1-20 of 79 Search Results for

AISI 1010

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1985) 34 (5): CS-106.
Published: 01 May 1985
... AISI 1010 is a low-carbon steel having good formability and weldability. It is recommended for sheet stock for deep-drawing operations and in sheet and stock for structural shapes and carburized parts. Among its many applications are bushings, clutch discs, flanges, thrust washers, tinplate, nails...
Journal Articles
Alloy Digest (1985) 34 (12): Al-262.
Published: 01 December 1985
... should be sealed to prevent moisture entry. Specification Equivalents: UNS No. A96009. Table 5 - RELATIVE WEIGHTS OF ALUMINUM AND STEEL .AUTO BODY DECKLIDS OF A GIVEN MODEL Inner Panel Outer Panel Relative Allo> Gage Alloy Gage Weight AISI 1010 0.023 AISI 1010 0.030 1.00 51f32* 0.03 I 2036* 0.037 0.45...
Journal Articles
Alloy Digest (2004) 53 (1): TS-602.
Published: 01 January 2004
... better than AISI D2 while main- taining good toughness. Micro-Melt is a registered trademark of Carpenter Technology Corporation. Table 1 Typical Hardness Values Tempering temperature Austenitizing temperature °C °F °C °F Hardness, HRC 482 900 1010 1850 60.5 1038 1900 62 1066 1950 62 1093 2000 63 1121...
Journal Articles
Alloy Digest (1979) 28 (1): CI-47.
Published: 01 January 1979
...-Hard 4 CD4MCu 174PH CF8M CN7M CA15 AISI 1010 PH = 1.0 pH = 2.5 2.5% H2SO4 Using H2SO4 2120 5829 6846 125 149 138 177 4277 - 77 3773 4884 148 149 159 207 1426 7703 pH = 7.0 pH= 11.0 Using NaOH 12 11 ; ii:; 65 66 2: ;5 105 131 60 55 67 80 2.5% Nail 15 8 18 68 64 87 123 54 304 0.276 7.64 2435 0.102 8.47...
Journal Articles
Alloy Digest (1973) 22 (6): Al-207.
Published: 01 June 1973
... Alloy 3003H14. Compared to AISI 1010 steel, X2036-T4 has exhibited a corrosion rate (mils/year) in laboratory salt spray testing of about one-fifth that of steel. Ahnninum X2036 can be hot rolled readily to sheet and strip. It can be hot formed in the range of 800-1025oF and cooled by a strong air blast...
Journal Articles
Alloy Digest (2013) 62 (10): TS-723.
Published: 01 October 2013
... LSS 2367 is a European designation DIN 1.2367 and is similar to AISI H11. This datasheet provides information on composition, physical properties, and hardness. It also includes information on wear resistance as well as heat treating and machining. Filing Code: TS-723. Producer or source: Latrobe...
Journal Articles
Alloy Digest (2022) 71 (6): CS-224.
Published: 01 June 2022
...) The machinability rating is based on a value of 100 % for SAE 1212 cold drawn steel. Source: Ref 52 Table 13 Recommended machining data Turning, single point and box tools High speed steel tool Depth of cut Tool material Speed Feed Tool material mm ISO m/min mm/rev ISO (in.) (AISI) (fpm) (ipr) (C) Treatment...
Journal Articles
Alloy Digest (1993) 42 (11): TS-521.
Published: 01 November 1993
... THYRODUR 2510 (AISI D2) is an oil hardening, non-shrinking die steel which can be hardened at relatively low temperatures. The alloy exhibits excellent wear resistance. This datasheet provides information on composition, physical properties, and hardness. It also includes information on heat...
Journal Articles
Alloy Digest (1970) 19 (3): CS-33.
Published: 01 March 1970
... AISI C1010 is a low carbon steel having good formability and weldability. It is recommended in sheet stock for deep drawing operations and in sheet and bar stock for structural shapes and case hardened parts. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1994) 43 (10): TS-532.
Published: 01 October 1994
...: Tool steel mills. Producer or Source: Tool steel mills Copyright © ASM International® 1996 1996 ASM International AISI TYPE D5 chemical composition hardness heat treatability machinability physical properties softening resistance thermal properties UNS T30405 I Filing Code: TS...
Journal Articles
Alloy Digest (2001) 50 (9): TS-590.
Published: 01 September 2001
... Lanark is a silicon-manganese shock resistant tool steel with highest impact strength of the AISI S type tool steels. It is used for pneumatic tools, shear blades, and mandrels. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes...
Journal Articles
Alloy Digest (2000) 49 (11): SS-808.
Published: 01 November 2000
... Lescalloy 410Cb is a modification of AISI Type 410 changed by the addition of niobium (columbium). This change provides for an increase in strength for structural applications. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well...
Journal Articles
Alloy Digest (1988) 37 (9): SS-99.
Published: 01 September 1988
... steel 60-90 Fishing High-speed steel loo-120 Heat Treatment: Anneal: Heat to 1850-2050 F(1010-1120°C). aircoolorwater quench, depending on thickness. Stress Relief: Heat to below 9OO F (482 C) for dimensional stability and removal of peak smsses. Machinability AISI Type 302 work hardness readily...
Journal Articles
Alloy Digest (1999) 48 (2): TS-567.
Published: 01 February 1999
... Uddeholm AISI D2 is a high-carbon, high-chromium, air-hardening tool and die steel capable of great hardness and high resistance to abrasive wear. It is nondeforming and is also somewhat corrosion resistant. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1986) 35 (2): SS-424.
Published: 01 February 1986
... ARMCO 12 SR was developed specifically for automotive exhaust applications. It has greater oxidation resistance than AISI Type 409 and it exhibits formability and weldability comparable to more highly alloyed ferritic grades. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2001) 50 (5): TS-586.
Published: 01 May 2001
... minimum. Then cool slowly with the furnace at a rate not exceeding 28 °C (50 °F) per hour to 538 °C (1000 °F). Continue cooling to ambient tempera- ture in the furnace or in air. The resultant hardness should be a maximum of 255 HB. Specification Equivalents: AISI M4 (High Carbon) General Characteristics...
Journal Articles
Alloy Digest (1991) 40 (9): TS-505.
Published: 01 September 1991
... IMPAX WELD COATED ELECTRODE and IMPAX TIG-WELD TIG FILLER ROD give a deposited weld metal almost identical in composition to IMPAX SUPREME parent metal. Both the electrode and the filler rod are also suitable for welding standard AISI P20 tool steel grades and Uddeholm Holder grades. Composed...
Journal Articles
Alloy Digest (2005) 54 (4): TS-562.
Published: 01 April 2005
... hardness. Specification Equivalents: UNS T41907 General Characteristics: Crucible S7 XL is a double-refined high-purity grade of AISI S7. The extra melt refining produces a cleaner, more uniform microstructure in S7 XL than in conventional S7. Advantages of Crucible S7 XL over conventional S7 include...
Journal Articles
Alloy Digest (1981) 30 (11): SS-395.
Published: 01 November 1981
.... Machinability: In turning operations, Carpenter Stainless Type 405 machines somewhat like AISI Type 410 and Type 430 stainless steels and AISI 1045 carbon steel. Typical speeds for turning operations are 90/140 surface feet per minute. when using high-speed steel tools. Carpenter Type 405 has a machinability...
Journal Articles
Alloy Digest (1999) 48 (4): SS-742.
Published: 01 April 1999
... properties comparable to AISI type 316, along with high yield strength, good weldability, and good formability. Chemical Composition, wt Physical Properties: Mechanical Properties: Heat Treatment: Annealing is performed at 899 1010 °C (1650 1850 °F), fol- lowed by a water quenching or fan cooling. Hardening...