1-4 of 4 Search Results for

AISI 1118

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1974) 23 (8): CS-55.
Published: 01 August 1974
... AISI 1118 is a resulfurized carbon steel for applications requiring a free-machining carburizing steel. Its relatively high manganese content provides increased hardenability in all applications and increased hardness and strength in uncarburized uses and in the core of carburized components...
Journal Articles
Alloy Digest (1982) 31 (12): CS-91.
Published: 01 December 1982
... AISI 1118 is a low carbon steel containing relatively high manganese and sulfur to provide free-machining characteristics. It is resulfurized coarse-grain type of steel. AISI 1118 is commonly used to produce carbunized components and parts but can be used without carburizing for some applications...
Journal Articles
Alloy Digest (1973) 22 (3): CS-50.
Published: 01 March 1973
... methods such as hot dilute sulphuric acid with a good inhibitor and by sand or shot blasting. Specification Equivalents: B&W 1118 FM is produced to the same specifications as AISI 1118, but with some changes in the steelmak& process. See General Characteristics. General Charactwistics: B&W 1118 FM...
Journal Articles
Alloy Digest (1957) 6 (7): SA-58.
Published: 01 July 1957
.... Machinability: Cold drawn mate&I has a ma&inability rating of 60% of AISI Bll12 Besmmer screw stock- When anneaied prior to cold drawing the ma&inability apecrnncg an be ad- vanced 10% for most machming opuatiopr. single point turning tools of high speed smel should be ground to 8-12 deg side rake, 6-10 deg...