1-1 of 1 Search Results for

AFCOMET 40

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1953) 2 (9): CI-2.
Published: 01 September 1953
... AFCOMET 40 is a dense, close-grained nickel-molybdenum cast iron with good resistance to wear and abrasion. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness...