1-20 of 128 Search Results for

1060

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2022) 71 (4): CS-220.
Published: 01 April 2022
... 1059, 1060, C60, C60E, and C60R are wrought high-carbon non-alloy steels that are used in the normalized, cold worked, quenched and tempered, or austempered condition. 1059, 1060, C60E, and C60R may also be flame or induction hardened. These steels are widely used for moderately and highly...
Journal Articles
Alloy Digest (2023) 72 (9): CS-259.
Published: 01 September 2023
... 1059, 1060, C60, C60E, and C60R are wrought high-carbon (carbon = 0.55–0.65%) non-alloy steels that are used in the normalized, cold worked, quenched and tempered, or austempered condition. 1059, 1060, C60E, and C60R may also be flame or induction hardened, nitrided, or nitrocarburized...
Journal Articles
Alloy Digest (1979) 28 (8): Al-134.
Published: 01 August 1979
... ALUMINUM 1060 is a commercially pure grade of aluminum (99.6% minimum aluminum) recommended for applications requiring one or more of the following characteristics: excellent formability, excellent resistance to corrosion and excellent weldability. It has relatively low strength. It is recommended...
Journal Articles
Alloy Digest (1983) 32 (2): CS-92.
Published: 01 February 1983
... AISI 1060 is a high-carbon steel of low hardenability; it may be used in the as-rolled, annealed, normalized or liquid-quenched-and-tempered condition, depending on the desired properties. It is normally hardened by austenitizing and quenching in oil; however, it may be quenched in water...
Journal Articles
Alloy Digest (1997) 46 (10): Al-342.
Published: 01 October 1997
... Lanxide 91-X-1060-30P is a metal-matrix composite (MMC) consisting of an aluminum-silicon magnesium alloy matrix and 30 vol.% of silicon carbide. The MMC is designed to outperform its unreinforced counterpart. It is available as sand castings with a T6 heat treatment. This datasheet provides...
Journal Articles
Alloy Digest (1987) 36 (12): CS-116.
Published: 01 December 1987
... SAE 1060 is a high-carbon steel of low hardenability; it may be used in the as-rolled, annealed, normalized or liquid-quenched-and-tempered condition, depending on the desired properties. It is normally hardened by austenitizing and quenching in oil; however, it may be quenched in water...
Journal Articles
Alloy Digest (2001) 50 (2): W-23.
Published: 01 February 2001
... ELKONITE G13, G14, 1060, 3042 and 3150 tungsten carbide-silver alloys have good erosion resistance and low contact resistance. The major characteristics are superior resistance to contact welding or sticking and excellent corrosion resistance. Tungsten carbide is a hard, chemically inert material...
Journal Articles
Alloy Digest (2002) 51 (2): Al-375.
Published: 01 February 2002
... AlcoTech Weld Metal 1100 is a 99% minimum or high-purity aluminum welding product that does not respond to heat treatment. It is used to weld the aluminum base alloys 1100, 1060, 1070, 1080 and 1350. This datasheet provides information on composition, physical properties, hardness, tensile...
Journal Articles
Alloy Digest (2010) 59 (4): SS-1060.
Published: 01 April 2010
... deg C (2000 deg F). This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as casting, machining, and joining. Filing Code: SS-1060. Producer...
Journal Articles
Alloy Digest (2016) 65 (12): SA-774.
Published: 01 December 2016
... Durehete 1055 has excellent room and elevated temperature strength, good creep and relaxation resistance to 570 deg C (1060 deg F) coupled with high notch tolerance. In addition, it has thermal expansion coefficients compatible with low alloy steel turbine casing materials. This datasheet provides...
Journal Articles
Alloy Digest (2005) 54 (7): Al-395.
Published: 01 July 2005
... chemical composition corrosion-resistant alloys joinability machinability physical properties shear strength tensile properties workability thermal properties UNS A91060, A91100, A91350 Chemical Composition, wt (Typical) Alloy 1060 Alloy 1100 Alloy 1350 Silicon 0.25 max 0.95 min (Si + Fe) 0.10...
Journal Articles
Alloy Digest (1991) 40 (3): CS-129.
Published: 01 March 1991
... are only moderately satisfactory. Specification Equivalents: AMS 7240. SAE J408(1060). J412(1060). J414(1060) UNS No. Cl0600 Federal: QQ-S-633 and QQ-S-00640 (Army Ord). Military: MIL-S-16974(Gr1060) AIS1 1060, ASTM A29( 1060). A5 lO( 1060). A576( 1060). A682( 1060). General Characteristics: UNS No. Cl0600...
Journal Articles
Alloy Digest (2002) 51 (2): Ti-126.
Published: 01 February 2002
... Reduction °C °F MPa ksi in 300 h, % MPa ksi MPa ksi in 5D, % in area, % 400 752 560 81 0.087 1080 157 167 1150 19 43 450 842 350 51 0.085 1060 154 174 1200 14 40 500 932 193 28 0.094 1060 154 165 1140 18 43 (a) The creep testpiece is subjected to a room-temperature tensile test after surface removal. DOI...
Journal Articles
Alloy Digest (1993) 42 (5): TS-516.
Published: 01 May 1993
... 209 216 Hole Diameter in. mm .16 4 .32 8 .32 16 1.0 25 2xD 1400 (.003) 1400 (.08) 875 (.006) 875 (.15) 450 (.OlO) 450 (.25) 295 (0.12) 295 (.30) Drilling Depth of Hole 6xD 8xD r.p.mJfeed (in/rev or mm/rev) 1060 (003) loo0 (.002) 1060 (.08) loo0 (.05) 720 (.004) 650 (.003) 720 (.lO) 650 (.08) 370 (.008...
Journal Articles
Alloy Digest (2003) 52 (9): Cu-710.
Published: 01 September 2003
... 7026 (C 7026) physical properties power applications tensile properties workability thermal properties UNS C70260 Chemical Composition, wt Copper (incl. Ni, Si, P) 99.5 min Nickel (incl. Co) 1.0 3.0 Silicon 0.2 0.7 Phosphorus 0.010 max Physical Properties: TM00-TM04 TM0S Liquidus, °C (°F) 1060...
Journal Articles
Alloy Digest (1992) 41 (11): SS-536.
Published: 01 November 1992
... OF THYROPLAST 2316FM I Hole Dia. 1 2xD Depth of Hole* 6xD 8xD 10xD I in .16 .32 64 1.0 mm I -p.m. (feed - in or mm/rev) 1700 (.003) 1420 (.003) 4 1700 (-08) 1420 (05) 1060 mw 880 (.004) 8 1060 (14) 880 (.ll) 550 (.OlO) 460 (.OOS) 16 550 (-25) 460 (. 19) 350 (.012) 290 (.009) 25 350 (.29) 290 (.22) 1300 (.002...
Journal Articles
Alloy Digest (2009) 58 (11): SA-611.
Published: 01 November 2009
... Ultimate tensile strength EL, % Impact strength Apparent hardness °C °F kg/m3 lb/in.3 MPa ksi MPa ksi J ft · lbf HV10 HRC 1120 2050 7140 0.257 0.05 750 109 1060 154 1.9 20 15 324 33 1150 2100 7140 0.257 0.03 765 111 1105 160 2.0 22 16 324 33 1175 2150 7160 0.258 0.01 780 113 1140 165 2.2 23 17 324 33 1260...
Journal Articles
Alloy Digest (1958) 7 (9): SA-75.
Published: 01 September 1958
.... 100,000 hrs.* 932 24900 9500 14900 1022 12400 4400 7400 1060 8500 3000 13650 5300 1112 - - 9950 6000 L Extrapolated values. (Specimens mated for 220 BrineE hardness before testing.) Table 6 - STRESS-RUPTURE DATA (Heat treated, forged or cast bars) Test Temperature Sttess, Psi for Rupture in OF. 1,000 hrs...
Journal Articles
Alloy Digest (1994) 43 (2): TS-523.
Published: 01 February 1994
... 020max P. lo-P.20 225-325 45-95 H.S.S. 70-90 15-30 Drilling Hole Diameter Depth of Hole in. mm 2xD 6xD 8xD 1OxD r.p.mJfeed (in/rev or mm/rev) .16 1400 (.003) 1060 (.003) 1000 (.002) 940 (.002) 4 1400 (.08) 1060 (.08) 1000 (-05) 940 (.05) .32 875 (.006) 720 (.004) 650 (.003) 590 (.003) 8 875 (.15) 720...
Journal Articles
Alloy Digest (1987) 36 (12): TS-486.
Published: 01 December 1987
... be nitrided in ammonia gas at 975 F (525 C) for I O-40hours for casedepths of 0.0060.012 inch. Surface hardness will be about 1000 DPH (Vickers). Corrosion and erosion resistance are improved by nitriding. Tufftridiag: A Zhour treatment at 1060°F (570°C) produces a surface hardness of about 95&lOOODPH...