1-20 of 32 Search Results for

AISI 1095

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1984) 33 (1): CS-99.
Published: 01 January 1984
... AISI 1095 is a high-carbon, water-hardening tool and spring steel of low hardenability. Depending on the properties required, it may be used in the astrolled, annealed, normalized or liquid-quenched-and-tempered condition. It is hardened by austenitizing and quenching in water (preferably...
Journal Articles
Alloy Digest (1965) 14 (2): SA-173.
Published: 01 February 1965
... a machinability rating of approximately 655. char of AISI 1095 steel or 50% of AISI B1112 steel. Single point cutting tools of high speed steel should be ground to 15-200 side rake, 4-60 back rake, 4-80 side relief, 2-6O end relief, 8-120 end cutting-edge angle, 8-120 side cutting-edge angle, and a nose radius...
Journal Articles
Alloy Digest (2011) 60 (12): SS-1110.
Published: 01 December 2011
... ASTM A 608, grade HD 50 SAE 70327, 70446 Nearest wrought grade: AISI 327. The composition of the wrought grade differs from that of the cast alloy and has different properties. The cast alloy designation should always be used to identify castings. General Characteristics: HD alloy is a two phase...
Journal Articles
Alloy Digest (2012) 61 (1): SS-1112.
Published: 01 January 2012
... 0.54 HF 0.81 Gas, 1064 h at 960 °C (1760 °F) DOI: 10.31399/asm.ad.ss1112 Specification Equivalents: UNS J93005 ASTM A 297, grade HE ASTM A 608, grade HE 35 SAE 70327 Nearest wrought grade: AISI 312. The composition of the wrought grade differs from that of the cast alloy and has different properties...
Journal Articles
Alloy Digest (2011) 60 (11): SS-1108.
Published: 01 November 2011
.... Specification Equivalents: ASTM A297, grade HT ASTM A351, grade HT30 ASTM A608, grade HT50 Nearest wrought grade: AISI 330 The composition of the wrought grade differs from that of the cast alloy and has different properties. The cast alloy designation should always be used to identify casting. General...
Journal Articles
Alloy Digest (1959) 8 (12): CS-11.
Published: 01 December 1959
...: Specification Equivalents: AMS 5132 - 5121- 5122 - 7304 ASTM A108 Gr. 1095 SAE 1095 QQ-S-633, FS1095 ASTM A107 Gr. 1095 MII-S-16410 Camp. 1 FORGING: Heat slowly and uniformly to a maxioxuo tan- peramre of 1950°F. Cool after forging in air. Machinability: Machinability rating of 43% of AISI B1112 steeL Machines...
Journal Articles
Alloy Digest (1994) 43 (7): TS-528.
Published: 01 July 1994
... .55 4OO F 209 Bal. 750°F 216 PROPERTIES Table 1 -TYPICAL MACHINING VALUES FOR THYSSEN THYROPLAST 2798 (AISI P20 SPECIAL) Milling Operation in 0.08 min 0.08 max 2xD Depth of cut (C) Feed (9 Tool Type cutting speed (v) mm in/tooth mm/tooth fpm m/min 2min 0.008 min 0.20 min P.30-P.40 180-280 55-85 H.S.S...
Journal Articles
Alloy Digest (1992) 41 (12): TS-514.
Published: 01 December 1992
... Thyroplast 2311 tool steel is an AISI P20 modified grade, electric are melted and vacuum degassed, applicable to large plastic molds. It has good abrasion resistance and high impact strength This datasheet provides information on composition, physical properties, hardness, and tensile properties...
Journal Articles
Alloy Digest (1993) 42 (6): TS-518.
Published: 01 June 1993
... THYROPLAST 2738 is an AISI P20 modified tool steel, electric arc melted and vacuum degassed ideally suited for large intricate dies and plastic molds. It has high hardenability with high abrasion resistance and impact strength. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2006) 55 (11): SS-980.
Published: 01 November 2006
... 16 870 1600 152 22 110 16 18 83 12 980 1800 76 11 48 7 31 34 5 1095 2000 38 5.5 DOI: 10.31399/asm.ad.ss0980 The nearest wrought grade is AISI Type 309. The composition of the wrought grade differs from that of the cast alloy and has different properties. The cast alloy designation should...
Journal Articles
Alloy Digest (2003) 52 (2): CS-62.
Published: 01 February 2003
... steels. The results of abrasion tests run on a Taber Abrader for 3000 cycles for various materials are shown in Table 3. MartINsite exhibited weight losses that were in general sub- stantially lower than the AISI Types 1008, 1075, and 1095 steels tested. In addition, actual in-service tests conducted...
Journal Articles
Alloy Digest (2011) 60 (3): SS-1085.
Published: 01 March 2011
... Not required Post weld heat treatment 1095 ºC (2000 ºF) W.Q. Procedures for welding CH-20 alloy are available from Kubota Metal Corporation. Specification Equivalents: ASTM: A 743 (CH-20) The nearest wrought equivalent is AISI Type 309SS. General Characteristics: CH-20 is a Fe-Cr-Ni alloy with mechanical...
Journal Articles
Alloy Digest (2007) 56 (10): SS-998.
Published: 01 October 2007
... content and, subsequently, HK50 is stronger than HK40. The nearest wrought grade is AISI 310. The composition of the wrought grade differs from that of the cast alloy and has different properties. The cast alloy designation should always be used to identify casting. Product Forms Available: Horizontal...
Journal Articles
Alloy Digest (2001) 50 (12): TS-595.
Published: 01 December 2001
... Crucible CPM REX M35HCHS is a modification of the AISI M2 high-speed steel by an addition of cobalt and produced by powder metallurgy to be homogeneous with good toughness. This datasheet provides information on composition, physical properties, microstructure, hardness, and elasticity. It also...
Journal Articles
Alloy Digest (1989) 38 (3): TS-497.
Published: 01 March 1989
... WIDE METALS AND ALLOYS g+b P&&Mby: Alloy Oigest. Inc /201-6%6161 27 Chliild Street. Orange. N.J. 07060 / U.S.A. IMPAX SUPREME (Prehardened Mold Steel: AISI Type P20, Improved) IMPAX SUPREME* is a vacuum &gassed chromium-nickel-molybdenum steel, manufactured to consistently high quality. It is ideally...
Journal Articles
Alloy Digest (1994) 43 (7): SA-227.
Published: 01 July 1994
... ON THE LGNGITUDINAL TENSILE PROPERTIES OF LEDLOY-A LEDLOY-AX STEEL BARS Test Temp. F C LEDLOY AX (AISI 12L14 + Te) Tensile Elongation SlEllgth % in 1 ksi MPa (25.4 nun) - - - 80 27 59 407 38 200 93 61 423 21 400 204 79 545 22 500 260 80 550 28 600 316 75 517 28 700 371 63 434 21 Table 4 -TYPICAL CHARPY v NOTCH...
Journal Articles
Alloy Digest (2010) 59 (10): TS-693.
Published: 01 October 2010
... Equivalents: AISI Type T15 SAE Type T15 General Characteristics: REX M3-1 is a lower carbon, lower vanadium modification of M3-2 high speed steel. This lower alloy content results is better machining and grinding characteristics compared to M3-2, with a slight improvement in toughness and a moderate decrease...
Journal Articles
Alloy Digest (2006) 55 (7): CS-146.
Published: 01 July 2006
.... It is recommended that blanking is carried out in a straight- sided press, using blanking tools with sharp edges. Worn or damaged tools can cause edge defects. A punch to die clearance of 2 6% of the strip thickness is recommended. High-speed steel, such as AISI M2, and cemented carbide are used most often...
Journal Articles
Alloy Digest (1985) 34 (2): TS-435.
Published: 01 February 1985
... Tool Steel Or FEBRUARY 1995 bIGBST - DATA ON WORLD WIDE METALS AND ALLOYS @ Copyright 1980, Enginaaring Publications, Inc. A41 rights reserved. IW: 002-614X fuhlrshed hi Alloy Digest. Inc. 27 Canfield Street Orange. New Jersey 07050 (201) 761-1090 AIRKOOL (Air-Hardening Tool Steel: AISI Type A2...
Journal Articles
Alloy Digest (2010) 59 (8): SS-1073.
Published: 01 August 2010
...) solution followed by thorough rinsing to remove all residual solution. Specification Equivalents: AISI Types 316L ASTM A314, A182, A276, A479, A484, A580, A581, A582 UNS S31603 EN 10083-3 No. 1.4404/1.4401 EN 10083-3 X2CrNiMo17-12-2 General Characteristics: Ugima 316L XL is the next generation of improved...