1-20 of 39

Search Results for 1016

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2022) 71 (7): CS-226.
Published: 01 July 2022
... 1016, C16E, and C16R are wrought low-carbon non-alloy steels that are used in the as rolled, normalized, or cold worked condition. These steels are widely used for lightly and moderately stressed parts that require higher strength levels than can be achieved by the lower carbon grades, and also...
Journal Articles
Alloy Digest (1976) 25 (2): CS-58.
Published: 01 February 1976
... SAE 1016 is a low-carbon steel combining good machinability, good workability and good weldability. It is used for components case-hardened by carburizing. It is also used in the hot-rolled, annealed, normalized or cold-worked condition for a variety of construction and engineering applications...
Journal Articles
Alloy Digest (2024) 73 (4): CS-269.
Published: 01 December 2024
... 1016, C16E, and C16R are wrought low-carbon (carbon = 0.12–0.18%) non-alloy steels that are used in the as-rolled, annealed, normalized, or cold worked condition. They are widely used for lightly and moderately stressed parts that require higher strength levels than can be achieved by the lower...
Journal Articles
Alloy Digest (2008) 57 (7): SS-1016.
Published: 01 July 2008
... properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-1016. Producer or source: Sandmeyer Steel Company. Producer or Source: Sandmeyer Steel Company Copyright © ASM International® 2008 2008...
Journal Articles
Alloy Digest (1985) 34 (8): CS-108.
Published: 01 August 1985
... temperatures. Small additions of copper increase its atmospheric corrosion resistance. Specification Equivalents: AISI 1016. ASTM: A 29(1016), A 108(1016), A 510(1016), A 513(1016), A 545(1016). A 548(1016), A 549(1016), A 576( 1016) and A 659( 1016). Military MIL-S-866(1016). SAE: J403(1016), J412(1016...
Journal Articles
Alloy Digest (1998) 47 (12): Cu-625.
Published: 01 December 1998
... that of conventional phos- phor bronzes of equal strength. The alloy is excellent for plating. Products Available: sheet, snip Producer: Waterbury Rolling Mills, Inc. 240 E. Aurora Street Mterbury, CT 06708 (800) 243-3002 (203) 7m151 (203) 754-1016 (fax) ISSN: 002614X 1/?had Hard X-hard Spriag (a) I hattanpmtue...
Journal Articles
Alloy Digest (1999) 48 (12): Cu-643.
Published: 01 December 1999
... 100 1184. Producer: Waterbury Rolling Mills, Inc. 240 E. Aurora Street Waterbury, CT 06708 (800) 243-3002 (203) 754-0151 (203) 754-1016 (fax) ISSN: 002-614X ©Copyright 1999, ASM International. All rights reserved. Data shown are typical, not to be used for specification or final design. Published...
Journal Articles
Alloy Digest (2000) 49 (8): Cu-629.
Published: 01 August 2000
... (oscillated) reels can be supplied with gages from 0.006 0.080 in., in widths from 0.150 2.25 in. Reels are pack- aged in 500, 1000, 2000, and 4000 lb. Producer: Waterbury Rolling Mills, Inc. 240 E. Aurora Street Waterbury, CT 06708 (800) 243-3002 or (203) 754-0151 (203) 754-1016 (fax) ISSN: 002-614X Tin 1.7...
Journal Articles
Alloy Digest (1995) 44 (3): SS-586.
Published: 01 March 1995
... For furnaces Producer: Paralloy Limited Billingham, England 0642-370-686 (Tested In air) In Ibis severe lest. an odrlion 1016 01 l.Snm/vr in air is considcrrd IO bL SIIIS~~CIO~Y Fig. 3 -Oxidation resistance (tested In air) Carbon gmdient in Cr-Ni alloy8 3.0 25135 WCb 1050 115oc 1800 19Qo 2000 2100 F...
Journal Articles
Alloy Digest (1999) 48 (3): Cu-630.
Published: 01 March 1999
.... Aurora Street Waterbury, CT 06708 (800) 243-3002 or (203) 754-0151 Fax: (203) 754-1016 ISSN: 002-614X ©Copyright 1999, ASM International. All rights reserved. Data shown are typical, not to be used for specification or final design. Published by: ASM International Materials Park, Ohio 44073-0002 440-338...
Journal Articles
Alloy Digest (1999) 48 (10): Cu-633.
Published: 01 October 1999
... (oscillated) reels can be supplied with gages from 0.006 0.080 in., in widths from 0.150 2.25 in. Reels are packaged in 500, 1000, 2000, and 4000 lb units. Producer: Waterbury Rolling Mills, Inc. 240 E. Aurora St. Waterbury, CT 06708 (800) 243-3002 (203) 754-0151 (203) 754-1016 (fax) ISSN: 002-614X ©Copyright...
Journal Articles
Alloy Digest (1999) 48 (10): Cu-634.
Published: 01 October 1999
... Mills, Inc. 240 E. Aurora Street Waterbury, CT 06708 (800) 243-3002 (203) 754-0151 (203)754-1016 (fax) ISSN: 002-614X ©Copyright 1999, ASM International. All rights reserved. Data shown are typical, not to be used for specification or final design. Published by: ASM International Materials Park, Ohio...
Journal Articles
Alloy Digest (1998) 47 (11): Cu-624.
Published: 01 November 1998
... are 500,lOOO. 2000. and 4000 pounds. Applications: Producer: Waterbury Rolling Mills, Inc. 240 E. Aurora Street Wuehry, CT 06708 (800) 243-3002 (203) 754-0151 (203) 754-1016 (fax) Typical applications for WRM alloy 4085 include connectors, contact springs, terminals, and lead frames. MN: 002614X Cu-624B ...
Journal Articles
Alloy Digest (1999) 48 (1): Cu-626.
Published: 01 January 1999
..., 2000, and 4000 lb. Applications: Typical applications for WRM Alloy 5108 include terminals, connectors, lead frames, and contact springs. Producer: Waterbury Rolling Mills, Inc. 240 E. Aurora Street Waterbury, CT 06708 (800) 243-3002 or (203) 754-0151 (203) 754-1016 (fax) ISSN: 002-614X Cu-626B ...
Journal Articles
Alloy Digest (1999) 48 (8): Cu-638.
Published: 01 August 1999
... tubes. Producer: Waterbury Rolling Mills, Inc. 240 E. Aurora Street Waterbury, CT 06708 (800) 243-3002 or (203) 754-0151 (203) 754-1016 (fax) ISSN: 002-614X ©Copyright 1999, ASM International. All rights reserved. Data shown are typical, not to be used for specification or final design. Published...
Journal Articles
Alloy Digest (1999) 48 (10): Cu-636.
Published: 01 October 1999
... in. Packages come in 500, 1000, 2000, and 4000 lb reels. Applications: Typical applications for WRM alloy 5118 include terminals, connectors, lead frames, and contact springs. Producer: Waterbury Rolling Mills, Inc. 240 E. Aurora Street Waterbury, CT 06708 (800) 243-3002 (203) 754-0151 (203) 754-1016 (fax...
Journal Articles
Alloy Digest (1999) 48 (10): Cu-616.
Published: 01 October 1999
... 06708 (800) 243-3002 (203) 754-0151 (203) 754-1016 (fax) ISSN: 002-614X Cu-616B Table 2 Bend Properties Temper Goodway R/T Badway R/T Soft 0 0 1 2 hard 0 0 Hard 0.5 1.0 X-hard 1.0 1.5 R/T, radius to thickness ratio. 90° bends, 0.020 in. thick and below, with width to thick- ness ratios up to 10 Table 3...
Journal Articles
Alloy Digest (2023) 72 (1): SS-1355.
Published: 01 January 2023
... Product Forms Coils and cut lengths in thicknesses from 0.25 to 2.29 mm (0.010 to 0.090 in.) and widths up to and including 1016 mm (40 in Applications Cleveland-Cliffs 444 is ideal for applications requiring high corrosion resistance and high resistance to chloride stress corrosion cracking. Typical...
Journal Articles
Alloy Digest (1990) 39 (5): P-13.
Published: 01 May 1990
... 0.02 0.03 0.03 Volume resistivity D257 Ohm-cm x 1016 4.0 1.6 1.2 - DOI: 10.31399/asm.ad.p0013 Copyright © ASM International® 1996 Table 3 - UNDERWRITER LABORATORY PROPERTIES OF VALOX@ 300 FAMILY Test Resin fi0pel-Q Method Units 325 31OSEO 357 365 FIammabiIity* uL94 - V-0x).028 - 5Vfl.123 HB/O.O58 5V...
Journal Articles
Alloy Digest (2005) 54 (12): SS-947.
Published: 01 December 2005
... of elasticity, GPa (106 psi) 214 (31) Heat Treatment: Annealing must be performed after hot working and before rehardening. Heat at a rate not exceeding 222 °C/h (400 °F/h) to 1016 1038 °C (1860 1900 °F) and hold at temperature for 1 h/in. (25.4 mm) of maximum thickness or 2 h minimum. Then cool slowly...