Alloy Digest (1971) 20 (2): CS-39.
Published: 01 February 1971
... AISI 1020 is a low carbon steel combining good machinability, workability, and weldability. It is used for case-hardened components and for a wide range of applications in the hot-worked, cold-worked, normalized or quenched-and-tempered conditions. This datasheet provides information...
Journal Articles
Alloy Digest (1971) 20 (3): CS-19.
Published: 01 March 1971
... of Cut 0.010 in. 0.050 In. 0.100 in. Tool Speed Feed Speed Feed Speed Feed Steel Material fpm ipr fpm ipr fpm ipr Fremax 15 High Speed Steel 160 0.005 150 0.007 145 0.010 AISI 1020 High Speed Steel 120 0.005 115 0.007 110 0.010 Fremax 15 Brazed Carbide 600 0.006 570 0.010 540 0.015 Al.9 1020 Brazed...
Journal Articles
Alloy Digest (2008) 57 (10): SS-1020.
Published: 01 October 2008
... Maxival 188HS is an enhanced machining version of AISI Type 303 stainless steel. The alloy has a specified inclusion picture to enhance machining by modifying both sulfide and oxide inclusions. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1987) 36 (2): CS-113.
Published: 01 February 1987
.... Small additions of copper increase its atmospheric corrosion resistance. Specification Equivalents: AISI 1020. AMS: 5032 and 5045. ASTM: A 129(1020). A 5lO(lO20). A 519(1020). A 544 (1020). 575(M 1020). A 576f 1020). and A 659( 1020). Federal QQ-W46 I ( 1020). Military: MIL-T-3520. MIL-S-7952. MIL-S-I...
Journal Articles
Alloy Digest (1974) 23 (6): CS-54.
Published: 01 June 1974
... (Qrd). MIL-S-16974 Wavy). General Characteristics: AISI 1022 steel is a low-carbon steel with a wide range of applications. It has higher hardenability than AISI 1020 or 1025 because of a higher manganese content; however, it can be hardened fully by water quenching only in thin sections. only partial...
Journal Articles
Alloy Digest (1965) 14 (4): Cu-17.
Published: 01 April 1965
... Heat Treatmeni: Cannot be heat treated to improve mechanical proper- ties, but can be relief annealed to Rockwell B82 to eliminate internal stresses. Machinability: Ic is easy to machine, having a relative machinability of 90% of AISI 1020 steel or 30% of free cutting brass. This alloy develops...
Journal Articles
Alloy Digest (2004) 53 (9): SS-909.
Published: 01 September 2004
... properties thermal properties Chemical Composition: The alloy is a modified AISI 420. It is a Cr-Ni-Mo-V alloyed material. See also Stavax ESR (Alloy Digest SS-507). Physical Properties: (Hardened and tempered to 50 HRC) Density, 20 °C (68 °F), kg/m3 (lb/in.3 ) 7740 (0.280) Coefficient of linear thermal...
Journal Articles
Alloy Digest (2008) 57 (2): TS-661.
Published: 01 February 2008
... Orvar 2M is a conventional tool steel of overall good ductility, toughness, weldability, and machinability. The alloy has the best overall product consistency for conventionally produced AISI H13 type tool steels. This datasheet provides information on composition, physical properties, elasticity...
Journal Articles
Alloy Digest (1982) 31 (12): Ni-281.
Published: 01 December 1982
...: RA 200 can be cold formed by conventional methods. in general, it will respond similarly to mild steel except for requiring somewhat greater power. The elastic limit of RA 200 is higher than that of mild steel. and the rate of workhardening is slightly greater than that of mild steel (AISI 1020...
Journal Articles
Alloy Digest (1991) 40 (8): SA-461.
Published: 01 August 1991
... UDDEHOLM AISI 52100 is an extremely versatile high-strength steel available in strip form. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on heat treating. Filing Code: SA-461. Producer or source: Uddeholm Corporation. Producer...
Journal Articles
Alloy Digest (1980) 29 (2): TS-359.
Published: 01 February 1980
... FAGERSTA M-7 is a molybdenum-type high-speed steel similar to AISI Type M1, but with higher percentages of carbon and vanadium than M1. The higher levels of carbon and vanadium provide an improved cutting efficiency without significantly lowering toughness. The many applications of FAGERSTA M-7...
Journal Articles
Alloy Digest (2022) 71 (5): CS-222.
Published: 01 May 2022
... is 300 HK 0.2. Source: Ref 47 48 Alloy Digest: Data on Worldwide Metals and Alloys CS-222 / 8 Table 13 Recommended machining data Turning, single point and box tools High speed steel tool Depth of cut Tool material Speed Feed Tool material mm ISO m/min mm/rev ISO (in.) (AISI) (fpm) (ipr) (C) Treatment...
Journal Articles
Alloy Digest (2005) 54 (3): SS-919.
Published: 01 March 2005
... International corrosion-resistant alloys elasticity hardness heat treatability indentation resistance joinability machinability physical properties RAMAX 2 tensile properties thermal properties Chemical Composition: Typical analysis is similar to AISI 420F, but modified. Ramax 2 is a Cr- Ni-Mo...
Journal Articles
Alloy Digest (2006) 55 (5): TS-631.
Published: 01 May 2006
... machinability and similar heat treatment to AISI Type D2. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on forming, heat treating, machining, surface treatment, and powder metal forms. Filing Code: TS...
Journal Articles
Alloy Digest (2000) 49 (8): TS-579.
Published: 01 August 2000
... in. (0.1 mm) max for hot-work applica- tions, and the formation of a white-layer must be avoided. Weldability: Weld repairs may be performed successfully when proper procedures are followed. The preheat and interpass temperature is 325 375 °C (620 710 °F). Use a filler metal of the AISI H13-type...
Journal Articles
Alloy Digest (1988) 37 (9): SA-18.
Published: 01 September 1988
... AISI 4140 is a through-hardening chromium-molybdenum medium carbon steel. It is not subject to temper embrittlement. It is recommended for heavy duty service. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture...
Journal Articles
Alloy Digest (1975) 24 (3): CS-56.
Published: 01 March 1975
... corrosion resistance. Specification Equivalents: SAE 1018. QQ-S-633, FS 1018. QQ-W409, Comp 1018. MIL-S-113lO(ord), CS1018. ASTM A 108, Grade 1018. General Characteristics: AISI 1018 steel is a low-carbon steel with a wide range of applications. It has higher hardenability than AISI 1015 or 1020 because...
Journal Articles
Alloy Digest (1994) 43 (9): TS-531.
Published: 01 September 1994
.... Filing Code: TS-531. Producer or source: Tool steel mills. Producer or Source: Tool steel mills Copyright © ASM International® 1996 1996 ASM International AISI TYPE A9 chemical composition hardness heat treatability machinability physical properties softening resistance tensile...
Journal Articles
Alloy Digest (2000) 49 (10): TS-581.
Published: 01 October 2000
... per inch of wall thickness, or hold at temperature for a minimum of 2 h. Specification Equivalents: AISI H13 DIN 1.2344 JIS SKD61 ISO 40CrMoV5 General Characteristics: A driving force in the die casting industry has been to develop a premium quality die steel that possesses outstanding toughness...
Journal Articles
Alloy Digest (1992) 41 (8): TS-512.
Published: 01 August 1992
... THYRAPID 3341 is similar to AISI M2, but adds sulfur. It is general purpose high-speed tool steel with good toughness, red hardness, and excellent machinability. This datasheet provides information on composition, physical properties, and hardness. It also includes information on forming, heat...