Skip Nav Destination
Close Modal
Search Results for
1021
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-17 of 17 Search Results for
1021
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (2022) 71 (5): CS-223.
Published: 01 May 2022
... 1021, 1022, C20C, and C20GC are wrought low-carbon non-alloy steels that are used in the as rolled, normalized, cold worked, or quenched and tempered condition. They are widely used for lightly and moderately stressed parts that require higher strength levels than can be achieved by the lower...
Abstract
View article
PDF
1021, 1022, C20C, and C20GC are wrought low-carbon non-alloy steels that are used in the as rolled, normalized, cold worked, or quenched and tempered condition. They are widely used for lightly and moderately stressed parts that require higher strength levels than can be achieved by the lower carbon grades, and also for applications where a combination of low-to-moderate strength, good ductility, good cold formability, and good weldability are required. 1021 and 1022 may also be used in the carburized or carbonitrided, and subsequently quench hardened and tempered condition for parts requiring a hard, wear-resistant surface, but with little need for increased mechanical properties in the core. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: CS-223. Producer or source: Data Survey.
Journal Articles
Alloy Digest (2023) 72 (10): CS-263.
Published: 01 October 2023
... 1021, 1022, C20C, and C20GC are wrought low-carbon (carbon = 0.18–0.23%) non-alloy steels that are used in the as rolled, normalized, cold worked, or quenched and tempered condition. They are widely used for lightly and moderately stressed parts that require higher strength levels than can...
Abstract
View article
PDF
1021, 1022, C20C, and C20GC are wrought low-carbon (carbon = 0.18–0.23%) non-alloy steels that are used in the as rolled, normalized, cold worked, or quenched and tempered condition. They are widely used for lightly and moderately stressed parts that require higher strength levels than can be achieved by the lower carbon grades, and also for applications where a combination of low-to-moderate strength, good ductility, good cold formability, and good weldability are required. 1021 and 1022 may also be used in the case hardened, nitrided, or nitrocarburized condition. This datasheet provides information on composition, physical properties, microstructure, hardness, and tensile properties. It also includes information on forming and heat treating. Filing Code: CS-263. Producer or source: Heat Treater's Guide.
Journal Articles
Alloy Digest (1976) 25 (11): CS-64.
Published: 01 November 1976
... SAE 1021 is a carbon steel of relatively high manganese content which increases hardenability and hardness over that of carbon steels of lower manganese. It combines good machinability, good workability (hot or cold) and good weldability. It is used in the annealed, hot-worked, normalized, cold...
Abstract
View article
PDF
SAE 1021 is a carbon steel of relatively high manganese content which increases hardenability and hardness over that of carbon steels of lower manganese. It combines good machinability, good workability (hot or cold) and good weldability. It is used in the annealed, hot-worked, normalized, cold-worked or water-quenched-and-tempered condition for many applications. It may be used in uncarburized applications and for components case-hardened by carburizing. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: CS-64. Producer or source: Carbon steel mills.
Journal Articles
Alloy Digest (2008) 57 (11): SS-1021.
Published: 01 November 2008
... as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as forming and heat treating. Filing Code: SS-1021. Producer or source: Carpenter Technology Corporation. Producer or Source: Carpenter Technology Corporation Copyright © ASM...
Abstract
View article
PDF
Carpenter 286-LNi Alloy is a precipitation-hardenable Fe-Ni-Cr alloy designed to resist corrosion while providing high strength at temperatures up to 704 deg C (1300 deg F). This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as forming and heat treating. Filing Code: SS-1021. Producer or source: Carpenter Technology Corporation.
Journal Articles
Alloy Digest (1988) 37 (9): CS-122.
Published: 01 September 1988
.... Specification Equivalents: AISI 1021. SAE J403 (1021); J412 (1021); J414 (1021) ASTM A29 (1021); A510 (1021) A519 (1021) A545 (1Ml); A548 (1021); A576 (1021); A659 (1021) General Characteristics: UNSG10201 isused withoutorwithcase-hardening developed by carburizing. carbonittiding or cyanidmg. UNS G10201 steel...
Abstract
View article
PDF
UNS G10210 is a carbon steel of relatively high manganese content which increases hardenability and hardness over that of carbon steels of lower manganese. It combines good machinability, good workability (hot or cold) and good weldability. It is used in the annealed, hot-worked, normalized, cold-worked or water-quenched-and-tempered condition for many applications. It may be used in uncarburized applications and for components case-hardened by carburizing. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: CS-122. Producer or source: Carbon steel mills.
Journal Articles
Alloy Digest (1989) 38 (8): Al-298.
Published: 01 August 1989
.... thin and thick section extrusions, sheet. foil, rivets, tubing. Applications: Aircraftstruceures,wheels.gas~ineenginecomponents,missile components, fasteners. Producer: Allied-Signal Inc. Corporate Technology P.O. Box 1021 R Morristown, New Jersey 07962-1021 Tel: (201)455-5336 ...
Abstract
View article
PDF
FVS 0812 is a rapidly solidified Al-Fe-V Sialloy which combines the strength, ductility and fracture toughness of conventional aerospace aluminum alloys with the high-temperature strength and stability of the FVS aluminum alloys. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance and corrosion resistance as well as casting, forming, machining, and joining. Filing Code: Al-298. Producer or source: Allied-Signal Inc..
Journal Articles
Alloy Digest (2020) 69 (11): TS-803.
Published: 01 November 2020
... Properties Hardness Treatment condition Annealed Quenched Quenched and tempered Hardness 235 HBW max(a) 59 63 HRC(b) 54 60 HRC(c) Guidance values. (a) Carpenter Technology Corporation. (b) Source: Metals Handbook Desk Edition, 2nd ed., ASM International, 1998, p 1021. (c) Source: Metals Handbook Desk Edition...
Abstract
View article
PDF
CarTech A6, also known as CarTech Vega, is an air-hardening, high-carbon (0.70%), Mn-Cr-Mo, alloy cold-work tool steel. It combines the deep-hardening and minimum size change characteristics of air-hardening tool steels with the simplicity of low-temperature heat treatment possible in many oil-hardening tool steels. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, and machining. Filing Code: TS-803. Producer or source: Carpenter Technology Corporation.
Journal Articles
Alloy Digest (2002) 51 (2): Ti-126.
Published: 01 February 2002
... 739 107 891 129 19 49 300 572 679 98 851 123 18 49 400 752 644 93 828 120 17 48 450 842 622 90 811 118 18 48 Oil quenched and aged 20 68 970 140 1110 161 8 25 100 212 940 136 1118 162 14 43 200 392 819 119 1021 148 15 46 300 572 738 107 986 143 14 46 400 752 701 102 932 135 14 46 450 842 688 100 899...
Abstract
View article
PDF
TIMETAL 679 is a Ti-11Sn-5Zr-2.25Al-1Mo-0.2Si alloy with three phases at room temperature. It has high strength with creep resistance. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength as well as creep and fatigue. It also includes information on forming and heat treating. Filing Code: TI-126. Producer or source: Timet.
Journal Articles
Alloy Digest (2020) 69 (2): Cu-905.
Published: 01 February 2020
... conductivity MS/m (%IACS) (a) For annealed condition At 20 °C (68 °F) 20 300 °C (68 572 °F) 20 °C (68 °F) 20 °C (68 °F) 20 °C (68 °F Value 1021 (1870) 8910 (0.322) 17.5 (9.7) 200 (115) 0.0345 (20.74) 29.0a) (50)(a) Mechanical Properties See Tables 1 and 2. The comparison of yield strength and electrical...
Abstract
View article
PDF
Olin Brass Alloy C19020 is a copper-nickel-tin low-alloyed copper. It was developed as alloy NB-105 by Dowa Metaltech Company Limited, Japan, to meet increasing requirements of current carrying capacity, stiffness, formability and service temperature survivability being demanded by the automotive and electronic industries. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming and joining. Filing Code: Cu-905. Producer or source: Olin Brass, GBC Metals, LLC.
Journal Articles
Alloy Digest (2020) 69 (1): Cu-904.
Published: 01 January 2020
... Property Unit At Value Melting point Liquidus °C (°F) 1041 (1905) Melting point Solidus °C (°F) 1021 (1870 Density kg/m3 (lb/in.3) 20 °C (68 °F) 8800 (0.318) Coefficient of linear thermal expansion 10 6/K (10 6/°F) 20 300 °C (68 572 °F) 18.4 (10.2) Thermal conductivity W/(m K) (Btu/(h·ft·°F)) 20 °C (68...
Abstract
View article
PDF
Olin Brass Alloy C42200 (Tradename: Lubronze) is a copper-zinc-tin alloy (tin brass). The mechanical properties and performance of C42200 are very similar to those of high-zinc brass alloys with the added benefit of improved resistance to stress relaxation. It is also a cost-effective alternative to phosphor bronze. This datasheet provides information on composition and physical properties. It also includes information on corrosion resistance as well as forming. Filing Code: Cu-904. Producer or source: Olin Brass GBC Metals, LLC.
Journal Articles
Alloy Digest (2010) 59 (7): Ni-680.
Published: 01 July 2010
.../m·K (Btu/h·ft·ºF) 11.2 (65) See Table 1 for the linear coefficient of expansion. Mechanical Properties: See Tables 2 and 3. Heat Treatment: A wide range of mechanical properties may be obtained depending on the heat treatment. For oil and gas applications: Solution treat: 1021 to 1052 ºC (1870 to 1925...
Abstract
View article
PDF
Although LSS 718 EP is a premier aerospace nickel-base alloy, it has a significant presence in exploration and production (EP) of oil and gas and this modification is meant for those applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: Ni-680. Producer or source: Latrobe Specialty Steel Company.
Journal Articles
Alloy Digest (2021) 70 (4): Cu-919.
Published: 01 April 2021
... Products NA Physical Properties ASTM B36/B36M:2018 CuZn10 (CW501L) EN 1652:1997 C 2200 Property Unit At Value JIS H 3100:2018 Melting point, 1043 liquidus °C (1910)(a) General Characteristics Melting point, (°F) 1021 solidus (1870)(a) Attractive color; good electrical and thermal conductivity; Density...
Abstract
View article
PDF
Wieland C22000 (C220) is a 90Cu-10Zn alloy. Known for years as Commercial Bronze, this alloy derives its name from its rich bronze color. Wieland C22000 offers a unique set of properties that makes it suitable for applications requiring deep drawing and resistance to corrosion. Its appealing color also makes it ideal for architectural applications. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and machining. Filing Code: Cu-919. Producer or source: Wieland Rolled Products NA.
Journal Articles
Alloy Digest (1974) 23 (1): Zr-6.
Published: 01 January 1974
... resisring properties similar to those of the Zircaloys in 7500F steam at a pressure of 1500 psi. The corrosion of Zr-3Nb-1Sn alloy was lower than that of the Zircaloys after 174 days in ammonia (pH 10) at 530oF and in a fluence of 1.7 X 1021 neutrons/sq cm. Sensitivity to oxygen contamination of the reactor...
Abstract
View article
PDF
Zr-3Nb-1Sn was developed to provide improved elevated temperature mechanical properties over the Zircaloys without reducing corrosion resistance. It is used in nuclear applications. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Zr-6. Producer or source: Teledyne Wah Chang Albany.
Journal Articles
Alloy Digest (2021) 70 (3): CS-209.
Published: 01 March 2021
... C20 Quench Hardening and Tempering ASTM A576:2017 Grade 1020 Grade 1021 Quench Hardening. Heat to 860 900 °C (1580 1650 EN 10083-2:2006 (UNS G10200) (UNS G10210) °F). Wait for equalization of the temperature. Soak JIS G 4051:2016 for at least 30 min. Quench in water, aqueous poly- C22E (1.1151...
Abstract
View article
PDF
Lucefin C20 is a low-carbon, non-alloy steel that is used in the normalized, cold finished, or quenched and tempered condition. It may also be used in the carburized or carbonitrided, and subsequently quench hardened and tempered, condition for parts requiring a hard wear-resistant surface, but with little need for increased mechanical properties in the core. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: CS-209. Producer or source: Lucefin S.p.A..
Journal Articles
Alloy Digest (1997) 46 (5): Fe-56.
Published: 01 May 1997
... 857 1472 1015 1613 1112 20.2 60.0 1600 871 1465 1010 158.1 1090 226 56.8 1625 885 148.1 1021 1643 1133 I 54.5 1650 899 1373 947 1615 1114 15.0 22.3 1675 913 132.9 916 1582 1091 11.6 18.9 1700 927 130.9 903 155.0 1069 10.0 19.7 Roprr*sbawdon%insquarrwanrrwakcdbPsroiluionmaredlMXPFIhaircooled *aged...
Abstract
View article
PDF
Pyromet CTX-1 is a high-strength, precipitation-hardenable superalloy exhibiting a low coefficient of thermal expansion and high strength up to about 1200 deg F. The alloy possesses high hot hardness and good thermal fatigue resistance. Its applications include components for gas turbine engines, hot-work die applications and high-pressure hydrogen environments. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: FE-56. Producer or source: Carpenter. Originally published February 1976, revised May 1997.
Journal Articles
Alloy Digest (2001) 50 (3): Cu-662.
Published: 01 March 2001
...) tearing on mechanical Alloy °C °F Celsius Farenheit superheat(a), cm resistance(b) Drossing Soldering Brazing properties C83600 1010 1850 156 280 24 15 21 Low Excellent Good Large C84400 1004 1840 161 291 30 23 24 Medium Excellent Good Large EnviroBrass I (C89510) 1021 1871 206 371 24 14 Low Excellent...
Abstract
View article
PDF
EnviroBrass III is one of a series of alloys pursued by an industry consortium to develop alloys that meet the National Sanitation Foundation’s standard on low lead pickup in water supply systems. The research showed that a combination of bismuth and selenium provides the same beneficial effect on machinability as does lead. EnviroBrass III contains up to 1.2% Bi and 0.1% Se and is suitable for permanent mold and pressure die castings. SeBiLOY was the original name used to represent these alloys (see SeBiLOY I, Alloy Digest Cu-605, June 1996, and SeBiLOY II, Alloy Digest Cu-606, revised October 1996). This datasheet provides information on composition, hardness, and tensile properties. It also includes information on casting and machining. Filing Code: CU-662. Producer or source: Copper and copper alloy mills.
Journal Articles
Alloy Digest (2006) 55 (2): Ni-630.
Published: 01 February 2006
... 113 391 57 42 200 392 700 102 380 55 44 400 752 640 93 371 54 47 600 1112 600 87 360 52 47 800 1472 577 84 340 49 7 1000 1832 78 11 73 11 100 Solution treated as above and precipitation hardened at 780 °C (1435 °F) for 4 h and air cooled 20 68 1075 156 716 104 24 200 392 1021 148 670 97 27 400 752 983...
Abstract
View article
PDF
Nicrofer 7016TiAl (also known as alloy 751) is an age-hardening Ni-Cr-Fe alloy with both good corrosion resistance and high rupture strength. It is a slight modification of alloy Nicrofer 7016TiNb (alloy X-750) and is used in diesel exhaust valves. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-630. Producer or source: VDM Technologies Corporation.