1-2 of 2 Search Results for

AEREX 350

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2022) 71 (6): Ni-780.
Published: 01 June 2022
... SPS Technologies Aerex 350 is a proprietary high-strength, corrosion-resistant nickel-based superalloy that is suitable for demanding applications up to 730 °C (1350 °F). It has the highest temperature limit of the three SPS superalloys. Like MP35N and MP159, this alloy not only undergoes...
Journal Articles
Alloy Digest (1995) 44 (3): Ni-479.
Published: 01 March 1995
... AEREX 350 is a bolt alloy with a combination high temperature creep strength, notch toughness, and thermal stability. It was designed for aerospace bolting applications. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength...