Alloy Digest (1959) 8 (6): TS-24.
Published: 01 June 1959
... AIRQUE is an intermediate chromium-molybdenum air-hardening die steel which finds its best application in intricate dies where difficulty in distortion and cracking is encountered with the usual oil-hardening types of tool steels. It is classed as type A-2 tool steel. This datasheet provides...