Alloy Digest (1976) 25 (6): CS-60.
Published: 01 June 1976
... SAE 1026 is a low-to-medium-carbon steel used in the annealed, hot-worked, normalized, cold-worked or water-quenched-and-tempered condition for a variety of engineering and construction applications. It combines good workability (hot or cold), good machinability and good weldability. It has...
Journal Articles
Alloy Digest (2022) 71 (4): CS-221.
Published: 01 April 2022
... 1025, 1026, C25, C25E, and C25R are wrought low-carbon non-alloy steels that are used in the normalized, cold worked, or quenched and tempered condition. These steels are widely used for small, moderately stressed parts that require higher strength levels than can be achieved by the lower carbon...
Journal Articles
Alloy Digest (2023) 72 (8): CS-255.
Published: 01 August 2023
... 1026 is a wrought low-carbon (carbon = 0.22-0.28%) non-alloy steel that has a higher manganese content (manganese = 0.60-0.90%) than 1025 (manganese = 0.30-0.60%). It is used in the normalized, cold worked, or quenched and tempered condition. 1026 may also be nitrided or nitrocarburized...
Journal Articles
Alloy Digest (1988) 37 (11): CS-123.
Published: 01 November 1988
... readily by acids, but is reasonably resistant to alkalis at ordinary tanpera- tures. Small additions of copper increase its atmospheric corro- sion resistance. Specification Equivalents: AISI 1026 ASTM A29(1026). A273(1026), A510(1026). A519(1026). A545(1026).A576(1026). MIL SPEC MIL-T-20157. MIL-F-20670...
Journal Articles
Alloy Digest (2008) 57 (12): SS-1026.
Published: 01 December 2008
... as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, and machining. Filing Code: SS-1026. Producer or source: Carpenter Technology Corporation. Producer or Source: Carpenter Technology Corporation Copyright © ASM International® 2008 2008 ASM...
Journal Articles
Alloy Digest (2020) 69 (2): Al-461.
Published: 01 February 2020
... Solidification range °C (°F) Density kg/m3 (lb/in.3) Coefficient of linear thermal expansion 10 6/K (10 6/°F) Thermal conductivity W/(m K) (Btu/(h·ft·°F)) At 20 °C (68 °F) 20 300 °C (68 572 °F) 20 °C (68 °F) Value 608 552 (1126 1026) 2640 (0.095) 21 (11.7) 135 170 (78.1 98.3) Mechanical Properties...
Journal Articles
Alloy Digest (2007) 56 (11): Ag-13.
Published: 01 November 2007
... MPa ksi MPa ksi MPa ksi MPa ksi 0 1091 158.2 1026 148.8 1031 149.6 856 124.1 20 1388 201.3 1318 191.2 1328 192.6 1122 162.8 37 1555 225.6 1493 216.5 1474 213.8 1143 165.8 50 1636 237.3 1567 227.3 1549 224.7 1327 192.4 61 1696 246.0 1627 236.0 1602 232.4 1379 200.0 69 1770 256.7 1682 244.0 1650 239.3...
Journal Articles
Alloy Digest (1977) 26 (10): SS-345.
Published: 01 October 1977
... 8.25 .289 7.35 .258 6.54 .229 5.83 .204 5.19 .182 4.62 .162 4.12 ,144 3.67 ,128 3.26 .114 2.91 .102 2.59 .091 2.31 ,081 2.05 ,072 1.83 .064 1.63 ,057 1.45 .051 1.29 ,045 1.15 .040 1.02 ,036 0.912 .0320 0.812 510.3 647.5 811.5 1026. 2.731 3.461 4.339 5.511 1294. 1639. 2055. 2611. 6.853 8.750 11.05 13.67...
Journal Articles
Alloy Digest (1961) 10 (8): Co-29.
Published: 01 August 1961
... Saey Life El~ngscioo Time is Hours for Da1 Hours ln 1 7. total Elonsacion of 1200 20000 :Eii 40000 50000 l%E 1350 20000 20000 5704 1296t f 3r 12st 1730 1598 2363 1610+ 0:3 0.6 1.2 1058 1475 - 1693 - 249 14;t 115 1026 :z I Table 5- ULTIMATE STRRNGTHLIWACTDATA (Resin shell cssc) Test Tempersnue Tensile...
Journal Articles
Alloy Digest (2023) 72 (7): CS-252.
Published: 01 July 2023
... be tempered at a temperature not lower than 30 °C (55 °F) above the nitrocarburizing temperature. Source: Ref 53, 62, 65 References 1. SAE 1025, SAE 1026, CEN C25, ISO C25 STEEL DATA SURVEY: Wrought Low-Carbon Non-Alloy Steels, Alloy Digest, Vol 71 (No.4), 2022, CS-221, httpsdoi.org/10.31399 /asm.ad.cs0221 2...