Alloy Digest (1958) 7 (5): SS-74.
Published: 01 May 1958
... FAHRALLOY 2817 is a 28% Cr-16% Ni heat and corrosion resistant casting alloy. It is non-hardenable and corresponds to A.C.I. Type HI alloy. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes...
Journal Articles
Alloy Digest (1959) 8 (4): SS-86.
Published: 01 April 1959
... temperature performance and corrosion resistance as well as casting, heat treating, and machining. Filing Code: SS-86. Producer or source: Stainless steel foundries. Producer or Source: Stainless steel foundries Copyright Ā© ASM InternationalĀ® 1996 1996 ASM International A.C.I. TYPE HI...
Journal Articles
Alloy Digest (1956) 5 (2): SS-40.
Published: 01 February 1956
... X-ITE is a high chromium-nickel casting alloy having high resistance to corrosion, heat and abrasion. It corresponds to A.C.I. Type HU alloy. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and...
Journal Articles
Alloy Digest (1963) 12 (5): SS-143.
Published: 01 May 1963
... ASM International ACI type HF castability chemical composition corrosion-resistant alloys creep properties elasticity hardness heat treatability high-temperature alloys joinability machinability oxidation resistance physical properties tensile properties Filing Code: 35-143 A.C.I...
Journal Articles
Alloy Digest (1969) 18 (10): SS-230.
Published: 01 October 1969
.... This solution will remove the oxide and whiten the surface. Specification Equivalents: ASTM-Al67 Cr. 8; A314 Ty. 309; A264 Gr. 8; A312 Ty. 309 ASTM-B190 (castmg); A296 Gr. CH20 & Cr. CG12 SAE 30309 & 60309 AMS 5650 QQ-S-766 Gr. 1 F MIL-R-503 1, Comp. 2 MlL-E-6844, Cl. 2 A.C.I. Type CA22 and Type CH20...
Journal Articles
Alloy Digest (1958) 7 (7): SS-76.
Published: 01 July 1958
... for arc welding. Specification Equivalents: A.C.I. Type HI Mod&d Castabilw Section thicknesses of 3/16 inch up can be cast satis- factorily. Somewhat lighter sections are also feasible depending on casting design and pattern equipment. Good castibility of this alloy permits designs involving intricate...
Journal Articles
Alloy Digest (1989) 38 (10): SS-75.
Published: 01 October 1989
... welding, and the flame should be adjusted to be slightIy rich in acetylene. Lime-coated electr0des of Type 309 steel are recommended for arc welding. Specification Equivalents: A.C.I. Type HI Modified Castabilityz Section thicknesses of 3/16 inch up can be cast satis- factorily. Somewhat lighter sections...
Journal Articles
Alloy Digest (1962) 11 (2): SS-128.
Published: 01 February 1962
... about 33% of cast carbon steel. Cast Ducsloy HI can be rough curned at 40-45 sfpm surface speed using l/16-3/32 depth of cut and 40-50 rev./in. feed. On finishing cuts the feed is generally reduced about half (twice the revolutions per inch of indicated value) giving a finer pitch. Since the depth of...