Alloy Digest (2022) 71 (1): CI-89.
Published: 01 January 2022
... ACO Eurobar EN-GJL-150C (5.1102) is a low-tensile-strength gray cast iron that is produced by the continuous casting process. It is useful in situations where very high thermal conductivity, machinability, and damping capacity are important, but where tensile strength and hardness...