Alloy Digest (1981) 30 (7): SA-381.
Published: 01 July 1981
... AIRCO METAL-COR 6 is a continuous tubular steel welding electrode with a powdered-metal core; gas shielding rather than slag is used to protect the core. It eliminates 50 to 70% of the smoke and fumes generated by self-shielded flux-cored electrodes and about 30% of the smoke from gas-shielded...
Journal Articles
Alloy Digest (1982) 31 (1): SA-384.
Published: 01 January 1982
..., psi Tabulated values are approximate. 0.283 7.83 0.11 ti ; ;;I; 7:7 x 10-6 28-f; ; ;$ PROPERTIES Table 1 - HOW TO USE VERTI-COR WELDING ELECTRODE (Typical Equipment: 450-ampere AIRCOMATIC@ CV 450 Power Supply, MIGhTya AHF-T Wire Feeder and AH 40F Gun. AU Airco equipment designed for 0.052 or l/16...
Journal Articles
Alloy Digest (1984) 33 (3): SA-399.
Published: 01 March 1984
... for job shop work. The benefits of using the Tuf-Cor I Welding Electrode may be summarized as follows: (I) Designed for flat and horizontal welds, (2) Wide current and voltage range, (3) Superior operator appeal, (4) Spray-like metal transfer, (5) Practically spatter-free, (6) Maximum resistance...
Journal Articles
Alloy Digest (1980) 29 (5): SA-373.
Published: 01 May 1980
...% argon + 60/70% helium. The following electrodes may be used with any of these gas mixtures: Airco AX-g!, Hobart HB-18. Linde 83, Linde HI-84. Flux-Coated-Wire Weldmg: The following wires are suitable for welding VAN QN (SO), using CO2 shielding: (1) Airco Tensil- Cor. (2) Hobart Fabco 801, (3) Hobart...