Alloy Digest (1983) 32 (7): CS-95.
Published: 01 July 1983
... AISI 1080 is a plain carbon steel containing nominally 0.80% carbon; it has relatively low hardenability. It may be used in the as-rolled, annealed, normalized or liquid-quenched-and-tempered condition, depending on the required properties. Normally it is hardened by austenitizing and quenching...
Journal Articles
Alloy Digest (2023) 72 (4): CS-245.
Published: 01 April 2023
... Welding of Carbon Steels, Welding, Brazing, and Soldering, Volume 6, ASM Handbook, ASM International, 1993, p 641 661, httpsdoi.org/10.31399/asm .hb.v06.a0001432 CS-245 / 14 37. AISI 1080: Carbon Tool and Spring Steel, Alloy Digest (1983) 32 (7): CS-95. httpsdoi.org/10.31399/asm.ad .cs0095 38. CS80 Spring...
Journal Articles
Alloy Digest (1981) 30 (3): SS-383.
Published: 01 March 1981
... of 90% of yield strength (0.2% offset) follows: Grade Time to Failure, hours AISI Type 304 50-400 AJSI Type 316 300600 UHB Stainless 44LN > 3000, no failure UHB Stainless 44LN possesses good resistance to stress-corrosion cracking in sulphidic environments containing H2S. Corrosion in 5% NaCl saturated...
Journal Articles
Alloy Digest (2013) 62 (10): TS-723.
Published: 01 October 2013
... LSS 2367 is a European designation DIN 1.2367 and is similar to AISI H11. This datasheet provides information on composition, physical properties, and hardness. It also includes information on wear resistance as well as heat treating and machining. Filing Code: TS-723. Producer or source: Latrobe...
Journal Articles
Alloy Digest (1961) 10 (12): CS-17.
Published: 01 December 1961
... AISI C1080 is a high carbon, water or oil hardening tool and spring steel having medium hardness penetration. It is recommended for general purpose tools, springs, and machinery parts requiring high hardness and wear resistance. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1986) 35 (6): SS-471.
Published: 01 June 1986
... Copyright © ASM International® 1996 Table 3 - CORROSION-RESISTING CHAR.4CTERISTICS A. STRESS-CORROSION CRPICKING Stress: 9OTc of 0.2crC. Offset j ield Strength Environment: 405, CaCI: at 100°C Steel Time to Stress-Crack Failure. Hours AISI Type 304 PIISI Type 316 .AVESTA 44 LN IOU-300 00-500 No iailure...
Journal Articles
Alloy Digest (1988) 37 (7): SS-88.
Published: 01 July 1988
... AISI TYPE Stainless Steel is a quench hardenable grade of relatively low carbon content with some added nickel. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information...
Journal Articles
Alloy Digest (2015) 64 (3): SS-1204.
Published: 01 March 2015
... Uranus UR 2202 is considered a lean duplex austenitic/ferritic stainless steel designed to match the corrosion resistance of AISI Type 304L. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture...
Journal Articles
Alloy Digest (1982) 31 (10): CS-90.
Published: 01 October 1982
... 325 800 157Otxl 112ooo 13 41 319 1080 142culo 98000 15 46 288 1200 117000 77000 21 53 237 1300 103090 68000 23 58 210 DOI: 10.31399/asm.ad.cs0090 Copyright © ASM International® 1996 Heat Treatment: Critical Temperatures: The approximate maximum safe tempering temperatures of AISI 1561 is 1300°F. Ael...
Journal Articles
Alloy Digest (1993) 42 (9): SA-468.
Published: 01 September 1993
... Holder is a fkee machining alloy tool steel. The sulfur content is maintained at higher levels than in AISI 4140. Data for milling and drilling is found in Table 1. Weldability: Welding is often an integral part of the production of mold base or holder material. When welding Thyssen 4140 Holder, the part...
Journal Articles
Alloy Digest (1988) 37 (12): SS-499.
Published: 01 December 1988
... Heat Treatment: FL4MAX S is intended for use in the as-delivered condi- tion, hardened and tempered to 320 Brinell hardness, average. Machinability: RAMAX S has greatly improved machinability compared to conventional AISI Type 420 stainless hardened and tempered to 290-330 Brinell. Milling and drilling...
Journal Articles
Alloy Digest (1989) 38 (7): SS-508.
Published: 01 July 1989
... tocarbon steel, nickel-base fillers may also be used. Corrosion Resistance: Generalcorrosion 2RK65 (alloy904L) wasoriginallydeveloped for use in sulfuric acid. Is owrrosion at 0.1 and 0.3mm/year is compared with 0.3mm/year rate for AISI Type 3 16L in Fig. 1. 2RK65 (alloy 904L) has been used successfully...
Journal Articles
Alloy Digest (1971) 20 (5): SA-265.
Published: 01 May 1971
... 132000 107000 Elongation (2 in B 18 16 20 Reduction of area, % 53 51 52 Table 2 - END-QUENCH HARDENABILITY DATA (Comparison of USS CARILLOY FC and AISI 4 150H) Distance from Rockwell C Hardness Quenched End USS CARILLOY FC* AISI 4 150H sixteenths of inch Max Min Max Min 1 65 60 65 57 2 64.5 59.5 64.5...
Journal Articles
Alloy Digest (2016) 65 (6): SS-1247.
Published: 01 June 2016
... products. Specification Equivalents: AISI Types 431 ASTM A276, A479, A314 UNS S43100 EN 10083-3 No. 1.4057 EN 10083-3 Name X17CrNi16-2, X15 CrNi17-3 SIS 2321 AIR 9160C, Z150N17-03 Table 2 Guaranteed mechanical properties Condition Specifications Diameter, mm (in.) Heat treatments QT Tensile strength, Rm...
Journal Articles
Alloy Digest (1976) 25 (5): SS-328.
Published: 01 May 1976
...) - - - - 5% H7S04 boiling 3.5 1.8 50.5 roomtemp. 0.2 0.15 1.2 105 H2S04 boiling 5.7 4.2 345.1 room temp. 0.15 0.15 3.3 65%. HN03 boiling 0.15 0.15 room temp. 0.15 0.15 i-15 17:1 0.50, HCI boihng 0.15 0.15 Note: SS = Shnless Steel (AISI Type). Table 5 - PITTING CORROSION RESISTANCE (25-m, dia bars, 108OOC 30...
Journal Articles
Alloy Digest (2011) 60 (1): SS-1080.
Published: 01 January 2011
... range of 50 to 300 ºC ( 58 to 572 ºF) Improved stress corrosion resistance compared to AISI Type 304SS Products Available: Forms: Sheets, blanks, strips Thicknesses: 0.7 up to 10 mm (0.028 up to 0.394 in.) Width: Up to 2000 mm (78.74 in.) according to thickness. Finish: Cold rolled or hot rolled...
Journal Articles
Alloy Digest (2001) 50 (11): Ni-574.
Published: 01 November 2001
... by operations such as hydroform- ing, drawing, spinning, bending, and roll forming. It is consider- ably stronger than the AISI 300 series stainless steels at room temperature. Annealed alloy bar has also been successfully cold headed into fastener configurations. Intermediate annealing is normally required...
Journal Articles
Alloy Digest (2010) 59 (7): SS-1070.
Published: 01 July 2010
... acid is used in pickling. To the extent the NAS 354N is more resistant to corrosion than AISI Type 304, descaling is more difficult. Alkaline immersion for a short time before acid pickling and shot blasting, if possible, are effective at descaling. Workability: Care should be taken when cold working...
Journal Articles
Alloy Digest (1987) 36 (7): TS-208.
Published: 01 July 1987
... PYROVAN is nominally a 5% chromium, air-hardening die steel with more carbon and vanadium than found in AISI Type H13. PYROVAN has improved wear resistance over conventional die steels. The optimum combination of alloying elements in this grade promotes a good balance of properties. It has...
Journal Articles
Alloy Digest (2005) 54 (11): TS-621.
Published: 01 November 2005
... machining. Specification Equivalents: AISI H13 modified General Characteristics: Finkl DCF is a long-lasting die steel with excellent high- temperature properties. The machinability of this alloy in the pre- hardened condition is comparable to H13 (hardness 300 HB or 32 HRC), and DCF is nearly as machinable...