Alloy Digest (1990) 39 (8): CI-62.
Published: 01 August 1990
... 55-06 and 70-02 Ductile Dura-Bar are continuously cast ductile irons with about 50 and 75% pearlitic microstructures, respectively. 55-06 has about the same tensile strength as SAE 1045 as-hot-rolled steel. Its maximum yield strength and elongation are equivalent to a eutectoid carbon steel. 70-02...