1-20 of 27 Search Results for

AISI 1060

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1983) 32 (2): CS-92.
Published: 01 February 1983
... AISI 1060 is a high-carbon steel of low hardenability; it may be used in the as-rolled, annealed, normalized or liquid-quenched-and-tempered condition, depending on the desired properties. It is normally hardened by austenitizing and quenching in oil; however, it may be quenched in water...
Journal Articles
Alloy Digest (1987) 36 (12): CS-116.
Published: 01 December 1987
... 49.4 241 llod Impact R-lb I I.5 14.5 12.5 I I.0 13.0 14.5 IS.0 Il.7 16.0 15.5 15.5 12.2 Machinability: The machinability rating of AIS) 1060. compared with freemachining AISI l2lZat lOO.isabout 55forannealed barsand 6&65 for annealed and cold-drawn bars. The chips are continuous, springy and hard...
Journal Articles
Alloy Digest (1992) 41 (11): SS-536.
Published: 01 November 1992
... Thyroplast 2316 is a modified AISI 420F stainless combining corrosion resistance, with the free machining capability and resistance indentation in coining. This datasheet provides information on composition and physical properties. It also includes information on corrosion resistance as well...
Journal Articles
Alloy Digest (2022) 71 (4): CS-220.
Published: 01 April 2022
... tool Uncoated carbide tool Depth of cut Tool material Speed Feed Tool material Speed Brazed Indexable mm ISO m/min mm/rev ISO m/min m/min (in.) (AISI) fpm) (ipr) (C) (fpm) (fpm) Treatment condition: +AR, +N, +A, or +C. Hardness: 175 225 HBW. 1 (0.040) S4, S5 (M2, M3) 37 (120) 0.18 (0.007) P10 (C-7) 130...
Journal Articles
Alloy Digest (2006) 55 (5): TS-631.
Published: 01 May 2006
... machinability and similar heat treatment to AISI Type D2. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on forming, heat treating, machining, surface treatment, and powder metal forms. Filing Code: TS...
Journal Articles
Alloy Digest (2008) 57 (7): SS-1015.
Published: 01 July 2008
... Uginox MA3 (X30Cr13, No. 1.4028; AISI 420) is an age-hardenable martensitic stainless steel, mostly used where a sharp edge for cutting is needed. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (1999) 48 (2): TS-567.
Published: 01 February 1999
... Uddeholm AISI D2 is a high-carbon, high-chromium, air-hardening tool and die steel capable of great hardness and high resistance to abrasive wear. It is nondeforming and is also somewhat corrosion resistant. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1981) 30 (7): Ni-269.
Published: 01 July 1981
... AISI No. 664 is a nickel-base high-temperature alloy that can be precipitation hardened because of its contents of aluminum and titanium. Vacuum melting is used in its production to provide excellent quality and reproducability. It is used for applications requiring a good combination of creep...
Journal Articles
Alloy Digest (1988) 37 (10): TS-493.
Published: 01 October 1988
... Canfiekl Slmel. Orange. NJ. 07060 / U.S.A ORVAR SUPREME (Hot Work Tool Steel, AISI Hl3)) ORVAR* SUPREME is a chromium-molybdenum-vanadium alloyed steel. Special processing techniques and close control are responsible for its high purity and very fine structure. It has improved isotropic properties. *ORVAR...
Journal Articles
Alloy Digest (2019) 68 (1): SS-1301.
Published: 01 January 2019
... Sandvik APM 2354 is a powder metallurgical, molybdenum alloyed, hot isostatic pressed product that is an austenitic stainless steel with improved corrosion resistance over AISI Type 304 and 304L. This datasheet provides information on composition, physical properties, and tensile properties...
Journal Articles
Alloy Digest (2008) 57 (5): SS-1012.
Published: 01 May 2008
... Uginox MA2 (X20Cr13, No. 1.4021; AISI type 420) is an age-hardenable martensitic stainless steel, mostly used where a sharp edge for cutting is needed. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes...
Journal Articles
Alloy Digest (1983) 32 (9): SA-393.
Published: 01 September 1983
...: These are about the same for Ingersoll-Rand ESR HY 140 as for quenched and tempered AISI 4140 steel at Rockwell C 36. Workability: Ingersoll-Rand ESR HY I40 steel is readily forgeable in the temperature range I700-2250 F. the maximum forging temperature is 23000 F. The alloy may be either hot or cold formed...
Journal Articles
Alloy Digest (1978) 27 (4): TS-332.
Published: 01 April 1978
...+g Inc. (High-Speed Steel; AISI Type M7) Upper Modddr, New Jersey BETHLEHEM M-7 is a high-molybdenum type of high-speed steel. Because of its high-carbon and high-vanadium contents, it has superior resistance to abrasion and is used for tools where edge toughness and wear resistance are required...
Journal Articles
Alloy Digest (1959) 8 (8): TS-84.
Published: 01 August 1959
... BETHLEHEM 57HW is the 9% tungsten type of hot-work tool steel, having excellent red-hardness and abrasion resistance compared with relatively good shock resistance for high operating temperatures. It corresponds to AISI Type H21 hot work tool steel. This datasheet provides information...
Journal Articles
Alloy Digest (1992) 41 (2): TS-509.
Published: 01 February 1992
... will result in a surface hardness of 1000 to 1150HVl .It is recommended that case depths not exceed 0.012 (about 20 hours of plasma nitriding time). QRO 90 SUPREME nitrides somewhat faster than AISI H13 steel. Nitriding per- formed on soft annealed material will be somewhat slower than that on hardened...
Journal Articles
Alloy Digest (1956) 5 (1): SA-36.
Published: 01 January 1956
.... Sicromo2smelpossaxs a high degree of hot ductility under the combined iduena of time and stress at each of the temperatures considered. 77.5 78.8 886s: Machinability: Machinability rating of 60% of AISI Blll2 smeL Single poinr turning took of high speed steel should be ground co 10-15 deg. side rake, S-10 deg. back...
Journal Articles
Alloy Digest (1970) 19 (12): SS-248.
Published: 01 December 1970
...: Cannot be hardened by thermal treatment. Can be hardened only by cold work. Stress Relief: Heat to 1560-17400F for 10-15 minutes. air cool thin sections and water quench heavy sections. Machinability: Machines rather poorly due to toughness of material Its machinability rating is about 45% of AISI B1112...
Journal Articles
Alloy Digest (2000) 49 (4): SS-778.
Published: 01 April 2000
... resistance to rust- ing caused by humid working and storage conditions and when molding corrosive plastics under normal production conditions. Specification Equivalents: AISI 420F General Characteristics: RAMAX S is a chromium-alloyed-stainless holder steel, which is supplied in the hardened and tempered...
Journal Articles
Alloy Digest (1984) 33 (6): Ni-298.
Published: 01 June 1984
... resistance Good Heat-treatable base metals Good Diffusion bonding Excellent *Depends on design of the brazements. base metal and brazing condition. Table 2 - BRAZED JOINT HARDNESS (AISI Type 316 stamless steel base metal) Knoop microhardness ( IO@gram load and l5-second identation time) 79Ot I30 Last...
Journal Articles
Alloy Digest (2023) 72 (5): CS-246.
Published: 01 May 2023
...) above the nitrocarburizing temperature. Source: Ref 73, 82, 85 Fig. 43 Hardness profile for various ion-nitrided materials. 1, gray cast iron; 2, ductile cast iron; 3, AISI 1040; 4, carburizing steel; 5, low-alloy steel; 6, nitriding steel; 7, 5% Cr hot-worked steel; 8, cold-worked die steel; 9...