 6150 is a tough, shock resisting, shallow-hardening chromium-vanadium steel. It has high fatigue and impact resistance in the heat treated condition. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture...
Journal Articles
Alloy Digest (1980) 29 (4): TS-361.
Published: 01 April 1980
... punches slitter knives UNS T30407 Filing Coda: TS-361 1 Tool steel O8 MITER1 D-7 APRIL 1666 IMGSSt - DATA ON WORLD WIDE METALS AND ALLOYS @ Copyright 1980, Engiwring Publicatiom, Inc. WI rights res~~cd. hblbhai by w-&g&v~f=& Inc. Upper Montclair, New Jersey GUTERL D-7 (Cold-Work Tool Steel; AISI...
Journal Articles
Alloy Digest (1975) 24 (8): SA-317.
Published: 01 August 1975
... CANNON-MUSKEGON 4140 is a medium-carbon cast alloy steel with good hardenability, strength and toughness. It is used in large quantities in the investment casting industry. A higher silicon content is permissible in this steel than in AISI 4140 (wrought) alloy steel. This datasheet provides...
Journal Articles
Alloy Digest (1956) 5 (4): TS-45.
Published: 01 April 1956
... VDC is an air-hardening 5% chromium die steel recommended for a wide range of hot work applications requiring resistance to heat and abrasion, and is particularly useful for white metal die casting and extrusion applications. It is equivalent to AISI TYPE H13. This datasheet provides information...
Journal Articles
Alloy Digest (1984) 33 (4): TS-422.
Published: 01 April 1984
... Steel APRIL 1984 - DATA ON WORLD WIDE METALS AND ALLOYS Published b> @ &pyripht 1980. bIQiMi?rhQ PubliCOtionS. k. Ait rights rCSWw?d. ISSN : 002-614X Alloy Digest. Inc. Post Office Box 823 Upper Montclair, New Jersey JESSOP* SUPERSHOCK 7 (Air-Hardening Shock Steel: AISI Type S7) JEfjSOp SUPERSHOCK 7...