Alloy Digest (1982) 31 (8): Fe-66.
Published: 01 August 1982
... The 42 Nickel-Iron alloy has the lowest expansivity of the Iron-Nickel alloys that are commonly used for glass-sealing applications. Its thermal expansion closely matches the 1075 glass and it is sometimes used for sealing action with the 0120 and 0010 glasses. It is made close metallurgical...
Journal Articles
Alloy Digest (1987) 36 (6): Fe-77.
Published: 01 June 1987
... NILO Alloy 42 is a binary nickel-iron alloy having a low and nominally constant expansion coefficient over the range 20-300 C (68-572 F). It is used for semiconductor lead frames, thermostats and glass-to-metal seals. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1956) 5 (2): Fe-9.
Published: 01 February 1956
... D.H No. 42 is a 42% nickel-iron alloy having low controlled coefficient of expansion. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining...
Journal Articles
Alloy Digest (1979) 28 (10): Fe-59.
Published: 01 October 1979
... TECHALLOY GLASSEAL 42 is an iron-nickel alloy with thermal expansion that closely matches the 1075 glass. Also, it is sometimes used for sealing action for the 0120 and 0010 glasses. It has the lowest expansivity of the iron-nickel alloys that are commonly used for glass-sealing applications...
Journal Articles
Alloy Digest (1954) 3 (12): Ni-13.
Published: 01 December 1954
... K-42-B is a nickel-cobalt-chromium-iron alloy having high resistance to heat and corrosion. It responds to a precipitation-hardening heat treatment producing high tensile and creep characteristics at elevated temperatures. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1993) 42 (12): Fe-103.
Published: 01 December 1993
... Core Rod is suggested. Brazing: Copper and zinc-free brazing alloys are sug- gested. General Characteristics: Carpenter Low Expansion 42 Dumet Core Rod is a42 % nickel-iron alloy possessing a virtually constant low rate of thermal expansion at temperatures up to approximately 650°F (343°C...
Journal Articles
Alloy Digest (1990) 39 (6): Fe-91.
Published: 01 June 1990
... Carpenter Low Expansion 43-PH is an age hardenable iron/nickel austenitic alloy. It differs from most metals and alloys in that it has a constant modulus of elasticity over a temperature range of -30 to +150 F(-47 to +66 C). Its thermal elastic coefficient can be adjusted to zero or near zero...
Journal Articles
Alloy Digest (1970) 19 (8): Fe-44.
Published: 01 August 1970
... Alloy) UNISEAL. 42 is a closely controlled thermal expansion iron alloy used for glass-temetal and metal-to-ceramic seals. *Registered trademark of UniversalCyclops. Composition: Carbon Manganese Silicon Nickel Iron Typical Analysis 0.03% 0.80% 0.15% 41.5% Remainder Physical Constants: Density, lb/ cu...
Journal Articles
Alloy Digest (2005) 54 (6): Fe-137.
Published: 01 June 2005
... Analysis) Carbon 0.07 Silicon 0.25 Nickel 42.50 Manganese 0.50 Chromium 5.75 Iron bal Physical Properties: Specific gravity 8.12 Density, kg/m3 (lb/in.3 ) 8110 (0.293) Mean specific heat capacity, J/kg 502 (0.120) K (Btu/lb °F) Thermal conductivity, W/m K 12.5 (7.2) (Btu/(ft h °F)) Resistivity...
Journal Articles
Alloy Digest (1993) 42 (11): Fe-102.
Published: 01 November 1993
... 42 is suggested Brazing: Copper and zinc-free brazing alloys are sug- gested General Characteristics: Carpenter Glass Sealing 42 is a 41% nickel-iron con- trolled expansion alloy which has been used in a wide DOI: 10.31399/asm.ad.fe0102 Copyright © ASM International® 1996 70 0 0 loo 200 300 400 500...
Journal Articles
Alloy Digest (2011) 60 (11): Fe-156.
Published: 01 November 2011
... Sulfur 0.025 Nickel 40.0 43.0 Chromium 0.25 Iron bal Physical Properties: Specific heat, J/kg·K (Btu/lb·°F) 176.7 (0.0422) Thermal conductivity, 20 °C (70 °F), W/m·K (Btu/(h·ft·°F)) 15.5 (9.0) Coefficient of thermal expansion, 10 6/K (10 6/°F) 30 400 °C (85 750 °F) 4.6 (2.6) 30 450 °C (85 840 °F) 7.0...
Journal Articles
Alloy Digest (1954) 3 (11): CI-9.
Published: 01 November 1954
... NI-HARD is a white cast iron alloyed with nickel and chromium to give high hardness and outstanding resistance to abrasion. The structure consists of hard carbide matrix rendered martensitic by the nickel content. The wearing faces of heavy castings may be chilled, thus giving a white iron face...
Journal Articles
Alloy Digest (1971) 20 (4): Cu-231.
Published: 01 April 1971
... COPPER ALLOY No. 706 is an alloy of copper and nickel which has been modified by the addition of approximately 1.4% iron to improve its resistance to salt water corrosion. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well...
Journal Articles
Alloy Digest (1996) 45 (4): Ni-339.
Published: 01 April 1996
.... Applications include components for gas turbines, bolting, and valve stems for power applications. Nirnonic is a trademark of the lnco family of companies. Chemical Composition, wt.Ok: (Nominal) Carbon Silicon Copper Iron Manganese Chromium Titanium Aluminum Cobalt Molybdenum sulfur Nickel 0.1 max 0.4 max 0.5...
Journal Articles
Alloy Digest (2011) 60 (1): Fe-153.
Published: 01 January 2011
... Fax 440-338-8542 www.asminternational.org Filing Code: Iron January 2011 Fe-153 HPM Precision C is heat treatable and has a constant elastic modulus value. HPM® PRECISION C (Nickel-Iron Alloy) HPM® PRECISION C Chemical Composition, wt. %: (Nominal) Nickel 42 Chromium 5.3 Titanium 2.4 Aluminum 0.55...
Journal Articles
Alloy Digest (2012) 61 (2): Fe-158.
Published: 01 February 2012
... SSC Invar 36 was developed for use in applications where dimensional stability is essential. It is a nickel-iron alloy with a very low coefficient of thermal expansion from cryogenic temperatures to 200 deg C (390 deg F). It is utilized in aerospace composite tooling and die applications, as well...
Journal Articles
Alloy Digest (2004) 53 (11): Fe-133.
Published: 01 November 2004
... Carpenter Low Expansion 49 alloy is a 48% nickel-iron alloy with a low rate of thermal expansion useful for glass sealing of fiber optics. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on heat treating...
Journal Articles
Alloy Digest (2004) 53 (12): Fe-134.
Published: 01 December 2004
... Carpenter Low-Expansion 45 alloy is a 45% nickel-iron alloy with a constant rate of thermal expansion useful in thermostats. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature...
Journal Articles
Alloy Digest (2011) 60 (2): Ni-687.
Published: 01 February 2011
... ALLOY 825 Chemical Composition, wt (Typical) Carbon 0.05 max Chromium 19.5 23.5 Nickel 38.0 46.0 Molybdenum 2.5 3.5 Sulfur 0.03 max Manganese 1.00 max Silicon 0.5 max Aluminum 0.2 max Copper 1.5 3.0 Titanium 0.6 1.2 Iron 22.0 min Physical Properties: Density, kg/m3 (lb/in.3) 8140 (0.240) Specific heat...
Journal Articles
Alloy Digest (2011) 60 (8): Fe-154.
Published: 01 August 2011
... NAS 36 is a nickel-iron alloy with a low coefficient of thermal expansion and is sensitive to changes in size. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on corrosion resistance as well as forming. Filing Code: Fe-154...