Alloy Digest (1974) 23 (6): CS-54.
Published: 01 June 1974
... AISI 1022 is a carbon steel of relatively high manganese content which provides increased hardenability in all applications and increased hardness and strength in uncarburized uses and in the core of carburized components. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2022) 71 (5): CS-223.
Published: 01 May 2022
... tool Depth of cut Tool material Speed Feed Tool material mm ISO m/min mm/rev ISO (in.) (AISI) (fpm) (ipr) (C) Treatment condition: +AR, +N, +A, or +C. Hardness: 125 175 HBW. 1 (0.040) S4, S5 (M2, M3) 44 (145) 0.18 (0.007) P10 (C-7) 4 (0.150) S4, S5 (M2, M3) 37 (120) 0.40 (0.015) P20 (C-6) 8 (0.300) S4...
Journal Articles
Alloy Digest (2018) 67 (8): ts-752.
Published: 01 August 2018
.... Specification Equivalents DIN/EN <1.3355 > HS18-0-1 AISI T1 UNS T12001 BS BT1 UNE F5520 18-0-1 UNI HS 18-0-1 X75WCrV18 JIS SKH2 GOST R18 AFNOR Z80WCV18-04-01 General Characteristics This material is produced by powder-metallurgy methods. Segregation-free and homogenous metal powders of highest purity...
Journal Articles
Alloy Digest (1957) 6 (5): SS-56.
Published: 01 May 1957
... annealing is ordinarily done for best ma- chinability. Fair machinability rating about 55% of AISI B1112 Bessemer screw stock. It is easier to machine than Type 18-8 stainless steel, but there is a tendency to gall or build up on the cutting edges of the tool. Chips produced are brittle and stringy. Galling...
Journal Articles
Alloy Digest (2018) 67 (7): TS-751.
Published: 01 July 2018
... (2102 1994 °F). Slow cooling in furnace or in thermoinsulating material. Machining Recommendations on machining are shown in Table 1. Contact the producer for additional data. Specification Equivalents AISI T15 UNS T12015 ASTM A600 General Characteristics Böhler S393 is a tungsten high-speed tool steel...
Journal Articles
Alloy Digest (2019) 68 (11): TS-781.
Published: 01 November 2019
... Cryodur 2357 is a shock resistant tool steel (AISI S7) with excellent toughness and high strength. It is suitable for cold and hot work applications up to 538 °C (1000 °F). This datasheet provides information on composition, physical properties, and hardness. It also includes information on low...
Journal Articles
Alloy Digest (1987) 36 (6): SS-486.
Published: 01 June 1987
... ARMCO 439 HIGH PERFORMANCE-10 is a ferritic stainless steel sheet and strip alloy suited to automotive-exhaust system applications where oxidatin resistance is needed at temperatures beyond the capability of AISI Type 409 to withstand. The alloy also has good resistance to wet chloride...
Journal Articles
Alloy Digest (1987) 36 (4): SS-484.
Published: 01 April 1987
... 777 1022 ALUMINIZED STEEL, Type I** 22.I 36.8 65.4 117 152 Discontinued AISI Type 409 18.3 93.9 310 Discontinued ARMCO 18Cr-Cb HIGH PERFORMANCE-IO 0.9 1.0 I.1 1.1 1.2 I.3 1.4 1.5 1.4 1.2 1.2 0.8 AISI Type 304 I.1 1.2 I.1 -9.8 -36.4 -II2 -710 Discontinued *Cycle: 25 minutes heat, 5 minutes cool...
Journal Articles
Alloy Digest (2018) 67 (5): SS-1287.
Published: 01 May 2018
.... With a calculated average PREN of 15, this alloy has a better corrosion resistance than that of the AISI 420 series (1.4034; average calculated PREN of 13.5); but it remains less satisfactory than that of the AISI 431 series (1.4057; average calculated PREN of 17). that of the AISI 420 series (1.4034...
Journal Articles
Alloy Digest (2019) 68 (4): TS-762.
Published: 01 April 2019
... is at 800 880 °C (1472 1616 °F) and slow cooled. See Fig. 4 for a quench and tempered hardness curve. Specification Equivalents JIS SKH51 AISI M2 DIN WNr. 1.3342 General Characteristics High speed steel with high abrasion resistance and toughness for general use. Applications Cold forging dies, cold heading...
Journal Articles
Alloy Digest (1989) 38 (10): SA-441.
Published: 01 October 1989
... carburizing time, tempera- ture and carbon potential the resulting case depth on CBS-600 VIM-VAR is slightly less than for SAE/AISI 8720 and slightly deeper than for SAE/AISI 9310. CBS-600 VIM-VAR can be processed via double or single (direct from carburizing) quench practices. Preoxidation (30 min./1750 F...
Journal Articles
Alloy Digest (2012) 61 (8): SS-1126.
Published: 01 August 2012
... the hardness. General Characteristics: This alloy is a modified AISI 420 SS and is an electro slag remelted (ESR) martensitic stainless steel developed for corrosion- resistant applications. It is supplied in the annealed condition. Table 1 Mechanical properties tensile properties (room temperature) Hardness...
Journal Articles
Alloy Digest (2018) 67 (7): TS-750.
Published: 01 July 2018
.../asm.ad.ts0750 Weldability Use air hardening tool steel filler. See Table 1. Polishing Cryodur 2379 is not intended for tools that require a high surface finish. Specification Equivalents AISI D-2 General Characteristics Cryodur 2379 is a high-carbon, high-chromium tool steel developed for high-wear applications...
Journal Articles
Alloy Digest (2019) 68 (8): TS-772.
Published: 01 August 2019
... cooling in furnace or in thermoinsulating material. Specification Equivalents Normalized in: DIN/EN 1.3247 AISI M42 UNS T11342 BS BM42 UNE F5617 UNI HS2-9-1-8 JIS SKH59 SIS2716 AFNOR Z110DKCWV09-08-04-02-01 General Characteristics Cobalt molybdenum high-speed steel possessing high hardness, excellent...
Journal Articles
Alloy Digest (1977) 26 (9): TS-324.
Published: 01 September 1977
... of properties of high-speed steels for guidance only: seven AISI steels (M-l, M-2, M-7, M-10, M-42, T-l and T-15) and four Fagersta grades (D-950, FB-52, WKE-4 and WKE-45). Heat Treatment: Annealing: The temperature range for annealing is 1500-l SSOoF. The recommended practice is to pack in au inert material...
Journal Articles
Alloy Digest (2019) 68 (6): TS-767.
Published: 01 June 2019
... and welding temperatures. Process TIG/MMA Current DC Amperage, A 100 150 Electrode Tungsten thorium Electrode diameter 0.10 0.17 Protective gas Argon helium Flow (L/mm) 10 Filler Rod AISI H-11 or H-13 Preheat temperature, ºC (°F) 371 427 (700 800) Maintained temperature during welding, ºC (°F) Above 316 (600...
Journal Articles
Alloy Digest (2019) 68 (7): TS-769.
Published: 01 July 2019
... relieving, 30 50 ºC (86 122 ºF) below highest tempering temperature. Obtainable hardness after tempering is 63 65 HRC. See also Fig. 1 3. Specification Equivalents Normalized in: DIN/EN 1.3326 HS1-4-2 AISI M52 T11352 Hot Forming Forging. 1100 900 °C (2012 1652 °F). Slow cooling in furnace...
Journal Articles
Alloy Digest (2019) 68 (4): TS-761.
Published: 01 April 2019
... after tempering is 64 66 HRC. See also Fig. 1-4. Specification Equivalents DIN/EN 1.3243, HS6-5-2-5 AISI M41 UNE F5613, 6-5-2-5 UNI HS56-5-2-5 DOI: 10.31399/asm.ad.ts0761 Specification Equivalents (continued) AFNOR 90WDKCV06-05-05-04-02 UNS T11341 BS BM35 JIS SKH55 SIS 2723 Hot Forming Forging. 1100 900...
Journal Articles
Alloy Digest (2019) 68 (5): TS-765.
Published: 01 May 2019
... highest tempering temperature. Obtainable hardness after tempering is 64 66 HRC. See also Fig. 1-4. Specification Equivalents DIN/EN <1.3348> HS2-9-2 AISI M7 DOI: 10.31399/asm.ad.ts0765 UNS T11307 UNE F5607 2-9-2 UNI HS2-9-2 AFNOR Z100 DCWV09-04-02-02 JIS SKH58 Hot Forming Forging. 1100 900 °C (2012 1652...
Journal Articles
Alloy Digest (2019) 68 (6): TS-766.
Published: 01 June 2019
... is available from the producer. DOI: 10.31399/asm.ad.ts0766 Specification Equivalents Similar to: AISI M1 UNS T11301 BS BM1 AFNOR Z85DCWV08-04-02-01 W-No 1.3346 General Characteristics Properties. Molybdenum high-speed steel with high toughness and good cutting ability. Applications Taps, twist...